Lightweight laminated photochromic lenses
Assignee: Corning Glass Works
•
Filing: 1979-03-07
•
Granted: 1981-05-19
•
Expires: 1999-03-07
Abstract
Abstract A photochromic glass/plastic laminated lens of improved physical durability comprising a buried layer of photochromic glass, surface layers of optically clear plastic, and adhesive bonding layers of high strength but low elastic modulus between the buried glass and plastic surface layers, is described.
Inventors
- 👤 Suresh T. Gulati
- 👤 Norman A. Smith
- 👤 Anton A. Spycher
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 15:12
CPC Classifications
G; G02; G02C; G02C7/00; G02C7/10; G02C7/102; G02B; G02B5/00; G02B5/20; G02B5/22; G02B5/23; G02C2202/00; G02C2202/16
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
155 words
A curved glass-plastic laminated lens comprising a plastic front surface layer, a photochromic glass core, and a plastic back surface layer, each plastic surface layer being bonded to the glass core by an adhesive bonding layer, wherein: (a) the ratio of the thickness of the plastic front surface layer to the thickness of the plastic back surface layer is in the range of about 1:8 to 8:1 at all peripheral portions of the lens within about 2 lens thicknesses of the lens edge; (b) the plastic front and back surface layers are composed of a polymerized allyl diglycol carbonate resin; and (c) each adhesive bonding layer is composed of an adhesive having a tensile strength of at least about 4000 psi and a shear strength of at least about 2000 psi, and comprises a region at least about 0.002 inches in thickness wherein the elastic modulus of the adhesive does not exceed about 10,000 psi.
Claim 2
Dependent Claim
155 words
A curved glass-plastic laminated lens comprising a plastic front surface layer, a photochromic glass core, and a plastic back surface layer, each plastic surface layer being bonded to the glass core by an adhesive bonding layer, wherein: (a) the ratio of the thickness of the plastic front surface layer to the thickness of the plastic back surface layer is in the range of about 1:8 to 8:1 at all peripheral portions of the lens within about 2 lens thicknesses of the lens edge; (b) the plastic front and back surface layers are composed of a polymerized allyl diglycol carbonate resin; and (c) each adhesive bonding layer is composed of an adhesive having a tensile strength of at least about 4000 psi and a shear strength of at least about 2000 psi, and comprises a region at least about 0.002 inches in thickness wherein the elastic modulus of the adhesive does not exceed about 10,000 psi.
Claim 3
Dependent Claim
22 words
A curved laminated lens in accordance with claim 1 wherein the thickness of the glass core does not exceed about 0.025 inches.
Claim 4
Dependent Claim
24 words
A curved laminated lens in accordance with claim 2 wherein the thickness of the glass core is in the range of about 0.010-0.020 inches.
Claim 5
Dependent Claim
38 words
A curved laminated lens in accordance with claim 1 wherein the ratio of the thickness of the plastic front surface layer to the thickness of the plastic back surface layer is in the range of 1:8 to 1:1.
Claim 6
Dependent Claim
32 words
A curved laminated lens in accordance with claim 1 wherein the adhesive bonding layer comprises a region at least 0.005 inches in thickness wherein the elastic modulus does not exceed 10,000 psi.
Claim 7
Dependent Claim
20 words
A curved laminated lens in accordance with claim 1 wherein the adhesive bonding layer is composed of a polyurethane adhesive.
Claim 8
Dependent Claim
21 words
A curved laminated lens in accordance with claim 1 wherein the adhesive bonding layer is composed of a polyvinyl butyral adhesive.
Claim 9
Dependent Claim
23 words
A curved laminated lens in accordance with claim 1 which has a front and back surface curvature in the range of 6-8 diopters.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-05-18 | 1984-11-17 | 1985-05-19 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-05-18 | 1988-11-17 | 1989-05-19 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-05-18 | 1992-11-17 | 1993-05-19 | $7700.00 | Window Closed / Lapsed |