US4278629A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Preparation of padded articles
Assignee: Storey Brothers and Co Ltd
•
Filing: 1979-06-18
•
Granted: 1981-07-14
•
Expires: 1999-06-18
Abstract
Abstract A method of preparing a cushion or like padded article comprising a plasticized vinyl chloride polymer cover filled with foam in which the cover is shaped and the foam prepared in situ within the cover, wherein a superior bond between the cover and foam is achieved by coating the interior surface of the cover prior to foaming with a primer composition comprising: (A) a latex of butadiene-acrylonitrile copolymer containing a hydroxyl or carboxyl group; and (B) a latex chosen from the group consisting of natural rubber, styrene-butadiene latex and mixtures thereof in an amount sufficient to promote bonding and wherein the weight ratio of (A) and (B) is from 4:1 to 1:4.
Inventors
- 👤 Peter S. Bennett
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 12:00
CPC Classifications
C; C09; C09J; C09J131/00; C09J131/02; C09J131/04; C09J121/00; C09J121/02; C09J133/00; C09J133/04; C09J133/06; C09J133/08; C08; C08L; C08L2666/00; C08L2666/02; C08L2666/04; Y; Y10; Y10T; Y10T428/00; Y10T428/249921; Y10T428/249953; Y10T428/249982; Y10T428/249985; Y10T428/249987; Y10T428/249991; Y10T428/249992; Y10T428/31504; Y10T428/31551; Y10T428/31569; Y10T428/31573; Y10T428/31855; Y10T428/31931
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
170 words
A method of preparing a resilient padded article comprising the steps of (a) shaping a sheet of plasticized vinyl chloride polymer by vacuum forming to provide a shaped cover, (b) holding said cover in a female mould, (c) placing within said cover the precursors of a polyurethane foam, (d) allowing said precursors to foam and fill said cover to provide a resilient foam filling, said foam being bonded to said cover and retaining said cover in the required shape, wherein the surface of said sheet which is to be in contact with said foam is treated at any time before step (c) and substantially in the absence of organic solvent with an aqueous primer composition comprising: (A) a latex of butadiene-acrylonitrile copolymer containing a carboxyl group; and (B) a latex chosen from the group consisting of natural rubber, styrene-butadiene latex and mixtures thereof in an amount sufficient to promote bonding and wherein the weight ratio of (A) and (B) is from 4:1 to 1:4, and the treated surface is dried.
Claim 2
Independent Claim
170 words
A method of preparing a resilient padded article comprising the steps of (a) shaping a sheet of plasticized vinyl chloride polymer by vacuum forming to provide a shaped cover, (b) holding said cover in a female mould, (c) placing within said cover the precursors of a polyurethane foam, (d) allowing said precursors to foam and fill said cover to provide a resilient foam filling, said foam being bonded to said cover and retaining said cover in the required shape, wherein the surface of said sheet which is to be in contact with said foam is treated at any time before step (c) and substantially in the absence of organic solvent with an aqueous primer composition comprising: (A) a latex of butadiene-acrylonitrile copolymer containing a carboxyl group; and (B) a latex chosen from the group consisting of natural rubber, styrene-butadiene latex and mixtures thereof in an amount sufficient to promote bonding and wherein the weight ratio of (A) and (B) is from 4:1 to 1:4, and the treated surface is dried.
Claim 3
Dependent Claim
20 words
The method of claim 1 wherein in said priming composition the weight ratio of (A) to (B) is about 1:1.
Claim 4
Dependent Claim
47 words
The method of claim 1 wherein said aqueous priming composition comprises in relative parts by weight 10 parts wetting agent, 20 parts thickener/stabilizer, 100 parts water, 100 parts styrene-butadiene latex, 50 parts carboxylic modified butadiene high acrylonitrile latex and 50 parts carboxylic modified butadiene medium acrylonitrile latex.
Claim 5
Dependent Claim
24 words
The method of claim 1 wherein said aqueous priming composition is applied to said sheet of vinyl chloride polymer prior to shaping said sheet.
References Cited (Backward Citations)
US3075863A
Cited
US3382138A
Cited
US3502542A
Cited
US3528848A
Cited
US3729370A
Cited
US3911190A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-07-13 | 1985-01-12 | 1985-07-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-07-13 | 1989-01-12 | 1989-07-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-07-13 | 1993-01-12 | 1993-07-14 | $7700.00 | Window Closed / Lapsed |