Abstract

Abstract A double mask raster method for application of a number of different slurries in a discrete pattern, to produce a raster such as can be used in color television picture tubes, has a first mask having a plurality of apertures therein which remains immovably on the substrate throughout the application of all slurries. A separate second mask having a smaller number of aligned apertures therein is utilized with each successive application of a different slurry, allowing the slurry to penetrate the two masks to the substrate only where apertures in the two masks are aligned. The method may be used to apply slurries to flat or curved substrates in a vertical or horizontal position adapted for conventional spraying, or by means of electrostatic spraying.

Inventors

  • 👤 Rolf Wengert
  • 👤 Wilhelm Huber

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 04:18
CPC Classifications
H; H01; H01J; H01J9/00; H01J9/20; H01J9/22; H01J9/227; H01J9/2277

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 131 words
A method for applying a plurality of different slurries to a glass television picture screen comprising the steps of: maintaining a base mask having a plurality of apertures immovably in position adjacent the glass screen; placing a second mask associated with a slurry to be applied over said base mask, said second mask having a plurality of apertures which is less than the plurality of apertures in said base mask; aligning the apertures in said second mask with apertures in said base mask; applying a slurry evenly over said second mask; rinsing away excess slurry; removing said second mask; repeating said method with a second mask associated with each slurry to be applied, each said second mask having apertures therein which do not overlap apertures in masks associated with other slurries.
Claim 2
Independent Claim 131 words
A method for applying a plurality of different slurries to a glass television picture screen comprising the steps of: maintaining a base mask having a plurality of apertures immovably in position adjacent the glass screen; placing a second mask associated with a slurry to be applied over said base mask, said second mask having a plurality of apertures which is less than the plurality of apertures in said base mask; aligning the apertures in said second mask with apertures in said base mask; applying a slurry evenly over said second mask; rinsing away excess slurry; removing said second mask; repeating said method with a second mask associated with each slurry to be applied, each said second mask having apertures therein which do not overlap apertures in masks associated with other slurries.
Claim 3
Dependent Claim 42 words
The method of claim 1 wherein the number of apertures in each second mask associated with each slurry is a fraction of the number of apertures in said base mask equal to the reciprocal of the number of slurries to be applied.
Claim 4
Dependent Claim 26 words
The method of claim 1 wherein the step of applying a slurry evenly over said second mask consists of spraying said slurry onto said second mask.
Claim 5
Dependent Claim 48 words
The method of claim 1 wherein the step of applying a slurry evenly over said second mask comprises the steps of: providing a means for positively charging said glass screen; grounding a means of spraying said slurry over said second mask; spraying said slurry over said second mask.
Claim 6
Dependent Claim 26 words
The method of claim 4 wherein a potential in the range of 20 to 30 kV exists between said glass screen and said grounded spraying means.
Claim 7
Independent Claim 278 words
A method for applying three different slurries to a glass television picture screen, each slurry containing a fluorescent substance in the range of 10% to 35% by weight, butylacetate in the range of 10% through 20% by volume, ethanol in the range of 1% through 20% by volume, xylene in the range of 0% through 30% by volume, volatile acetates with methanol and butanol in the range of 10% through 30% by volume, and other low alcohols in the range of 0% through 20% by volume, said method comprising: maintaining a base mask having a plurality of apertures immovably in position adjacent the glass screen; taking a first slurry with a fluorescent substance which is a red emitting phosphor; placing a second mask associated with said first slurry over said base mask, said second mask having a plurality of apertures which is less than the plurality of apertures in said base mask; aligning the aperturs in said second mask with apertures in said base masks; applying said slurry evenly over said second mask; removing said second mask; repeating said method substituting for said first slurry which is a blue emitting phosphor, and substituting a third mask associated with said second slurry for said second mask, said third mask having a plurality of apertures therein in non-alignment with said apertures in said second mask; repeating said method substituting for said first slurry a third slurry with a fluorescent substance which is a green emitting phosphor and substituting a fourth mask associated with said third slurry for said second mask, said fourth mask having a plurality of apertures therein in non-alignment with said apertures in said second and third masks.
Claim 8
Independent Claim 278 words
A method for applying three different slurries to a glass television picture screen, each slurry containing a fluorescent substance in the range of 10% to 35% by weight, butylacetate in the range of 10% through 20% by volume, ethanol in the range of 1% through 20% by volume, xylene in the range of 0% through 30% by volume, volatile acetates with methanol and butanol in the range of 10% through 30% by volume, and other low alcohols in the range of 0% through 20% by volume, said method comprising: maintaining a base mask having a plurality of apertures immovably in position adjacent the glass screen; taking a first slurry with a fluorescent substance which is a red emitting phosphor; placing a second mask associated with said first slurry over said base mask, said second mask having a plurality of apertures which is less than the plurality of apertures in said base mask; aligning the aperturs in said second mask with apertures in said base masks; applying said slurry evenly over said second mask; removing said second mask; repeating said method substituting for said first slurry which is a blue emitting phosphor, and substituting a third mask associated with said second slurry for said second mask, said third mask having a plurality of apertures therein in non-alignment with said apertures in said second mask; repeating said method substituting for said first slurry a third slurry with a fluorescent substance which is a green emitting phosphor and substituting a fourth mask associated with said third slurry for said second mask, said fourth mask having a plurality of apertures therein in non-alignment with said apertures in said second and third masks.
Claim 9
Independent Claim 265 words
A method for applying three different slurries to a glass television picture screen, each slurry containing a fluorescent substance in the range of 10% through 35% by weight, deionized water in the range of 20% through 35% by volume, polyvinyl alcohols in the range of 20% through 60% by volume, and anti-foaming agents in the range of 0.05% through 1% by volume, said method comprising: maintaining a base mask having a plurality of apertures immovably in position adjacent the glass screen; taking a first slurry with a fluorescent substance which is a red emitting phosphor; placing a second mask associated with said first slurry over said base mask, said second mask having a plurality of apertures which is less than the plurality of apertures in said base mask; aligning the apertures in said second mask with apertures in said base mask; applying said slurry evenly over said second mask; rinsing away excess slurry; removing said second mask; repeating said method substituting for said first slurry a second slurry with a fluorescent substance which is a blue emitting phosphor, and substituting a third mask associated with said second slurry for said second mask, said third mask having a plurality of apertures therein in non-alignment with said apertures in said second mask; repeating said method substituting for said first slurry a third slurry with a fluorescent substance which is a green emitting phosphor, and substituting a fourth mask associated with said third slurry for said second mask, said fourth mask having a plurality of apertures therein in non-alignment with said apertures in said second and third masks.
Claim 10
Independent Claim 265 words
A method for applying three different slurries to a glass television picture screen, each slurry containing a fluorescent substance in the range of 10% through 35% by weight, deionized water in the range of 20% through 35% by volume, polyvinyl alcohols in the range of 20% through 60% by volume, and anti-foaming agents in the range of 0.05% through 1% by volume, said method comprising: maintaining a base mask having a plurality of apertures immovably in position adjacent the glass screen; taking a first slurry with a fluorescent substance which is a red emitting phosphor; placing a second mask associated with said first slurry over said base mask, said second mask having a plurality of apertures which is less than the plurality of apertures in said base mask; aligning the apertures in said second mask with apertures in said base mask; applying said slurry evenly over said second mask; rinsing away excess slurry; removing said second mask; repeating said method substituting for said first slurry a second slurry with a fluorescent substance which is a blue emitting phosphor, and substituting a third mask associated with said second slurry for said second mask, said third mask having a plurality of apertures therein in non-alignment with said apertures in said second mask; repeating said method substituting for said first slurry a third slurry with a fluorescent substance which is a green emitting phosphor, and substituting a fourth mask associated with said third slurry for said second mask, said fourth mask having a plurality of apertures therein in non-alignment with said apertures in said second and third masks.
Claim 11
Dependent Claim 44 words
The method of claim 6 further including the step of choosing the fluorescent substance for said first slurry from a group consisting of yttrium venadate doped with europium, yttrium oxide doped with europium, yttrium sulphoxide doped with europium, and calcium silicate doped with manganese.
Claim 12
Dependent Claim 35 words
The method of claim 6 further including the step of choosing the fluorescent substance for said second slurry from a group consisting of zinc sulphide doped with silver, calcium tungstate, and barium-magnesium-aluminate doped with europium.
Claim 13
Dependent Claim 59 words
The method of claim 6 further including the step of choosing the fluorescent substance for said third slurry from a group consisting of zinc cadmium sulphide doped with zinc copper, zinc sulphide doped with silver, zinc cadmium doped with silver, zinc silicate doped with manganese, zinc oxide, and gadolinium sulphoxide doped with terbium, and lanthanum sulphoxide doped with terbium.
Claim 14
Dependent Claim 44 words
The method of claim 7 further including the step of choosing the fluorescent substance for said first slurry from a group consisting of yttrium venadate doped with europium, yttrium oxide doped with europium, yttrium sulphoxide doped with europium, and calcium silicate doped with manganese.
Claim 15
Dependent Claim 35 words
The method of claim 7 further including the step of choosing the fluorescent substance for said second slurry from a group consisting of zinc sulphide doped with silver, calcium tungstate, and barium-magnesium-aluminate doped with europium.
Claim 16
Dependent Claim 59 words
The method of claim 7 further including the step of choosing the fluorescent substance for said third slurry from a group consisting of zinc cadmium sulphide doped with copper, zinc sulphide doped with silver, zinc cadmium sulphide doped with silver, zinc silicate doped with manganese, zinc oxide, and gadolinium sulphoxide doped with terbium, and lanthanum sulphoxide doped with terbium.

References Cited (Backward Citations)

DE1139875B Cited
DE1447791A1 Cited
US3484269A Cited
DE1462853B2 Cited
US3593678A Cited
DE1537483A1 Cited
DE2219261A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-01-06 1984-07-07 1985-01-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-01-06 1988-07-07 1989-01-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-01-06 1992-07-07 1993-01-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag