US4263121A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method to fabricate polymeric membranes and diaphragms
Assignee: Dow Chemical Co
•
Filing: 1979-10-10
•
Granted: 1981-04-21
•
Expires: 1999-10-10
Abstract
Abstract A method is disclosed to fabricate shaped membranes or diaphragms with substantially leak-free seams suitable for use in electrolytic cells to produce a halogen and an alkali metal hydroxide. A preferred polymeric sheet material is formed into a desired configuration and a fusible substance is placed at or near the edges of the polymeric material prior to applying heat and, optionally, pressure to the fusible substance.
Inventors
- 👤 Marvin M. Christensen
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 22:55
CPC Classifications
C; C25; C25B; C25B13/00; C25B13/02
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
121 words
A method to fabricate a polymeric membrane or polymeric diaphragm for an electrolytic cell to produce a halogen and an alkali metal hydroxide from an aqueous alkali metal halide solution comprising: (a) placing a fusible substance on at least one surface portion of the polymeric material at or near at least one edge of the polymeric material, the fusible substance being more readily fusible than the polymeric material; (b) contacting the fusible substance with the same or a different polymeric material so as to form a configuration suitable to encase the working portion of an electrode for an electrolytic diaphragm cell; (c) heating the fusible substance sufficiently to form a substantially leak-free bond between the polymeric material and the fusible material.
Claim 2
Independent Claim
121 words
A method to fabricate a polymeric membrane or polymeric diaphragm for an electrolytic cell to produce a halogen and an alkali metal hydroxide from an aqueous alkali metal halide solution comprising: (a) placing a fusible substance on at least one surface portion of the polymeric material at or near at least one edge of the polymeric material, the fusible substance being more readily fusible than the polymeric material; (b) contacting the fusible substance with the same or a different polymeric material so as to form a configuration suitable to encase the working portion of an electrode for an electrolytic diaphragm cell; (c) heating the fusible substance sufficiently to form a substantially leak-free bond between the polymeric material and the fusible material.
Claim 3
Dependent Claim
23 words
The method of claim 1 wherein the heating is carried out at a temperature lower than the fusing temperature of the polymeric material.
Claim 4
Dependent Claim
21 words
The method of claim 2 wherein the heating is carried out at a temperature of about 490° to about 600° F.
Claim 5
Dependent Claim
11 words
The method of claim 1 wherein the polymeric material is polytetrafluoroethylene.
Claim 6
Dependent Claim
21 words
The method of claim 1 wherein the heating is carried out at a temperature of about 490° to about 600° F.
Claim 7
Independent Claim
35 words
The method of claims 1, 5 or 3 including applying a pressure of from about 5 to about 200 pounds per square inch gauge to that portion of the membrane to be bonded during heating.
Claim 8
Dependent Claim
123 words
An electrolytic cell for producing a halogen and an alkali metal hydroxide from an aqueous alkali metal halide solution comprising an anode and a cathode disposed in suitable compartments spaced apart by a polymeric membrane or polymeric diaphragm with one open end and at least a portion of the closed end having edge portions thermally bonded together by at least one fusible substance interposed between separate portions of the polymer material, the fusible substance being more readily fusible than the polymeric material, means to feed the solution to the cell, means to remove the gaseous halogen from the anode compartment, means to remove the alkali metal hydroxide from the cathode compartment and means to conduct an electric current to the anode and cathode.
Claim 9
Dependent Claim
123 words
An electrolytic cell for producing a halogen and an alkali metal hydroxide from an aqueous alkali metal halide solution comprising an anode and a cathode disposed in suitable compartments spaced apart by a polymeric membrane or polymeric diaphragm with one open end and at least a portion of the closed end having edge portions thermally bonded together by at least one fusible substance interposed between separate portions of the polymer material, the fusible substance being more readily fusible than the polymeric material, means to feed the solution to the cell, means to remove the gaseous halogen from the anode compartment, means to remove the alkali metal hydroxide from the cathode compartment and means to conduct an electric current to the anode and cathode.
Claim 10
Dependent Claim
22 words
The electrolytic cell of claim 7 wherein the bonded polymeric material is a pocket-like structure encasing the working portion of the cathode.
Claim 11
Dependent Claim
30 words
The electrolytic cell of claim 7 wherein the bonded polymeric material is a pocket-like structure with the bonded edges positioned at the upper and lower portions of the pocket-like structure.
Claim 12
Dependent Claim
14 words
The electrolytic cell of claims 7 or 9 wherein the polymeric material is polytetrafluoroethylene.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-04-20 | 1984-10-20 | 1985-04-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-04-20 | 1988-10-20 | 1989-04-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-04-20 | 1992-10-20 | 1993-04-21 | $7700.00 | Window Closed / Lapsed |