Abstract

Abstract An article of manufacture, the crosslinked product of a semi-conductive composition directly bonded to a crosslinked polyolefin substrate, as for example, an electrical conductor having, as primary insulation, a crosslinked polyolefin and, as semi-conductive shielding, the crosslinked product of a semi-conductive composition.

Inventors

  • 👤 Lucio Ongchin

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 16:50
CPC Classifications
B; B32; B32B; B32B27/00; B32B27/06; B32B27/08; B32B27/32; C; C08; C08K; C08K3/00; C08K3/02; C08K3/04; C08L; C08L23/00; C08L23/02; C08L23/04; C08L23/08; C08L23/0846; C08L23/0853; H; H01; H01B; H01B1/00; H01B1/20; H01B1/24; B32B2305/00; B32B2305/72; B32B2307/00; B32B2307/20; B32B2307/206; B32B2323/00; B32B2323/04; C08L2312/00; C08L9/00; C08L9/02; Y; Y10; Y10S; Y10S428/00; Y10S428/91; Y10T; Y10T428/00; Y10T428/25; Y10T428/31504; Y10T428/31855; Y10T428/31909; Y10T428/31913; Y10T428/31928

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 204 words
An article of manufacture comprising the crosslinked product of a vulcanizable semi-conductive composition consisting essentially of (A) an ethylene copolymer selected from the group consisting of an ethylene-alkyl acrylate copolymer containing from about 15 to 45 percent by weight of alkyl acrylate based on the total weight of said copolymer, said alkyl acrylate being selected from the group consisting of the C 1 to C 8 alkyl esters of acrylic acid and methacrylic acid, and an ethylene-vinyl acetate copolymer containing from about 15 to 45 percent by weight of vinyl acetate based on the total weight of said copolymer, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition, said crosslinked product being directly bonded to a crosslinked polyolefin substrate.
Claim 2
Dependent Claim 204 words
An article of manufacture comprising the crosslinked product of a vulcanizable semi-conductive composition consisting essentially of (A) an ethylene copolymer selected from the group consisting of an ethylene-alkyl acrylate copolymer containing from about 15 to 45 percent by weight of alkyl acrylate based on the total weight of said copolymer, said alkyl acrylate being selected from the group consisting of the C 1 to C 8 alkyl esters of acrylic acid and methacrylic acid, and an ethylene-vinyl acetate copolymer containing from about 15 to 45 percent by weight of vinyl acetate based on the total weight of said copolymer, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition, said crosslinked product being directly bonded to a crosslinked polyolefin substrate.
Claim 3
Dependent Claim 170 words
An article of manufacture comprising the crosslinked product of a vulcanizable semi-conductive composition consisting essentially of (A) and ethylene-alkyl acrylate copolymer containing from about 15 to 45 percent by weight of alkyl acrylate based on the total weight of said copolymer, said alkyl acrylate being selected from the group consisting of the C 1 to C 8 alkyl esters of acrylic acid and methacrylic acid, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition, said crosslinked product being directly bonded to a crosslinked polyolefin substrate.
Claim 4
Dependent Claim 170 words
An article of manufacture comprising the crosslinked product of a vulcanizable semi-conductive composition consisting essentially of (A) and ethylene-alkyl acrylate copolymer containing from about 15 to 45 percent by weight of alkyl acrylate based on the total weight of said copolymer, said alkyl acrylate being selected from the group consisting of the C 1 to C 8 alkyl esters of acrylic acid and methacrylic acid, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition, said crosslinked product being directly bonded to a crosslinked polyolefin substrate.
Claim 5
Dependent Claim 146 words
An article of manufacture comprising the crosslinked product of a vulcanizable semi-conductive composition consisting essentially of (A) an ethylene-vinyl acetate copolymer containing from about 15 to 45 percent by weight of vinyl acetate based on the total weight of said copolymer, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition, said crosslinked product being directly bonded to a crosslinked polyolefin substrate.
Claim 6
Dependent Claim 146 words
An article of manufacture comprising the crosslinked product of a vulcanizable semi-conductive composition consisting essentially of (A) an ethylene-vinyl acetate copolymer containing from about 15 to 45 percent by weight of vinyl acetate based on the total weight of said copolymer, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition, said crosslinked product being directly bonded to a crosslinked polyolefin substrate.
Claim 7
Dependent Claim 40 words
An article of manufacture as defined in claim 3 wherein (D) of the said vulcanizable semi-conductive composition is present in an amount of from about 0.6 to about 2 percent by weight based on the total weight of the composition.
Claim 8
Dependent Claim 35 words
An article of manufacture as defined in claim 3 wherein the said vulcanizable semi-conductive material contains about 0.2 to about 1 percent by weight of an antioxidant based on the total weight of the composition.
Claim 9
Dependent Claim 17 words
An article of manufacture as defined in claim 3 wherein the peroxide crosslinking agent is di-α-cumyl peroxide.
Claim 10
Dependent Claim 19 words
An article of manufacture as defined in claim 2 wherein the polyolefin of the crosslinked polyolefin substrate is polyethylene.
Claim 11
Dependent Claim 19 words
An article of manufacture as defined in claim 3 wherein the polyolefin of the crosslinked polyolefin substrate is polyethylene.
Claim 12
Dependent Claim 34 words
An article of manufacture as defined in claim 1 wherein the said crosslinked polyolefin is the primary insulation about an electrical conductor and the said crosslinked product is the semi-conductive shielding for said insulation.
Claim 13
Dependent Claim 33 words
An article of manufacture as defined in claim 3 wherein the said crosslinked polyolefin is the primary insulation about an electrical conductor and said crosslinked product is the semi-conductive shielding for said insulation.
Claim 14
Dependent Claim 23 words
A process of producing an article as defined in claim 1 wherein the said vulcanizable composition and said polyolefin substrate are simultaneously crosslinked.

References Cited (Backward Citations)

US3950604A Cited
US4214030A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-08-24 1985-02-23 1985-08-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-08-24 1989-02-23 1989-08-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-08-24 1993-02-23 1993-08-25 $7700.00 Window Closed / Lapsed