Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
138 words
A photopolymerizable mixture which comprises: at least one olefinically unsaturated compound and at least one photoinitiator of the formula I ##STR8## where R 1 and R 2 are identical or different and each is H, halogen, phenyl, C 1 -C 6 -alkyl, C 1 -C 6 -alkoxy or C 1 -C 6 -alkylthio, R 3 is H, C 1 -C 6 -alkyl, hydroxyalkyl, cycloalkyl or aralkyl, R 4 and R 5 are identical or different and each is C 1 -C 6 -alkyl, phenyl, cycloalkyl or aralkyl or R 4 and R 5 together are a --(CH 2 ) 4 --bridge, a --(CH 2 ) 5 --bridge or a --(CH 2 ) 2 --O--(CH 2 ) 2 --bridge, R 6 is C 1 -C 6 -alkyl and X.sup.⊖ is Cl.sup.⊖, Br.sup.⊖, I.sup.⊖ or CH 3 SO 4 .sup.⊖.
Claim 2
Dependent Claim
138 words
A photopolymerizable mixture which comprises: at least one olefinically unsaturated compound and at least one photoinitiator of the formula I ##STR8## where R 1 and R 2 are identical or different and each is H, halogen, phenyl, C 1 -C 6 -alkyl, C 1 -C 6 -alkoxy or C 1 -C 6 -alkylthio, R 3 is H, C 1 -C 6 -alkyl, hydroxyalkyl, cycloalkyl or aralkyl, R 4 and R 5 are identical or different and each is C 1 -C 6 -alkyl, phenyl, cycloalkyl or aralkyl or R 4 and R 5 together are a --(CH 2 ) 4 --bridge, a --(CH 2 ) 5 --bridge or a --(CH 2 ) 2 --O--(CH 2 ) 2 --bridge, R 6 is C 1 -C 6 -alkyl and X.sup.⊖ is Cl.sup.⊖, Br.sup.⊖, I.sup.⊖ or CH 3 SO 4 .sup.⊖.
Claim 3
Dependent Claim
165 words
In a process for photopolymerizing a photopolymerizable mixture containing at least one olefinically unsaturated compound and at least one photoinitiator, wherein said mixture is irradiated to initiate the polymerization, the improvement which comprises: using as the photoinitiator at least one quaternary ammonium compound of the formula I ##STR9## where R 1 and R 2 are identical or different and each is H, halogen, phenyl, C 1 -C 6 -alkyl, C 1 -C 6 -alkoxy or C 1 -C 6 -alkylthio, R 3 is H, C 1 -C 6 -alkyl, hydroxalkyl, cycloalkyl or aralkyl, R 4 and R 5 are identical or different and each is C 1 -C 6 -alkyl, phenyl, cycloalkyl or aralkyl or R 4 and R 5 together are a --(CH 2 ) 4 --bridge, a --(CH 2 ) 5 --bridge or a --(CH 2 ) 2 --O--(CH 2 ) 2 --bridge, R 6 is C 1 -C 6 -alkyl and X.sup.⊖ is Cl.sup.⊖, Br.sup.⊖, I.sup.⊖ or CH 3 SO 4 .sup.⊖.
Claim 4
Dependent Claim
165 words
In a process for photopolymerizing a photopolymerizable mixture containing at least one olefinically unsaturated compound and at least one photoinitiator, wherein said mixture is irradiated to initiate the polymerization, the improvement which comprises: using as the photoinitiator at least one quaternary ammonium compound of the formula I ##STR9## where R 1 and R 2 are identical or different and each is H, halogen, phenyl, C 1 -C 6 -alkyl, C 1 -C 6 -alkoxy or C 1 -C 6 -alkylthio, R 3 is H, C 1 -C 6 -alkyl, hydroxalkyl, cycloalkyl or aralkyl, R 4 and R 5 are identical or different and each is C 1 -C 6 -alkyl, phenyl, cycloalkyl or aralkyl or R 4 and R 5 together are a --(CH 2 ) 4 --bridge, a --(CH 2 ) 5 --bridge or a --(CH 2 ) 2 --O--(CH 2 ) 2 --bridge, R 6 is C 1 -C 6 -alkyl and X.sup.⊖ is Cl.sup.⊖, Br.sup.⊖, I.sup.⊖ or CH 3 SO 4 .sup.⊖.
Claim 5
Dependent Claim
31 words
The process of claim 2 wherein from 0.001 to 10, preferably from 0.01 to 1, percent by weight, based on the olefinically unsaturated compounds, of the quaternary ammonium compound is employed.
Claim 6
Dependent Claim
31 words
The process of claim 2 wherein the radiation source used for the photopolymerization emits at least partially in the region from 2,000 to 5,000 A, preferably from 3,000 to 4,000 A.
Claim 7
Dependent Claim
21 words
The process of claim 2, wherein an aqueous photopolymerizable mixture is photopolymerized to form an aqueous polymer dispersion or polymer solution.
Claim 8
Dependent Claim
31 words
The process of claim 5, wherein from 0.001 to 10, preferably from 0.01 to 1, percent by weight, based on the olefinically unsaturated compounds, of the quaternary ammonium compound is employed.
Claim 9
Dependent Claim
31 words
the process of claim 5 wherein the radiation source used for the photopolymerization emits at least partially in the region from 2,000 to 5,000 A, preferably from 3,000 to 4,000 A.