US4243656A Expired / Lapsed US ⏱️ 0.0 years remaining

Biosynthetic polymeric compositions

Assignee: Individual
•
Filing: 1979-05-09
•
Granted: 1981-01-06
•
Expires: 1999-05-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Biosynthetic polymeric compositions containing polyacrylate polymer, humectants such as glycerol, proteinaceous material such as gelatin, and water are prepared. The compositions are suitable for treatment of burns or other wounds and may be applied directly or in the form of a prepared film. The film may include a strengthening nylon mesh matrix.

Inventors

  • 👤 Erwin G. Walliczek

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 16:21
CPC Classifications
A; A61; A61L; A61L26/00; A61L26/0009; A61L26/0052; A61L26/0028; A61L26/0038; C; C08; C08L; C08L33/00

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 84 words
A biosynthetic polymeric composition adapted to form a vapor permeable film, said composition including: (a) 10% to 40% by weight of a water dispersible acrylic polymer containing from 50 to 500 monomeric units; (b) 2% to 30% by weight of a humectant selected from the group consisting of glycerol, polyethylene glycol, and propyl 1, 2 diol; (c) 0.5% to 20% by weight of a material selected from a group consisting of gelatin, gum acacia, and albumin; and (d) 30% to 87.5% by weight water.
Claim 2
Dependent Claim 84 words
A biosynthetic polymeric composition adapted to form a vapor permeable film, said composition including: (a) 10% to 40% by weight of a water dispersible acrylic polymer containing from 50 to 500 monomeric units; (b) 2% to 30% by weight of a humectant selected from the group consisting of glycerol, polyethylene glycol, and propyl 1, 2 diol; (c) 0.5% to 20% by weight of a material selected from a group consisting of gelatin, gum acacia, and albumin; and (d) 30% to 87.5% by weight water.
Claim 3
Independent Claim 112 words
A method of producing a vapor permeable biosynthetic polymeric film for use as a wound dressing said method comprising: (a) preparing a composition consisting of: (i) 10% to 40% by weight of a water dispersible acrylic polymer containing from 50 to 500 monomeric units; (ii) 2% to 30% by weight of a humectant selected from the group consisting of glycerol, polyethylene glycol, and propyl 1, 2 diol; (iii) 0.5% to 20% by weight of a material selected from a group consisting of gelatin, gum acacia, and albumin; and (iv) 30% to 87.5% by weight water; and (b) pouring said composition into a liquid film and allowing said film to polymerize and harden.
Claim 4
Independent Claim 112 words
A method of producing a vapor permeable biosynthetic polymeric film for use as a wound dressing said method comprising: (a) preparing a composition consisting of: (i) 10% to 40% by weight of a water dispersible acrylic polymer containing from 50 to 500 monomeric units; (ii) 2% to 30% by weight of a humectant selected from the group consisting of glycerol, polyethylene glycol, and propyl 1, 2 diol; (iii) 0.5% to 20% by weight of a material selected from a group consisting of gelatin, gum acacia, and albumin; and (iv) 30% to 87.5% by weight water; and (b) pouring said composition into a liquid film and allowing said film to polymerize and harden.
Claim 5
Dependent Claim 25 words
A method according to claim 2 which further comprises dispersing in said liquid film a strengthening mesh matrix to increase the strength of said film.
Claim 6
Independent Claim 106 words
A method of producing a vapor permeable biosynthetic polymeric film for use as a wound dressing, said method comprising the application to a wound of a composition including; (a) 10% to 40% by weight of a water dispersable acrylic polymer containing from 50 to 500 monomeric units; (b) 2% to 30% by weight of a humectant selected from the group consisting of glycerol, polyethylene glycol, and propyl 1, 2 diol; (c) 0.5% to 20% by weight of a material selected from a group consisting of gelatin, gum acacia, and albumin; and (d) 30 to 87.5% by weight water and allowing said composition to polymerize and harden.
Claim 7
Independent Claim 106 words
A method of producing a vapor permeable biosynthetic polymeric film for use as a wound dressing, said method comprising the application to a wound of a composition including; (a) 10% to 40% by weight of a water dispersable acrylic polymer containing from 50 to 500 monomeric units; (b) 2% to 30% by weight of a humectant selected from the group consisting of glycerol, polyethylene glycol, and propyl 1, 2 diol; (c) 0.5% to 20% by weight of a material selected from a group consisting of gelatin, gum acacia, and albumin; and (d) 30 to 87.5% by weight water and allowing said composition to polymerize and harden.
Claim 8
Dependent Claim 16 words
A method according to claim 4 wherein said application comprises brushing said composition on said wound.
Claim 9
Dependent Claim 16 words
A method according to claim 4 wherein said application comprises spraying said composition on said wound.
Claim 10
Dependent Claim 21 words
A method according to claim 5 or 6 wherein said wound is a burn up to and including the second degree.

References Cited (Backward Citations)

US3579628A Cited
US3963685A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-01-06 1984-07-07 1985-01-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-01-06 1988-07-07 1989-01-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-01-06 1992-07-07 1993-01-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag