US4273885A Expired / Lapsed US ⏱️ 0.0 years remaining

Novel catalyst system for RIM elastomers

Assignee: Huntsman Corp
•
Filing: 1980-04-01
•
Granted: 1981-06-16
•
Expires: 2000-04-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The invention is a method for making reaction injection molded polyurethane of improved properties. The product comprises the reaction product of a high molecular weight polyhydric polyether, a low molecular weight active hydrogen containing compound of at least two functionality, a polyisocyanate and a catalyst combination comprising a weak tertiary amine, a fast gelation organo tin compound and a delayed action organo tin catalyst. This catalyst combination results in improved processing, a minimum of surface defects and excellent green strength. Reaction injection molded elastomers are useful as molded articles of commerce including, but not limited to, vehicle body parts.

Inventors

  • 👤 Richard J. G. Dominguez
  • 👤 Doris M. Rice

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 16:52
CPC Classifications
C; C08; C08G; C08G18/00; C08G18/06; C08G18/08; C08G18/16; C08G18/161; C08G18/163; C08G18/165; C08G18/28; C08G18/65; C08G18/66; C08G18/6666; C08G18/667; C08G2120/00

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 76 words
In a method for making a polyurethane elastomer of significantly improved properties wherein an aromatic polyisocyanate, a polyol of above about 500 equivalent weight, a chain extending agent comprising a low molecular weight active hydrogen containing compound of at least 2 functionality and a catalyst system is injected via a RIM machine into a mold cavity of the desired configuration the improvement which comprises using as the catalyst system dimorpholinodiethylether, dibutyltin dilaurate and an alkyltin mercaptide.
Claim 2
Dependent Claim 76 words
In a method for making a polyurethane elastomer of significantly improved properties wherein an aromatic polyisocyanate, a polyol of above about 500 equivalent weight, a chain extending agent comprising a low molecular weight active hydrogen containing compound of at least 2 functionality and a catalyst system is injected via a RIM machine into a mold cavity of the desired configuration the improvement which comprises using as the catalyst system dimorpholinodiethylether, dibutyltin dilaurate and an alkyltin mercaptide.
Claim 3
Dependent Claim 22 words
A method as in claim 1 wherein the polyol comprises a polyether of about 5000 molecular weight based on a trihydric initiator.
Claim 4
Dependent Claim 12 words
A method as in claim 1 wherein the polyisocyanate comprises 4,4'diphenylmethane diisocyanate.
Claim 5
Dependent Claim 15 words
A method as in claim 1 wherein the elastomer is postcured at about 325° F.

References Cited (Backward Citations)

US3397158A Cited
US4048105A Cited
US4150212A Cited
US4115321A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-06-15 1984-12-15 1985-06-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-06-15 1988-12-15 1989-06-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-06-15 1992-12-15 1993-06-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag