← Back to Patent Explorer
US4251641A Expired / Lapsed US ⏱️ 0.0 years remaining

Low shrinkage polyester resin compositions

Assignee: Resonac Corp
•
Filing: 1979-12-04
•
Granted: 1981-02-17
•
Expires: 1999-12-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Unsaturated polyester resin compositions that have a low shrinking property, and at the same time, an enough strength are provided. The compositions comprises (1) 30-70 parts by weight of an unsaturated polyester obtained by reactin terephthalic acid and/or isophthalic acid and one or more of unsaturated acids selected from the group consisting of maleic anhydride, maleic acid and fumaric acid, with a glycol, and having the unsaturation degree of 1.5-5.0 and the acid value of 18-40, (2) 70-30 parts by weight of alpha , beta -ethylenically unsaturated monomer, and (3) 5-30 parts by weight of an amorphous linear saturated polyester resin obtained by reacting terephthalic acid and/or isophthalic acid with a glycol component.

Inventors

  • 👤 Kouji Arakawa
  • 👤 Kanemasa Nomaguchi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 13:13
CPC Classifications
C; C08; C08G; C08G63/00; C08G63/02; C08G63/12; C08G63/52; C08G63/54; C08L; C08L67/00; C08L67/06

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 128 words
A low shrinkage unsaturated polyester resin composition which comprises (1) 30-70 parts by weight of an unsaturated polyester obtained by reacting (a) an acid selected from the group consisting of terephthalic acid, isophthalic acid and mixtures thereof and (b) an unsaturated acid selected from the group consisting of maleic anhydride, maleic acid, fumaric acid, and mixtures thereof with (c) a glycol, said polyester having the unsaturation degree (moles of the unsaturated acids in 1,000 g. of the unsaturated polyester) of 1.5-5.0 and the acid value of 18-40, (2) 70-30 parts by weight of α,β-ethylenically unsaturated monomer, and (3) 5-30 parts by weight of an amorphous linear saturated polyester resin obtained by reacting an acid selected from the terephthalic acid, isophthalic acid and mixtures thereof with a glycol component.
Claim 2
Dependent Claim 128 words
A low shrinkage unsaturated polyester resin composition which comprises (1) 30-70 parts by weight of an unsaturated polyester obtained by reacting (a) an acid selected from the group consisting of terephthalic acid, isophthalic acid and mixtures thereof and (b) an unsaturated acid selected from the group consisting of maleic anhydride, maleic acid, fumaric acid, and mixtures thereof with (c) a glycol, said polyester having the unsaturation degree (moles of the unsaturated acids in 1,000 g. of the unsaturated polyester) of 1.5-5.0 and the acid value of 18-40, (2) 70-30 parts by weight of α,β-ethylenically unsaturated monomer, and (3) 5-30 parts by weight of an amorphous linear saturated polyester resin obtained by reacting an acid selected from the terephthalic acid, isophthalic acid and mixtures thereof with a glycol component.
Claim 3
Dependent Claim 21 words
The composition according to claim 1, wherein the amorphous linear saturated polyester resin has the number average molecular weight of 3,000-20,000.

References Cited (Backward Citations)

US3489707A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-02-17 1984-08-18 1985-02-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-02-17 1988-08-18 1989-02-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-02-17 1992-08-18 1993-02-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag