Liquid photopolymerizable composition for making printing forms
Abstract
Abstract A liquid photopolymerizable composition, according to the invention, consists of methyl methacrylate, benzoin or benzoin ethers, a photopolymerizable component--an oligocarbonate methacrylate or a mixture thereof with an oligoester acrylate or oligoester maleinate at a weight ratio of these oligomers in the mixture of 1:1, the components being taken in the following proportions (in % by weight): methyl methacrylate: 5-10 benzoin or benzoin ethers: 0.1.0 photopolymerizable component: the balance Light sensitivity of this composition is up to 981 J/m 2 in terms of exposure H at d=1 mm (wherein d is the thickness of a photopolymeric layer obtained by acting with UV-radiation on the composition; the radiation source - luminescent UV-lamps of 80 W total output. Printing forms made on the basis of this composition exhibit improved physical and mechanical properties. Thus, tensile strength of the printing forms is as high as 5.25 kgf/mm 2 and durability, up to 1 million impressions.
Inventors
- 👤 Alfred A. Berlin
- 👤 Fedor I. Dubrovitsky
- 👤 Eduard T. Lazarenko
- 👤 Tamara Y. Kefeli
- 👤 Khaim-Mordke A. Brikenshtein
- 👤 Vladislav V. Bernatsek
- 👤 Tatyana A. Zhizhileva
- 👤 Boris V. Kovalenko
- 👤 Natalya L. Marshavina
- 👤 Roman I. Mervinsky
- 👤 Anna A. Radugina
- 👤 Anatoly R. Tischenko
- 👤 Julia M. Fillipovskaya
Bibliographic Details
Claims Analysis
Total Claims: 10References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-01-20 | 1984-07-21 | 1985-01-20 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-01-20 | 1988-07-21 | 1989-01-20 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-01-20 | 1992-07-21 | 1993-01-20 | $7700.00 | Window Closed / Lapsed |