Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
113 words
A method for producing an optical fiber preform comprising the steps of: blowing through at least one nozzle gaseous material which forms glass upon reaction to produce glass material soot by a CVD method which soot is deposited on a movable target to allow a soot rod to be formed thereon; and heating and rendering transparent said soot rod produced in the first step; wherein the improvement comprises: arranging a pipe substantially concentrically with the glass material soot so as to permit gas to flow through a clearance between the deposited glass material soot and the inner wall surface of the pipe in a direction in which the soot rod grows in size.
Claim 2
Independent Claim
113 words
A method for producing an optical fiber preform comprising the steps of: blowing through at least one nozzle gaseous material which forms glass upon reaction to produce glass material soot by a CVD method which soot is deposited on a movable target to allow a soot rod to be formed thereon; and heating and rendering transparent said soot rod produced in the first step; wherein the improvement comprises: arranging a pipe substantially concentrically with the glass material soot so as to permit gas to flow through a clearance between the deposited glass material soot and the inner wall surface of the pipe in a direction in which the soot rod grows in size.
Claim 3
Dependent Claim
26 words
A method for producing an optical fiber preform as set forth in claim 1, wherein said gas permitted to flow through said clearance is inert gas.
Claim 4
Dependent Claim
26 words
A method for producing an optical fiber preform as set forth in claim 1, wherein said gas permitted to flow through said clearance is oxygen gas.
Claim 5
Dependent Claim
22 words
A method for producing an optical fiber preform as set forth in claim 1, wherein said pipe is formed of glass material.
Claim 6
Dependent Claim
42 words
A method for producing an optical fiber preform as set forth in claim 1, wherein said target is moved axially thereof in a direction which is opposite to the direction in which said soot rod grows in size, while said target rotates.
Claim 7
Dependent Claim
21 words
A method for producing an optical fiber preform as set forth in claim 1, wherein said clearance is over 1 mm.
Claim 8
Independent Claim
51 words
A method for producing an optical fiber preform as set forth in any one of claims 1 to 6, wherein said pipe is formed on its outer circumference with at least one gas inlet branch pipe, said gas inlet branch pipe being inclined in the direction in which said target moves.
Claim 9
Independent Claim
44 words
A method for producing an optical fiber preform as set forth in any one of claims 1 to 6, wherein said step of producing a soot rod and said step of heating and rendering transparent said soot rod are performed continuously in one operation.
Claim 10
Independent Claim
52 words
A method for producing an optical fiber preform as set forth in any one of claims 1 to 6, wherein said nozzle is plural in number, and said gaseous material forming glass upon reaction is blown in different compositions through said plurality of nozzles each corresponding to one of said different compositions.
Claim 11
Dependent Claim
83 words
In a method for producing an optical fiber preform comprising the steps of: producing a glass material soot rod on a movable target by chemical vapor deposition; and heating said soot rod rendering said rod transparent; wherein the improvement comprises: establishing a gas flow between the soot rod and a pipe arranged substantially concentrically with said soot rod in a direction in which the soot rod grows in size, said movable target being rotated and moved in a direction opposite said gas flow.
Claim 12
Dependent Claim
83 words
In a method for producing an optical fiber preform comprising the steps of: producing a glass material soot rod on a movable target by chemical vapor deposition; and heating said soot rod rendering said rod transparent; wherein the improvement comprises: establishing a gas flow between the soot rod and a pipe arranged substantially concentrically with said soot rod in a direction in which the soot rod grows in size, said movable target being rotated and moved in a direction opposite said gas flow.