Preparation of aqueous polyacrylate dispersions having improved flow characteristics
Assignee: BASF SE
•
Filing: 1979-09-07
•
Granted: 1981-05-05
•
Expires: 1999-09-07
Abstract
Abstract Aqueous polyacrylate dispersions having improved flow characteristics are prepared by polymerizing esters of acrylic acid and/or methacrylic acid and alkanols of 1 to 10 carbon atoms, with or without admixture of styrene and/or vinyl esters and/or water-soluble monoolefinically unsaturated comonomers (the monomer feed being in the form of an emulsion), in aqueous emulsion in the presence of a free radical polymerization initiator, a protective colloid, a nonionic emulsifier and a regulator, at least a part of the protective colloid being introduced into an aqueous initial charge, and a water-soluble regulator being employed in the initial charge and in the feed.
Inventors
- 👤 Rudolf Mueller-Mall
- 👤 Kurt Wendel
- 👤 Hans J. Geelhaar
- 👤 Michael Melan
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 21:39
CPC Classifications
C; C08; C08F; C08F20/00; C08F20/02; C08F20/10; C08F20/12; C08F2/00; C08F2/38
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
171 words
In a process for the preparation of aqueous polyacrylate dispersions having improved flow characteristics by emulsion polymerizing at least 20 weight % of an ester of acrylic acid and/or methacrylic acid and an alkanol of 1 to 10 carbon atoms at from 30° to 95° C. in the presence of a free radical polymerization inhibitor, a protective colloid, from 0.5 to 5% by weight of a nonionic emulsifier and a molecular weight regulator, the percentages by weight each being based on the total amount of monomer, the improvement which comprises: admixing at least a portion of the protective colloid present in a total amount of 0.05 to 1.5% by weight and a portion of the water soluble molecular weight regulator present in a total amount of 0.1 to 0.5% by weight with from 10-30 weight % of the total number to form an initial charge, and admixing the remainder of the monomer and of the said water-soluble molecular weight regulator and any remainder of the protective colloid with said initial charge.
Claim 2
Dependent Claim
171 words
In a process for the preparation of aqueous polyacrylate dispersions having improved flow characteristics by emulsion polymerizing at least 20 weight % of an ester of acrylic acid and/or methacrylic acid and an alkanol of 1 to 10 carbon atoms at from 30° to 95° C. in the presence of a free radical polymerization inhibitor, a protective colloid, from 0.5 to 5% by weight of a nonionic emulsifier and a molecular weight regulator, the percentages by weight each being based on the total amount of monomer, the improvement which comprises: admixing at least a portion of the protective colloid present in a total amount of 0.05 to 1.5% by weight and a portion of the water soluble molecular weight regulator present in a total amount of 0.1 to 0.5% by weight with from 10-30 weight % of the total number to form an initial charge, and admixing the remainder of the monomer and of the said water-soluble molecular weight regulator and any remainder of the protective colloid with said initial charge.
Claim 3
Dependent Claim
25 words
The process of claim 1, wherein said water-soluble molecular weight regulator is admixed with said initial charge in increasing amount as a function of time.
Claim 4
Dependent Claim
84 words
The process of claim 1, wherein said monomer additionally contains from 0-50% by weight styrene, 0-20% by weight vinyl ester and 0-10% by weight of a water-soluble monoolefinically unsaturated co-monomer selected from the group consisting of an α,β-monoolefinically unsaturated monocarboxylic acid, an α,β-monoolefinically unsaturated dicarboxylic acid, an amide of said monocarboxylic acid or said dicarboxylic acid, the nitrogen atom(s) of said amide optionally being substituted, a monoalkyl ester of said dicarboxylic acid, a vinyl sulfonic acid and water-soluble salts of said vinyl sulfonic acid.
Claim 5
Dependent Claim
25 words
The process of claim 1, wherein said protective colloid is selected from the group consisting of carboxymethylcellulose, hydroxyethylcellulose, polyvinyl alcohol, and water-soluble N-vinyl pyrrolidone polymers.
Claim 6
Dependent Claim
31 words
The process of claim 1, wherein said molecular weight regulator is selected from the group consisting of thioglycolic acid, thiodiglycol, but-1-ene-3-ol, isopropanol, vinylglycol, cyclohexylamine hydrochloride, hydroxylammonium sulfate, but-2-ene-1,4-diol and thiodiacetic acid.
Claim 7
Dependent Claim
41 words
The process of claim 1, wherein polymerization of said initial charge is initiated and thereafter the remainder of the monomer, water-soluble molecular weight regulator and protective colloid is continuously admixed with the initial charge at the rate at which polymerization proceeds.
Claim 8
Dependent Claim
31 words
The process of claim 1, wherein about half of the protective colloid is admixed in forming the initial charge and the remainder is added subsequently with the remainder of the monomer.
Claim 9
Dependent Claim
9 words
The product produced by the process of claim 1.
References Cited (Backward Citations)
GB912068A
Cited
US3248356A
Cited
US3513120A
Cited
US3546154A
Cited
GB1152860A
Cited
GB1277877A
Cited
US3876596A
Cited
GB1466660A
Cited
US4039500A
Cited
GB1524018A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-05-04 | 1984-11-03 | 1985-05-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-05-04 | 1988-11-03 | 1989-05-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-05-04 | 1992-11-03 | 1993-05-05 | $7700.00 | Window Closed / Lapsed |