← Back to Patent Explorer
US4265407A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of producing a coal-water slurry of predetermined consistency

Assignee: Texaco Inc
•
Filing: 1979-07-13
•
Granted: 1981-05-05
•
Expires: 1999-07-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of producing a thick slurry of powdered coal and water. It includes feeding less coal than is required for the thick slurry into a ball mill, and introducing all of the water required so that a thin slurry is produced. The remaining coal required is pulverized in a dry grinder, and the thin slurry and dry powdered coal are mixed to produce the desired thick slurry.

Inventors

  • 👤 Richard V. Kessler
  • 👤 Roger J. Corbeels

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 13:27
CPC Classifications
C; C10; C10L; C10L1/00; C10L1/32; C10L1/326

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 104 words
Efficient method of preparing a coal and water slurry having a predetermined thickness from mined coal and a predetermined total quantity of water, comprising the steps of, feeding less of said mined coal than required for said slurry into a ballmill, introducing said total quantity of water required for said slurry into said ballmill to produce a relatively thin powdered coal slurry, grinding the remaining quantity of said mined coal required for said slurry in a dry grinder to produce dry powdered coal, and mixing said thin slurry with said dry powdered coal to produce said coal and water slurry having a predetermined thickness.
Claim 2
Dependent Claim 104 words
Efficient method of preparing a coal and water slurry having a predetermined thickness from mined coal and a predetermined total quantity of water, comprising the steps of, feeding less of said mined coal than required for said slurry into a ballmill, introducing said total quantity of water required for said slurry into said ballmill to produce a relatively thin powdered coal slurry, grinding the remaining quantity of said mined coal required for said slurry in a dry grinder to produce dry powdered coal, and mixing said thin slurry with said dry powdered coal to produce said coal and water slurry having a predetermined thickness.
Claim 3
Dependent Claim 11 words
Efficient method according to claim 1, wherein said steps are continuous.
Claim 4
Dependent Claim 32 words
Efficient method according to claim 2, wherein said step of feeding less of said mined coal comprises regulating said less mined coal to produce an easily pumpable relatively thin powdered coal slurry.
Claim 5
Dependent Claim 159 words
Efficient method of preparing a coal and water slurry having a high percentage solids from mined coal and a predetermined total amount of water, comprising continuously feeding a regulated amount of said mined coal into a ballmill being less than necessary for said high percentage solids slurry, continuously introducing said total amount of water into said ballmill required to produce said high percentage solids slurry to produce an easily pumpable relatively thin powdered coal and water slurry, pumping said thin slurry to a holding container, holding said thin slurry for controlled delivery to a mixer, continuously grinding another regulated amount of said mined coal in a dry grinder to produce dry powdered coal, delivering said dry powdered coal to a silo for temporary storage, continuously delivering a regulated amount of said dry powdered coal to said mixer, and mixing said thin slurry and said dry powdered coal to form said coal and water slurry having said high percentage solids.
Claim 6
Dependent Claim 159 words
Efficient method of preparing a coal and water slurry having a high percentage solids from mined coal and a predetermined total amount of water, comprising continuously feeding a regulated amount of said mined coal into a ballmill being less than necessary for said high percentage solids slurry, continuously introducing said total amount of water into said ballmill required to produce said high percentage solids slurry to produce an easily pumpable relatively thin powdered coal and water slurry, pumping said thin slurry to a holding container, holding said thin slurry for controlled delivery to a mixer, continuously grinding another regulated amount of said mined coal in a dry grinder to produce dry powdered coal, delivering said dry powdered coal to a silo for temporary storage, continuously delivering a regulated amount of said dry powdered coal to said mixer, and mixing said thin slurry and said dry powdered coal to form said coal and water slurry having said high percentage solids.

References Cited (Backward Citations)

US2421648A Cited
US2826370A Cited
US3606173A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-05-04 1984-11-03 1985-05-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-05-04 1988-11-03 1989-05-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-05-04 1992-11-03 1993-05-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag