Abstract

Abstract Vulcanizable semi-conductive compositions that can be used to provide strippable insulation shielding compositions for electrical conductors, and articles of manufacture wherein the cross-linked products of said vulcanizable compositions are directly bonded to a crosslinked polyolefin substrate.

Inventors

  • 👤 Lucio Ongchin

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 00:53
CPC Classifications
H; H01; H01B; H01B1/00; H01B1/20; H01B1/24; C; C08; C08K; C08K3/00; C08K3/02; C08K3/04; C08L; C08L23/00; C08L23/02; C08L23/04; C08L23/08; C08L23/0846; C08L23/0853; C08L9/00; C08L9/02

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 184 words
A vulcanizable semi-conductive insulation shielding composition consisting essentially of (A) an ethylene copolymer selected from the group consisting of an ethylene-alkyl acrylate copolymer containing from about 15 to 45 weight percent of alkyl acrylate based on the total weight of said copolymer, said alkyl acrylate being selected from the group consisting of the C 1 to C 8 alkyl esters of acrylic acid and methacrylic acid, and an ethylene-vinyl acetate copolymer containing from about 15 to 45 weight percent of vinyl acetate based on the total weight of said copolymer, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition.
Claim 2
Dependent Claim 184 words
A vulcanizable semi-conductive insulation shielding composition consisting essentially of (A) an ethylene copolymer selected from the group consisting of an ethylene-alkyl acrylate copolymer containing from about 15 to 45 weight percent of alkyl acrylate based on the total weight of said copolymer, said alkyl acrylate being selected from the group consisting of the C 1 to C 8 alkyl esters of acrylic acid and methacrylic acid, and an ethylene-vinyl acetate copolymer containing from about 15 to 45 weight percent of vinyl acetate based on the total weight of said copolymer, (B) a butadiene-acrylonitrile copolymer containing from about 10 to about 50 percent by weight of acrylonitrile based on the total weight of said copolymer, (C) conductive carbon black, and (D) a peroxide crosslinking agent, wherein the weight ratio of (A) to (B) in said composition is 1:9 to 9:1, wherein the weight ratio of (C) to the sum weight of (A)+(B) in said composition is 0.1 to 1.5 and wherein (D) is present in an amount of from about 0.2 to about 5 percent by weight based on the total weight of the composition.
Claim 3
Dependent Claim 18 words
A vulcanizable semi-conductive composition as defined in claim 1 wherein the ethylene copolymer is an ethylene-vinyl acetate copolymer.
Claim 4
Dependent Claim 34 words
A vulcanizable semi-conductive composition as defined in claim 2 wherein (D) is present in an amount of from about 0.6 to about 2 percent by weight based on the total weight of the composition.
Claim 5
Dependent Claim 32 words
A vulcanizable semi-conductive composition as defined in claim 3, wherein about 0.2 to about 1 percent by weight of an antioxidant based on the total weight of the composition is also present.
Claim 6
Dependent Claim 17 words
A vulcanizable semi-conducting composition as defined in claim 4 wherein said peroxide crosslinking agent is di-α-cumyl peroxide.

References Cited (Backward Citations)

US3862056A Cited
US3719769A Cited
US3950604A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-01-20 1984-07-21 1985-01-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-01-20 1988-07-21 1989-01-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-01-20 1992-07-21 1993-01-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag