Aqueous dispersion coating composition and application to molded articles

Assignee: PPG Industries Ohio Inc
•
Filing: 1979-07-23
•
Granted: 1981-04-21
•
Expires: 1999-07-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract PCT No. PCT/US79/00526 Sec. 371 Date July 23, 1979 Sec. 102(e) Date July 23, 1979 PCT Filed July 23, 1979 PCT Pub. No. WO81/00096 PCT Pub. Date Jan. 22, 1981 Described is an aqueous dispersion coating composition consisting essentially of an epoxy powder paint and a water carrier wherein the water has dissolved therein a water soluble nonionic surfactant in an amount ranging from about 0.01 to about 10% by weight (PBW) of the dry epoxy material and a dispersing agent in an amount from about 0.01 to 10 PBW of the dry epoxy material, wherein the pigment volume concentration of the coating composition is at least 10. Also described is a method of coating formed fiber reinforced plastics, such as sheet molding compound.

Inventors

  • 👤 Thomas F. Kaltenbach
  • 👤 John G. Martyn

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 17:57
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/02; C08J3/03; C08J3/05; C08G; C08G18/00; C08G18/06; C08G18/28; C08G18/40; C08G18/58; C08G59/00; C08G59/18; C08G59/40; C08G59/4007; C08G59/4014; C08G59/4028; C09; C09D; C09D163/00; C08J2363/00

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 77 words
An aqueous dispersion coating composition consisting essentially of an epoxy powder paint and a water carrier wherein the water carrier has dissolved therein a water soluble nonionic surfactant in an amount ranging from about 0.01 to about 10% by weight (PBW) of the dry epoxy material and a dispersing agent in an amount from about 0.01 to 10 PBW of the dry epoxy material, wherein the pigment volume concentration of the coating composition is at least 10.
Claim 2
Dependent Claim 77 words
An aqueous dispersion coating composition consisting essentially of an epoxy powder paint and a water carrier wherein the water carrier has dissolved therein a water soluble nonionic surfactant in an amount ranging from about 0.01 to about 10% by weight (PBW) of the dry epoxy material and a dispersing agent in an amount from about 0.01 to 10 PBW of the dry epoxy material, wherein the pigment volume concentration of the coating composition is at least 10.
Claim 3
Dependent Claim 15 words
The coating composition of claim 1 wherein the nonionic surfactant is an organic phosphate type.
Claim 4
Dependent Claim 16 words
The coating composition of claim 2 wherein the dispersing agent is an anionic polymeric dispersing agent.
Claim 5
Dependent Claim 16 words
The composition of claim 3 wherein the anionic dispersing agent is an acrylic acid containing composition.
Claim 6
Dependent Claim 17 words
The composition of claim 1 wherein the powder paint contains a cross-linking agent for an epoxy resin.
Claim 7
Dependent Claim 13 words
The composition of claim 5 wherein the cross-linking agent is a blocked isocyanate.
Claim 8
Dependent Claim 42 words
A method of coating formed fiber reinforced plastics comprising the steps; 1. applying an aqueous dispersion coating composition of claim 1 to the fiber reinforced plastic; 2. flashing off the water from the applied dispersion composition; and 3. curing the coating composition.
Claim 9
Dependent Claim 18 words
The method of claim 7 wherein the flashing off occurs at a temperature between 100° and 212° F.
Claim 10
Dependent Claim 31 words
The method of claim 8 wherein the curing occurs at a temperature from about 250° to about 400° F. for a period of time ranging from about 10 to 60 minutes.
Claim 11
Dependent Claim 15 words
The method of claim 7 wherein the formed fiber reinforced plastic is sheet molding compound.
Claim 12
Dependent Claim 13 words
The composition of claim 1 wherein the pigment volume concentration is about 35.
Claim 13
Dependent Claim 18 words
The composition of claim 1 wherein the pH of the composition ranges from about 8 to about 12.
Claim 14
Dependent Claim 17 words
The method of claim 7 wherein the coating composition has a pigment volume concentration is about 35.
Claim 15
Dependent Claim 19 words
The method of claim 7 wherein the coating composition has a pH ranging from about 8 to about 12.

References Cited (Backward Citations)

GB878139A Cited
GB1122414A Cited
US3787230A Cited
US4081578A Cited
US4061618A Cited
US4026857A Cited
US4009133A Cited
US4122055A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-04-20 1984-10-20 1985-04-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-04-20 1988-10-20 1989-04-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-04-20 1992-10-20 1993-04-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag