Method of visually detecting antioxidant in an organic mixture
Assignee: United States Department of the Army
•
Filing: 1980-01-21
•
Granted: 1981-03-24
•
Expires: 2000-01-21
Abstract
Abstract Method of screening a mixture of organic compounds to detect the presence of an antioxidant material wherein the organic mixture is first chromatographically separated on a polyamide coated plate and then coated with linoleic acid. The plate is heated until the linoleic acid oxidation products react with the free amine groups on the polyamide material to produce a color change. Antioxidant compounds separated on the plate inhibit the color change and can be visually detected.
Inventors
- 👤 William L. Porter
- 👤 Roslyn E. Kramer
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 03:39
CPC Classifications
G; G01; G01N; G01N30/00; G01N30/90; G01N30/94; G01N31/00; G01N31/22; Y; Y10; Y10T; Y10T436/00; Y10T436/20; Y10T436/200833; Y10T436/201666
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
245 words
A method of visually detecting the antioxidant gallic acid in a mixture of organic compounds which comprises the steps of: a. separating a mixture of organic compounds into its component compounds by thin layer chromatography by contacting a mixture of organic compounds suspected of containing the antioxidant gallic acid with a polyamide-coated plate, said polyamide-coated plate comprising a sheet or plastic or glass supporting a coating of powdered polyamide of about 100 to about 120 microns thickness, said polyamide being polymerized epsilon-caprolactam, said mixture of organic compounds being separated on said polyamide-coated plate into at least two spaced-apart spots, each of said spots being the site of a different compound from the others of said spots; b. depositing a thin layer of linoleic acid over each of said spaced-apart spots; c. placing said polyamide-coated plate, containing said linoleic acid deposited thereon, in an oven at about 65° C. and heating said polyamide-coated plate for at least 8 hours at about 65° C.; d. removing said polyamide-coated plate from said oven; and e. observing said spots and the adjacent areas of said polyamide-coated plate for color differences in reflected light, the presence of a creamy-white or yellow color where one of said spaced-apart spots was located surrounded by a brown field indicating the presence of an antioxidant in the creamy-white or yellow spot, a solid brown field lacking any creamy-white or yellow color indicating the absence of antioxidant from said one of said spaced apart spots.
Claim 2
Independent Claim
245 words
A method of visually detecting the antioxidant gallic acid in a mixture of organic compounds which comprises the steps of: a. separating a mixture of organic compounds into its component compounds by thin layer chromatography by contacting a mixture of organic compounds suspected of containing the antioxidant gallic acid with a polyamide-coated plate, said polyamide-coated plate comprising a sheet or plastic or glass supporting a coating of powdered polyamide of about 100 to about 120 microns thickness, said polyamide being polymerized epsilon-caprolactam, said mixture of organic compounds being separated on said polyamide-coated plate into at least two spaced-apart spots, each of said spots being the site of a different compound from the others of said spots; b. depositing a thin layer of linoleic acid over each of said spaced-apart spots; c. placing said polyamide-coated plate, containing said linoleic acid deposited thereon, in an oven at about 65° C. and heating said polyamide-coated plate for at least 8 hours at about 65° C.; d. removing said polyamide-coated plate from said oven; and e. observing said spots and the adjacent areas of said polyamide-coated plate for color differences in reflected light, the presence of a creamy-white or yellow color where one of said spaced-apart spots was located surrounded by a brown field indicating the presence of an antioxidant in the creamy-white or yellow spot, a solid brown field lacking any creamy-white or yellow color indicating the absence of antioxidant from said one of said spaced apart spots.
Claim 3
Dependent Claim
58 words
A method according to claim 1, wherein in step (c) said polyamide-coated plate is covered with a glass or plastic plate prior to the heating of said polyamide-coated plate in said oven to prevent the escape of volatile antioxidant from said spot on said polyamide-coated plate, whereby said spot remains creamy-white or yellow surrounded by a brown field.
Claim 4
Dependent Claim
53 words
A method according to claim 1 wherein in step (c) said polyamide-coated plate is placed on a glass plate of greater area than said polyamide-coated plate with said coating of powdered polyamide facing upwardly and not in contact with said glass plate and then heating said polyamide-coated plate supported on said glass plate.
Claim 5
Dependent Claim
33 words
A method according to claim 1 wherein in step (b) about 20 microliters of linoleic acid is deposited at the center of each spaced-apart spot, said linoleic acid spreading to cover the spot.
References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-03-23 | 1984-09-22 | 1985-03-24 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-03-23 | 1988-09-22 | 1989-03-24 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-03-23 | 1992-09-22 | 1993-03-24 | $7700.00 | Window Closed / Lapsed |