US4251572A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of restoring or repairing reflective glass
Assignee: Pilkington North America Inc
•
Filing: 1975-12-12
•
Granted: 1981-02-17
•
Expires: 1995-12-12
Abstract
Abstract Methods of restoring or repairing damaged areas in the coating of high performance reflective glass composed of a thin, transparent film such as a metal and/or a metal oxide deposited on a vitreous substrate. Damages to the film such as scratches, abrasive rubs and the like are covered with a compatible filler to substantially restore the light transmittance characteristics. The repaired areas are covered with a protective coating to increase their durability.
Inventors
- 👤 Siegfried H. Herliczek
- 👤 Lazarus D. Thomas
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 01:36
CPC Classifications
B; B29; B29C; B29C73/00; B29C73/04; C; C03; C03C; C03C17/00; C03C17/34; C03C17/36; C03C17/38; C03C17/42; G; G02; G02B; G02B1/00; G02B1/10; B29K; B29K2995/00; B29K2995/0018; B29K2995/0026; Y; Y10; Y10S; Y10S428/00; Y10S428/913; Y10S428/914
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
214 words
A method of repairing damaged areas in an original thin light transmitting film exhibiting a color and deposited on the surface of a transparent glass substrate, said film comprising one or more layers of a material selected from the group consisting of a metal, metal halide, metal oxide and mixtures thereof, comprising the steps of: a. cleaning the damaged areas in the original film to remove any foreign debris; b. covering the damaged areas with a transparent filler having similar light transmitting characteristics and exhibiting substantially the same color as the original thin film, said covering step including: (1) placing a transfer comprising a sheet containing a transparent film of substantially the same composition and light transmittance as the original thin film and a heat sensitive adhesive over said damaged areas; and (2) heating said transfer over the damaged areas to first deposit said adhesive in said damaged areas and then release said transparent film from said transfer whereby said transparent film adheres to and fills the damaged areas in the original thin film; and c. coating said filler with a transparent protective layer capable of physically protecting said filler whereby the light transmittant characteristics of the repaired damaged areas are substantially the same as the light transmittant characteristics of the original thin film.
Claim 2
Independent Claim
214 words
A method of repairing damaged areas in an original thin light transmitting film exhibiting a color and deposited on the surface of a transparent glass substrate, said film comprising one or more layers of a material selected from the group consisting of a metal, metal halide, metal oxide and mixtures thereof, comprising the steps of: a. cleaning the damaged areas in the original film to remove any foreign debris; b. covering the damaged areas with a transparent filler having similar light transmitting characteristics and exhibiting substantially the same color as the original thin film, said covering step including: (1) placing a transfer comprising a sheet containing a transparent film of substantially the same composition and light transmittance as the original thin film and a heat sensitive adhesive over said damaged areas; and (2) heating said transfer over the damaged areas to first deposit said adhesive in said damaged areas and then release said transparent film from said transfer whereby said transparent film adheres to and fills the damaged areas in the original thin film; and c. coating said filler with a transparent protective layer capable of physically protecting said filler whereby the light transmittant characteristics of the repaired damaged areas are substantially the same as the light transmittant characteristics of the original thin film.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-02-17 | 1984-08-18 | 1985-02-17 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-02-17 | 1988-08-18 | 1989-02-17 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-02-17 | 1992-08-18 | 1993-02-17 | $7700.00 | Window Closed / Lapsed |