← Back to Patent Explorer
US4287282A Expired / Lapsed US ⏱️ 0.0 years remaining

Composite magnetic developer

Assignee: Kyocera Mita Industrial Co Ltd
•
Filing: 1980-01-10
•
Granted: 1981-09-01
•
Expires: 2000-01-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Disclosed is a composite magnetic developer which consists essentially of a homogeneous intimate mixture comprising a plurality of electrically insulating magnetic particulate developers comprising a binder medium and a finely divided magnetic material dispersed in the binder medium, in which the difference of the dielectric constant between the developers is in the range of from 0.2 to 0.85. This composite magnetic developer can provide a clear transferred image having a high density on a transfer sheet such as plain paper, and even if the copying operation is conducted continuously for a long time by using this developer, excellent transferred images can be obtained without substantial change of the composition of the composite developer or substantial reduction of the image density.

Inventors

  • 👤 Nobuhiro Miyakawa
  • 👤 Takashi Teshima

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 16:56
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/083; G03G9/09; G03G9/0906

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 86 words
A composite magnetic developer which consists essentially of a homogeneous intimate mixture comprising a plurality of electrically insulating magnetic particulate developers, each developer comprising a binder medium and a finely divided magnetic material dispersed in the binder medium, wherein the difference of the dielectric constant (ε), as measured under conditions of an electrode spacing of 0.65 mm, an electrode sectional area of 1.43 cm 2 and an inter-electrode load of 105 g/cm 2 , between said developers is in the range of from 0.2 to 0.85.
Claim 2
Dependent Claim 86 words
A composite magnetic developer which consists essentially of a homogeneous intimate mixture comprising a plurality of electrically insulating magnetic particulate developers, each developer comprising a binder medium and a finely divided magnetic material dispersed in the binder medium, wherein the difference of the dielectric constant (ε), as measured under conditions of an electrode spacing of 0.65 mm, an electrode sectional area of 1.43 cm 2 and an inter-electrode load of 105 g/cm 2 , between said developers is in the range of from 0.2 to 0.85.
Claim 3
Dependent Claim 69 words
A composite magnetic developer as set forth in claim 1 wherein each of the component developers has a volume resistivity of at least 5×10 13 Ω-cm as measured under the same conditions as adopted for determination of the dielectric constant and said homogeneous intimate mixture has a volume resistivity of at least 1×10 14 Ω-cm as measured under the same conditions as adopted for determination of the dielectric constant.
Claim 4
Dependent Claim 38 words
A composite magnetic developer as set forth in claim 1 wherein said homogeneous intimate mixture has an electrostatic capacity of 7.8 to 15 piccofarad as measured under the same conditions as adopted for determination of the dielectric constant.
Claim 5
Dependent Claim 53 words
A composite magnetic developer for developing negative electrostatic latent images, as set forth in claim 1, wherein the homogeneous intimate mixture comprises (A) magnetic developer particles having a relatively high dielectric constant and (B) magnetic developer particles having a relatively low dielectric constant at an (A)/(B) weight ratio of from 1/0.08 to 1/1.
Claim 6
Dependent Claim 53 words
A composite magnetic developer for developing positive electrostatic latent images, as set forth in claim 1, wherein the homogeneous intimate mixture comprises (B) magnetic developer particles having a relatively low dielectric constant and (A) magnetic developer particles having a relatively high dielectric constant at a (B)/(A) weight ratio of from 1/0.08 to 1/l.
Claim 7
Dependent Claim 26 words
A composite magnetic developer for developing negative electrostatic latent images as set forth in claim 4 wherein the weight ratio (A)/(B) is from 1/0.1 to 1/0.5.
Claim 8
Dependent Claim 26 words
A composite magnetic developer for developing positive electrostatic latent images, as set forth in claim 5 wherein the weight ratio (B)/(A) is from 1/0.1 to 1/0.5.

References Cited (Backward Citations)

US3349703A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-08-31 1985-03-02 1985-09-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-08-31 1989-03-02 1989-09-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-08-31 1993-03-02 1993-09-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag