Antistatic agents, synthesis and use thereof
Assignee: SK Discovery Co Ltd
•
Filing: 1980-01-14
•
Granted: 1981-07-07
•
Expires: 2000-01-14
Abstract
Abstract Polyester fibers having excellent antistatic properties are produced by incorporating therein a novel antistatic agent synthesized by partially esterifying a dimetallic salt with a polyalkylene glycol.
Inventors
- 👤 Sam Kwon Choi
- 👤 Kee Dong Lee
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 16:42
CPC Classifications
C; C08; C08G; C08G79/00; C08G63/00; C08G63/66; C08G63/668; C08G63/672; C08G63/68; C08G63/681; C08G65/00; C08G65/02; C08G65/32; C08G65/329; C08G65/331; C08G65/332; C08G65/3322; C08L; C08L67/00; C08L67/02
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
167 words
A process for the manufacture of an antistatic agent useful for the manufacture of an antistatic polyester fiber which comprises: (i) reacting about one mole of a dimetallic compound selected from the group consisting of compounds of Be, Mg, Ca, Sr, Ba, Zn and Cd and about two moles of same or different acyl compounds having the structural formula of: ##STR11## wherein (1) X's, which may be either identical or different, are selected from the group consisting of (a) HO--, (b) NH 2 --, (c) OHSO 3 --and (d) Cl--, Br--, or I--; (2) R is selected from the group consisting of (a)--(CH 2 ) n --, wherein n is an integer ranging from 1 to 8, (b)--(HC═CH) k --, wherein k is either 1 or 2, (c)--(C.tbd.C)--, ##STR12## (ii) reacting the product formed in step (i) above with a polyalkylene glycol having the structural formula of ##STR13## where p is a number ranging from about 10 to about 1,500 and m is either 2 or 3.
Claim 2
Dependent Claim
167 words
A process for the manufacture of an antistatic agent useful for the manufacture of an antistatic polyester fiber which comprises: (i) reacting about one mole of a dimetallic compound selected from the group consisting of compounds of Be, Mg, Ca, Sr, Ba, Zn and Cd and about two moles of same or different acyl compounds having the structural formula of: ##STR11## wherein (1) X's, which may be either identical or different, are selected from the group consisting of (a) HO--, (b) NH 2 --, (c) OHSO 3 --and (d) Cl--, Br--, or I--; (2) R is selected from the group consisting of (a)--(CH 2 ) n --, wherein n is an integer ranging from 1 to 8, (b)--(HC═CH) k --, wherein k is either 1 or 2, (c)--(C.tbd.C)--, ##STR12## (ii) reacting the product formed in step (i) above with a polyalkylene glycol having the structural formula of ##STR13## where p is a number ranging from about 10 to about 1,500 and m is either 2 or 3.
Claim 3
Dependent Claim
203 words
A process for the manufacture of an antistatic polyester fiber which comprises: (a) preparing a master chip polyester by reacting an antistatic agent having the structural formula of: ##STR14## wherein (1) X is selected from the group consisting of (a) HO--, (b) NH 2 --, (c) OHSO 3 --, and (c) Cl--, Br--, or I--; (2) X 1 's, which can be either identical or different, are selected from the group consisting of (a)--O--, (b)--NH--, and (c)--SO 3 --; (3) R's, which can be either identical or different, are selected from the group consisting of (a)--(CH 2 ) n -- where n is an integer ranging from 1 to 8, (b)--(HC═CH) k where k is either 1 or 2, (c)--(C═C)--, ##STR15## (4) R 1 is a polyalkylene glycol radical having the structural representation of ##STR16## where p is a number ranging from about 10 to about 1,500 and m is either 2 or 3; and (5) M is a divalent metal selected from the group consisting of Be, Mg, Ca, Sr, Ba, Zn and Cd with a common polyester; and thereafter, (b) blending said master chip polyester defined in step (a) above with a common polyester, therby to produce said antistatic polyester fiber.
Claim 4
Dependent Claim
203 words
A process for the manufacture of an antistatic polyester fiber which comprises: (a) preparing a master chip polyester by reacting an antistatic agent having the structural formula of: ##STR14## wherein (1) X is selected from the group consisting of (a) HO--, (b) NH 2 --, (c) OHSO 3 --, and (c) Cl--, Br--, or I--; (2) X 1 's, which can be either identical or different, are selected from the group consisting of (a)--O--, (b)--NH--, and (c)--SO 3 --; (3) R's, which can be either identical or different, are selected from the group consisting of (a)--(CH 2 ) n -- where n is an integer ranging from 1 to 8, (b)--(HC═CH) k where k is either 1 or 2, (c)--(C═C)--, ##STR15## (4) R 1 is a polyalkylene glycol radical having the structural representation of ##STR16## where p is a number ranging from about 10 to about 1,500 and m is either 2 or 3; and (5) M is a divalent metal selected from the group consisting of Be, Mg, Ca, Sr, Ba, Zn and Cd with a common polyester; and thereafter, (b) blending said master chip polyester defined in step (a) above with a common polyester, therby to produce said antistatic polyester fiber.
References Cited (Backward Citations)
US3288175A
Cited
US3582448A
Cited
US3702350A
Cited
US3755497A
Cited
US3962185A
Cited
US3963803A
Cited
US4211859A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-07-06 | 1985-01-05 | 1985-07-07 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-07-06 | 1989-01-05 | 1989-07-07 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-07-06 | 1993-01-05 | 1993-07-07 | $7700.00 | Window Closed / Lapsed |