Abstract

Abstract Covers a polyurethane elastomer of improved moldability, particularly useful in RIM applications which comprises the reaction product of an aromatic polyisocyanate, a high molecular weight polyether triol containing an internal mixed propylene oxide-ethylene oxide segment comprising 2-35% ethylene oxide by weight and 65-98% by weight of propylene oxide and an ethylene oxide cap such that said polyol has a primary hydroxyl content greater than 50% and preferably greater than 90%, and a chain-extending agent. Also covers the method of making said elastomer.

Inventors

  • 👤 Kenneth G. McDaniel
  • 👤 Doris M. Rice
  • 👤 Michael Cuscurida

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 12:32
CPC Classifications
C; C08; C08G; C08G18/00; C08G18/06; C08G18/70; C08G18/72; C08G18/74; C08G18/76; C08G18/7657; C08G18/7664; C08G18/28; C08G18/40; C08G18/48; C08G18/4833; C08G18/4837; C08G18/4841; C08G18/65; C08G18/66; C08G18/6666; C08G18/667; C08G18/6674; C08G2120/00; Y; Y10; Y10S; Y10S264/00; Y10S264/83; Y10S521/00; Y10S521/914

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 69 words
A reaction injection molded polyurethane elastomer having improved moldability and other improved properties comprising the reaction product of an aromatic polyisocyanate, a high molecular weight triol containing an internal mixed propylene oxide-ethylene oxide segment comprising 2-35% by weight of ethylene oxide and 65-98% by weight of propylene oxide and an ethylene oxide cap such that said triol has a primary hydroxyl content greater than 50% and a chain-extending agent.
Claim 2
Dependent Claim 69 words
A reaction injection molded polyurethane elastomer having improved moldability and other improved properties comprising the reaction product of an aromatic polyisocyanate, a high molecular weight triol containing an internal mixed propylene oxide-ethylene oxide segment comprising 2-35% by weight of ethylene oxide and 65-98% by weight of propylene oxide and an ethylene oxide cap such that said triol has a primary hydroxyl content greater than 50% and a chain-extending agent.
Claim 3
Dependent Claim 14 words
The polyurethane of claim 1 wherein said triol has an equivalent weight of 1300-3000.
Claim 4
Dependent Claim 12 words
The polyurethane of claim 1 wherein said aromatic polyisocyanate is methylene bis(4-phenylisocyanate).
Claim 5
Dependent Claim 12 words
The polyurethane of claim 1 wherein said chain-extending agent is ethylene glycol.
Claim 6
Dependent Claim 11 words
The polyurethane of claim 1 wherein said chain-extending agent is 1,4-butanediol.
Claim 7
Dependent Claim 23 words
The polyurethane of claim 1 wherein said high molecular weight triol is a polyether triol having a primary hydroxyl content greater than 90%.
Claim 8
Independent Claim 91 words
A method of making a polyurethane elastomer of improved moldability which comprises injecting via a RIM machine into a mold cavity of the desired configuration a foam formulation and demolding the molded article, said formulation being the reaction product of an aromatic polyisocyanate, a high molecular weight triol containing an internal mixed propylene oxide-ethylene oxide segment comprising 2-35% by weight of ethylene oxide and 65-98% by weight of propylene oxide and an ethylene oxide cap such that said triol has a primary hydroxyl content greater than 50%, and a chain-extending agent.
Claim 9
Independent Claim 91 words
A method of making a polyurethane elastomer of improved moldability which comprises injecting via a RIM machine into a mold cavity of the desired configuration a foam formulation and demolding the molded article, said formulation being the reaction product of an aromatic polyisocyanate, a high molecular weight triol containing an internal mixed propylene oxide-ethylene oxide segment comprising 2-35% by weight of ethylene oxide and 65-98% by weight of propylene oxide and an ethylene oxide cap such that said triol has a primary hydroxyl content greater than 50%, and a chain-extending agent.
Claim 10
Dependent Claim 22 words
The method of claim 7 wherein said high molecular weight triol has an equivalent weight of from about 1500 to about 3000.
Claim 11
Dependent Claim 13 words
The method of claim 7 wherein said aromatic polyisocyanate is methylene bis (4-phenylisocyanate).
Claim 12
Dependent Claim 11 words
The method of claim 7 wherein chain-extending agent is ethylene glycol.
Claim 13
Dependent Claim 11 words
The method of claim 7 wherein said chain-extending agent is 1,4-butanediol.
Claim 14
Dependent Claim 23 words
The method of claim 7 wherein said high molecular weight is a polyether triol and has a primary hydroxyl content greater than 90%.

References Cited (Backward Citations)

US3535307A Cited
US3630973A Cited
US3857800A Cited
US4065410A Cited
US4125505A Cited
US4126742A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-01-06 1984-07-07 1985-01-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-01-06 1988-07-07 1989-01-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-01-06 1992-07-07 1993-01-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag