← Back to Patent Explorer
US4252415A Expired / Lapsed US ⏱️ 0.0 years remaining

Liquid crystal cell and process for its production

Assignee: BBC Brown Boveri France SA
•
Filing: 1978-07-11
•
Granted: 1981-02-24
•
Expires: 1998-07-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A liquid crystal cell with two flat glass plates aligned parallel to one another and at a distance from one another, a web of low-melting glass solder provided between the glass plates, a liquid crystal substance provided in the inner space formed by the glass plates and the glass solder web and with electrodes applied on the surfaces of the glass plates facing one another, the connections of which are brought out of the inner space via the glass solder web, wherein the glass solder web and/or the electrodes contain an at least partly reduced oxidizing agent which is formed by the reduction of an oxidizing agent during the glass soldering of the liquid crystal cell.

Inventors

  • 👤 Hans-Peter Klein
  • 👤 Hans-Rudolf Zeller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 05:52
CPC Classifications
G; G02; G02F; G02F1/00; G02F1/01; G02F1/13; G02F1/133; G02F1/1333; G02F1/1341; Y; Y10; Y10S; Y10S359/00; Y10S359/90

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 260 words
A process for producing a liquid crystal cell having two flat glass plates aligned parallel to one another and at a distance from one another, a web of low-melting glass solder provided between the glass plates, a liquid crystal substance provided in the inner space formed by the glass plates and the glass solder web, and electrodes applied on the surfaces of the glass plates facing one another, said electrodes having connections thereto which are brought out of the inner space via the glass solder web, comprising the steps of: mixing an oxidizing agent with the glass solder to form a first mixture; said oxidizing agent being 2.5 percent by weight of manganese dioxide; mixing an organic binder to said first mixture to form a glass solder paste; applying said glass solder paste on at least one of said glass plates provided with electrodes; aligning said glass plates in relation to one another; soldering said glass plates to form an inner space between said glass plates and said glass solder web, said oxidizing agent preventing the formation of electro-chemical corrosion effects on said electrodes during the soldering of said glass plates by oxidizing the uncombusted residue of the organic binder of the glass solder paste; and, filling said inner space with a liquid crystal substance having rod-shaped liquid crystal molecules in such a manner that the angle between the axis of the rod-shaped liquid crystal molecules and the projection of the liquid crystal molecules on the surfaces of the glass plates is substantially the same throughout said liquid crystal cell.
Claim 2
Dependent Claim 260 words
A process for producing a liquid crystal cell having two flat glass plates aligned parallel to one another and at a distance from one another, a web of low-melting glass solder provided between the glass plates, a liquid crystal substance provided in the inner space formed by the glass plates and the glass solder web, and electrodes applied on the surfaces of the glass plates facing one another, said electrodes having connections thereto which are brought out of the inner space via the glass solder web, comprising the steps of: mixing an oxidizing agent with the glass solder to form a first mixture; said oxidizing agent being 2.5 percent by weight of manganese dioxide; mixing an organic binder to said first mixture to form a glass solder paste; applying said glass solder paste on at least one of said glass plates provided with electrodes; aligning said glass plates in relation to one another; soldering said glass plates to form an inner space between said glass plates and said glass solder web, said oxidizing agent preventing the formation of electro-chemical corrosion effects on said electrodes during the soldering of said glass plates by oxidizing the uncombusted residue of the organic binder of the glass solder paste; and, filling said inner space with a liquid crystal substance having rod-shaped liquid crystal molecules in such a manner that the angle between the axis of the rod-shaped liquid crystal molecules and the projection of the liquid crystal molecules on the surfaces of the glass plates is substantially the same throughout said liquid crystal cell.
Claim 3
Dependent Claim 27 words
A process according to claim 1, wherein the proportion of the oxidizing agent comprises to 0.1 to 20 percent by weight of the quantity of glass solder.
Claim 4
Dependent Claim 33 words
A process according to claim 2, wherein the proportion of the oxidizing agent amounts to 1 to 5 percent, preferably more than 2.5 percent by weight of the quantity of the glass solder.
Claim 5
Dependent Claim 21 words
A process according to claim 1, wherein said oxidizing agent and said glass solder comprises powders mixed uniformly with one another.
Claim 6
Dependent Claim 24 words
A process according to claim 1, wherein said oxidizing agent has a particle size corresponding at most to the distance between the cell plates.
Claim 7
Dependent Claim 19 words
A process according to claim 1, wherein the glass soldering process is carried out at temperatures below 535° C.

References Cited (Backward Citations)

US3370966A Cited
US3995941A Cited
US4099977A Cited
US4158485A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-02-24 1984-08-25 1985-02-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-02-24 1988-08-25 1989-02-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-02-24 1992-08-25 1993-02-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag