US4269397A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for measuring the thickness of a refractory in a metallurgical apparatus

Assignee: Bethlehem Steel Corp
•
Filing: 1980-07-07
•
Granted: 1981-05-26
•
Expires: 2000-07-07
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for measuring the thickness of a refractory laid-up against the interior surface of the steel shell of a metallurgical apparatus includes placing at least one monitoring device in a critical wear area of the apparatus in a manner such that the free end of the device is at a known distance from the hot face of the refractory and the confined end extends beyond the outer surface of the steel shell. The device is connected to an electronic time-domain reflectometer by electrical connecting means. Timed pulses are generated and impressed in the device by the instrument and reflections of the pulses are received by and are visually displayed on the reflectometer. The length of the device appears on the display as a straight line bounded by two inflections. The straight line is indicative of the thickness of the refractory. The device includes a metallic conductor coaxial with an outer metallic sheath and separated therefrom by a refractory having a desired dielectric constant. The device has a free end and a confined end. The confined end may be contained in a junction box provided with electrical connecting means. Electric insulating packing may be used in the junction box.

Inventors

  • 👤 Robert A. Strimple
  • 👤 Joseph E. Snyder
  • 👤 Bruce F. Shoemaker

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 12:32
CPC Classifications
C; C21; C21B; C21B7/00; C21B7/24; F; F27; F27D; F27D21/00; F27D21/0021

Claims Analysis

Total Claims: 28
Claim 1
Independent Claim 238 words
In an improved method for measuring the thickness of a refractory laid-up against the interior surface of the steel shell of a metallurgical apparatus comprising: (a) placing at least one monitoring device of predetermined length comprised of a central metallic conductor coaxial with a metallic sheath and spaced therefrom by a closely packed pulverulent refractory, the device having a free end and a confined end, both being substantially flat surfaces, the confined end being connected to an electrical connector means, such that the free end is at a known predetermined distance from the hot face of the refractory and the confined end extends a known distance beyond the steel shell, (b) connecting the confined end by means of the connector means to an electronic instrument capable of generating and impressing fast-rise timed pulses in the device and receiving and displaying pulses reflected by physical features of the device, (c) adjusting the length of the device on the display using reflected pulses appearing as an inflection from the confined end as a reference point, the reflected pulses along the length of the device appearing as a substantially straight line and the reflected pulses from the free end appearing as an inflection and showing the termination of the device, (d) sending timed pulses through the device and displaying the reflected pulses, and (e) determining the thickness of the refractory from the length of the straight line displayed on the instrument.
Claim 2
Dependent Claim 238 words
In an improved method for measuring the thickness of a refractory laid-up against the interior surface of the steel shell of a metallurgical apparatus comprising: (a) placing at least one monitoring device of predetermined length comprised of a central metallic conductor coaxial with a metallic sheath and spaced therefrom by a closely packed pulverulent refractory, the device having a free end and a confined end, both being substantially flat surfaces, the confined end being connected to an electrical connector means, such that the free end is at a known predetermined distance from the hot face of the refractory and the confined end extends a known distance beyond the steel shell, (b) connecting the confined end by means of the connector means to an electronic instrument capable of generating and impressing fast-rise timed pulses in the device and receiving and displaying pulses reflected by physical features of the device, (c) adjusting the length of the device on the display using reflected pulses appearing as an inflection from the confined end as a reference point, the reflected pulses along the length of the device appearing as a substantially straight line and the reflected pulses from the free end appearing as an inflection and showing the termination of the device, (d) sending timed pulses through the device and displaying the reflected pulses, and (e) determining the thickness of the refractory from the length of the straight line displayed on the instrument.
Claim 3
Dependent Claim 45 words
The method of claim 1 in which the central conductor in the monitor device is at least one metal taken from the group consisting of stainless steel, molybdenum, iron, platinum tungsten, and nickel base alloy containing manganese and aluminum and nickel base alloys containing chromium.
Claim 4
Dependent Claim 12 words
The method of claim 2 in which the electrical conductor is molybdenum.
Claim 5
Dependent Claim 27 words
The method of claim 1 in which the sheath of the device is at least one metal taken from the group consisting of stainless steel and molybdenum.
Claim 6
Dependent Claim 39 words
The method of claim 4 in which the conductor of the device is at least one metal taken from the group consisting of metal base alloys containing chromium and molybdenum and the sheath of the device is stainless steel.
Claim 7
Dependent Claim 39 words
The method of claim 1 in which the electrically insulating refractory material of the device is at least one refractory taken from the group consisting of: high purity alumina, mullite, sillimanite, chromite, lime, magnesia, calcined dolomite, silica and zirconia.
Claim 8
Dependent Claim 19 words
The method of claim 6 in which the electrically insulating refractory material of the device is high purity alumina.
Claim 9
Dependent Claim 17 words
The method of claim 6 in which the electrically insulating refractory material of the device is magnesia.
Claim 10
Dependent Claim 19 words
The method of claim 5 in which the electrically insulating refractory material of the device is high purity alumina.
Claim 11
Dependent Claim 17 words
The method of claim 5 in which the electrically insulating refractory material of the device is magnesia.
Claim 12
Dependent Claim 26 words
The method of claim 1 in which at least one of the monitoring devices is laid-up in the refractory in the interior of a blast furnace.
Claim 13
Dependent Claim 26 words
The method of claim 1, in which at least one of the monitoring devices is laid-up in the refractory in the interior of an electric furnace.
Claim 14
Dependent Claim 27 words
The method of claim 1, in which at least one of the monitoring devices is laid-up in the refractory in the interior of a basic oxygen furnace.
Claim 15
Dependent Claim 291 words
In an improved method for measuring the thickness of a refractory laid-up against the interior surface of the steel shell of a metallurgical apparatus comprising: (a) placing at least one monitoring device of predetermined length comprised of a central metallic conductor coaxial with a metallic sheath and spaced therefrom by a closely packed pulverulent refractory, the device having a free end and a confined end, both being substantially flat surfaces, the confined end is contained in a junction box packed with an insulating material having a desired dielectric constant and is connected to an electrical connector means attached to the junction box, the conductor and sheath being separated by a material having a known dielectric constant in the junction box and being separated by the refractory at the free end of the device, such that the free end is at a known predetermined distance from the hot face of the refractory and the confined end extends a known distance beyond the steel shell, (b) connecting the confined end by means of the connector means to an electronic instrument capable of generating and impressing fast-rise timed pulses in the device and receiving and displaying pulses reflected by physical features of the device, (c) adjusting the length of the device on the display using reflected pulses appearing as an inflection from the confined end as a reference point, the reflected pulses along the length of the device appearing as a substantially straight line and the reflected pulses from the free end appearing as an inflection and showing the termination of the device, (d) sending timed pulses through the device and displaying the reflected pulses, and (e) determining the thickness of the refractory from the length of the straight line displayed on the instrument.
Claim 16
Dependent Claim 291 words
In an improved method for measuring the thickness of a refractory laid-up against the interior surface of the steel shell of a metallurgical apparatus comprising: (a) placing at least one monitoring device of predetermined length comprised of a central metallic conductor coaxial with a metallic sheath and spaced therefrom by a closely packed pulverulent refractory, the device having a free end and a confined end, both being substantially flat surfaces, the confined end is contained in a junction box packed with an insulating material having a desired dielectric constant and is connected to an electrical connector means attached to the junction box, the conductor and sheath being separated by a material having a known dielectric constant in the junction box and being separated by the refractory at the free end of the device, such that the free end is at a known predetermined distance from the hot face of the refractory and the confined end extends a known distance beyond the steel shell, (b) connecting the confined end by means of the connector means to an electronic instrument capable of generating and impressing fast-rise timed pulses in the device and receiving and displaying pulses reflected by physical features of the device, (c) adjusting the length of the device on the display using reflected pulses appearing as an inflection from the confined end as a reference point, the reflected pulses along the length of the device appearing as a substantially straight line and the reflected pulses from the free end appearing as an inflection and showing the termination of the device, (d) sending timed pulses through the device and displaying the reflected pulses, and (e) determining the thickness of the refractory from the length of the straight line displayed on the instrument.
Claim 17
Dependent Claim 45 words
The method of claim 14 in which the central conductor in the monitor device is at least one metal taken from the group consisting of stainless steel, molybdenum, iron, platinum, tungsten, and nickel base alloy containing manganese and aluminum and nickel base alloys containing chromium.
Claim 18
Dependent Claim 12 words
The method of claim 15 in which the electrical conductor is molybdenum.
Claim 19
Dependent Claim 27 words
The method of claim 14 in which the sheath of the device is at least one metal taken from the group consisting of stainless steel and molybdenum.
Claim 20
Dependent Claim 39 words
The method of claim 17 in which the conductor of the device is at least one metal taken from the group consisting of molybdenum and nickel base alloys containing chromium and the sheath of the device is stainless steel.
Claim 21
Dependent Claim 39 words
The method of claim 14 in which the electrically insulating refractory material of the device is at least one refractory taken from the group consisting of: high purity alumina, mullite, sillimanite, chromite, lime magnesia, calcined dolomite, silica and zirconia.
Claim 22
Dependent Claim 19 words
The method of claim 19 in which the electrically insulating refractory material of the device is high purity alumina.
Claim 23
Dependent Claim 17 words
The method of claim 19 in which the electrically insulating refractory material of the device is magnesia.
Claim 24
Dependent Claim 19 words
The method of claim 18 in which the electrically insulating refractory material of the device is high purity alumina.
Claim 25
Dependent Claim 17 words
The method of claim 18 in which the electrically insulating refractory material of the device is magnesia.
Claim 26
Dependent Claim 26 words
The method of claim 14 in which at least one of the monitoring devices is laid-up in the refractory in the interior of a blast furnace.
Claim 27
Dependent Claim 26 words
The method of claim 14 in which at least one of the monitoring devices is laid-up in the refractory in the interior of an electric furnace.
Claim 28
Dependent Claim 27 words
The method of claim 14 in which at least one of the monitoring devices is laid-up in the refractory in the interior of a basic oxygen furnace.

References Cited (Backward Citations)

FR839393A Cited
US2805272A Cited
US3018663A Cited
US2915305A Cited
US3015950A Cited
FR1431629A Cited
US3307401A Cited
DE1950939A1 Cited
US3836402A Cited
US3938385A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-05-25 1984-11-24 1985-05-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-05-25 1988-11-24 1989-05-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-05-25 1992-11-24 1993-05-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag