← Back to Patent Explorer
US4247624A Expired / Lapsed US ⏱️ 0.0 years remaining

Photopolymerizable elastomeric compositions with carbamated poly(vinyl alcohol) binder

Assignee: EIDP Inc
•
Filing: 1979-05-29
•
Granted: 1981-01-27
•
Expires: 1999-05-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Flexographic printing plates are prepared from photosensitive elastomeric compositions which comprise (1) about 15 to about 89 percent by weight of a carbamated poly(vinyl alcohol) polymeric binder, (2) about 10 to about 70 percent by weight of a compatible monomer, and (3) about 0.1 to about 10 percent by weight of a free-radical generating system.

Inventors

  • 👤 Robert P. Foss

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 12:47
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/027; G03F7/032; G03F7/033; C; C08; C08F; C08F8/00; C08F8/30; Y; Y10; Y10S; Y10S430/00; Y10S430/1053; Y10S430/1055; Y10S430/106; Y10S430/107; Y10S430/11

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 241 words
A photopolymerizable elastomeric composition which comprises, based on the total composition: (1) 15 to 89 percent by weight of a carbamated poly(vinyl alcohol) polymeric binder wherein (a) 15 to 100 mole percent of the recurring units in said binder have the formula ##STR10## wherein R is NH 2 in some recurring units and at least one of OR 1 and NHR 1 in the remaining recurring units wherein OR 1 is the residue remaining after removal of a hydrogen atom from an alcohol which has a boiling point of greater than 100° C. at normal atmospheric pressure, with the proviso that said alcohol is compatible with said polymeric binder, and the ratio of (OR 1 +NHR 1 )/NH 2 is within the range of 0.05 to 1.0, and (b) 0 to 85 mole percent of the recurring units in said binder have a formula selected from the group consisting of ##STR11## with the proviso that no more than 12 mole percent of the recurring units in said binder have the formula ##STR12## (2) 10 to 70 percent by weight of a nongaseous, ethylenically unsaturated compound containing at least one terminal ethylenic group, said compound being capable of forming a high polymer by radical initiated chain-propagating addition polymerization, and being compatible with polymeric binder (1); and (3) 0.1 to 10 percent by weight of a thermally stable, radiation-sensitive, radical generating system, activatable by actinic radiation, which initiates polymerization of the unsaturated compound.
Claim 2
Dependent Claim 241 words
A photopolymerizable elastomeric composition which comprises, based on the total composition: (1) 15 to 89 percent by weight of a carbamated poly(vinyl alcohol) polymeric binder wherein (a) 15 to 100 mole percent of the recurring units in said binder have the formula ##STR10## wherein R is NH 2 in some recurring units and at least one of OR 1 and NHR 1 in the remaining recurring units wherein OR 1 is the residue remaining after removal of a hydrogen atom from an alcohol which has a boiling point of greater than 100° C. at normal atmospheric pressure, with the proviso that said alcohol is compatible with said polymeric binder, and the ratio of (OR 1 +NHR 1 )/NH 2 is within the range of 0.05 to 1.0, and (b) 0 to 85 mole percent of the recurring units in said binder have a formula selected from the group consisting of ##STR11## with the proviso that no more than 12 mole percent of the recurring units in said binder have the formula ##STR12## (2) 10 to 70 percent by weight of a nongaseous, ethylenically unsaturated compound containing at least one terminal ethylenic group, said compound being capable of forming a high polymer by radical initiated chain-propagating addition polymerization, and being compatible with polymeric binder (1); and (3) 0.1 to 10 percent by weight of a thermally stable, radiation-sensitive, radical generating system, activatable by actinic radiation, which initiates polymerization of the unsaturated compound.
Claim 3
Dependent Claim 56 words
The photopolymerizable elastomeric composition of claim 1 wherein the composition contains 30 to 70 percent by weight of carbamated poly(vinyl alcohol) polymer binder, 20 to 40 percent by weight of ethylenically unsaturated compound having a boiling point of greater than 100° C. at atmospheric pressure, and 0.2 to 1 percent by weight of radical generating system.
Claim 4
Dependent Claim 64 words
The photopolymerizable elastomeric composition of claim 2 wherein 30 to 50 mole percent of the recurring units in said binder have the formula ##STR13## the ratio of (OR 1 +NHR 1 )/NH 2 is within the range of 0.1 to 0.3, and 50 to 70 mole percent of the recurring units in said binder have a formula selected from the group consisting of ##STR14##
Claim 5
Dependent Claim 257 words
A photopolymerizable element which comprises a substrate coated to a thickness of 0.5 to 250 mils with a photosensitive elastomeric composition which comprises, based on the total composition: (1) 15 to 89 percent by weight of a carbamated poly(vinyl alcohol) polymeric binder wherein (a) 15 to 100 mole percent of the recurring units in said binder have the formula ##STR15## wherein R is NH 2 in some recurring units and at least one of OR 1 and NHR 1 in the remaining recurring units wherein OR 1 is the residue remaining after removal of a hydrogen atom from an alcohol which has a boiling point of greater than 100° C. at normal atmospheric pressure, with the proviso that said alcohol is compatible with said polymeric binder, and the ratio of (OR 1 +NHR 1 )/NH 2 is within the range of 0.05 to 1.0, and (b) 0 to 85 mole percent of the recurring units in said binder have a formula selected from the group consisting of ##STR16## with the proviso that no more than 12 mole percent of the recurring units in said binder have the formula ##STR17## (2) 10 to 70 percent by weight of a nongaseous, ethylenically unsaturated compound containing at least one terminal ethylenic group, said compound being capable of forming a high polymer by radical initiated chain-propagating addition polymerization, and being compatible with polymeric binder (1); (3) 0.1 to 10 percent by weight of a thermally stable, radiation-sensitive, radical generating system, activatable by actinic radiation, which initiates polymerization of the unsaturated compound.
Claim 6
Dependent Claim 257 words
A photopolymerizable element which comprises a substrate coated to a thickness of 0.5 to 250 mils with a photosensitive elastomeric composition which comprises, based on the total composition: (1) 15 to 89 percent by weight of a carbamated poly(vinyl alcohol) polymeric binder wherein (a) 15 to 100 mole percent of the recurring units in said binder have the formula ##STR15## wherein R is NH 2 in some recurring units and at least one of OR 1 and NHR 1 in the remaining recurring units wherein OR 1 is the residue remaining after removal of a hydrogen atom from an alcohol which has a boiling point of greater than 100° C. at normal atmospheric pressure, with the proviso that said alcohol is compatible with said polymeric binder, and the ratio of (OR 1 +NHR 1 )/NH 2 is within the range of 0.05 to 1.0, and (b) 0 to 85 mole percent of the recurring units in said binder have a formula selected from the group consisting of ##STR16## with the proviso that no more than 12 mole percent of the recurring units in said binder have the formula ##STR17## (2) 10 to 70 percent by weight of a nongaseous, ethylenically unsaturated compound containing at least one terminal ethylenic group, said compound being capable of forming a high polymer by radical initiated chain-propagating addition polymerization, and being compatible with polymeric binder (1); (3) 0.1 to 10 percent by weight of a thermally stable, radiation-sensitive, radical generating system, activatable by actinic radiation, which initiates polymerization of the unsaturated compound.
Claim 7
Dependent Claim 56 words
The photopolymerizable element of claim 4 wherein the photosensitive elastomeric composition contains 30 to 70 percent by weight of carbamated poly(vinyl alcohol) polymeric binder, 20 to 40 percent by weight of ethylenically unsaturated compound having a boiling point of greater than 100° C. atmospheric pressure, and 0.2 to 1 percent by weight of radical generating system.
Claim 8
Dependent Claim 63 words
The photopolymerizable element of claim 5 wherein 30 to 50 mole percent of the recurring units in said binder have the formula ##STR18## the ratio of (OR 1 +NHR 1 )/NH 2 is within the range of 0.1 to 0.3, and 50 to 70 mole percent of the recurring units in said binder have a formula selected from the group consisting of ##STR19##

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-01-27 1984-07-28 1985-01-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-01-27 1988-07-28 1989-01-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-01-27 1992-07-28 1993-01-27 $7700.00 Window Closed / Lapsed