← Back to Patent Explorer
US4241111A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for consecutively coating both sides of web

Assignee: Fujifilm Holdings Corp
•
Filing: 1978-08-11
•
Granted: 1980-12-23
•
Expires: 1998-08-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for consecutively coating both sides of a continuously travelling web, which comprises coating a first coating solution onto a first side of a continuously travelling web to form a coated layer thereon, supplying a second coating solution while the coated layer on the first side of the travelling web is still in a non-dry state, using a bar which is supported by a supporting member and which rotates in contact with the web in the same direction as the travelling direction of the web in such a manner that a liquid pool of the second coating solution is formed immediately before the position where the bar comes into contact with the web while supporting the first coated side of the web with a pressurized gas, and applying the second coating solution to the second side of the web opposite to the first coated side using the bar.

Inventors

  • 👤 Ken Hamamura
  • 👤 Masuo Kabutomori
  • 👤 Eiichi Ohta
  • 👤 Hiroki Saito

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 05:40
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/74; B; B05; B05C; B05C1/00; B05C1/04; B05C1/08; B05C1/0826; B05C9/00; B05C9/04; B05D; B05D1/00; B05D1/36; B05D1/26; B05D1/28; B05D2252/00; B05D2252/02; B05D2252/10; B05D3/00; B05D3/04; B05D3/0493; B05D7/00; B05D7/02; B05D7/04; G03C2001/7403; G03C2001/7411; G03C2001/7425; G03C2001/7433; G03C2001/7459

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 251 words
A process for consecutively coating both sides of a continuously traveilling web, said process comprising: coating a first coating solution onto a first side of a continuously travelling web, to form a first coated layer thereon, supporting said first coated side of said web by a pressurized gas, and supplying a second coating solution to the second side of said web while said first coated side of said travelling web is supported with said pressurized gas, and while said web is still in a non-dry state, the improvement wherein: said step of supplying a second coating solution comprises: supporting a rotatable bar for rotation about its axis at right angles to the direction of web movement and being peripherally grooved in the direction of bar rotation, for rotating contact with said web on said second side, forming a liquid pool of said second coating solution upstream of said moving web and between said rotating bar and a portion of said web supported by said pressurized gas, and rotating said peripherally grooved rotatable bar at a peripheral speed in excess of the velocity of web movement in the same direction as the travelling direction of said web, to pick up a sufficient amount of said coating liquid to cause said second coating solution to flow onto said second side of said travelling web, over the grooved periphery of said rotating bar to insure evenness and the absence of longitudinal streaks of said second coating on said second side of said travelling web.
Claim 2
Dependent Claim 251 words
A process for consecutively coating both sides of a continuously traveilling web, said process comprising: coating a first coating solution onto a first side of a continuously travelling web, to form a first coated layer thereon, supporting said first coated side of said web by a pressurized gas, and supplying a second coating solution to the second side of said web while said first coated side of said travelling web is supported with said pressurized gas, and while said web is still in a non-dry state, the improvement wherein: said step of supplying a second coating solution comprises: supporting a rotatable bar for rotation about its axis at right angles to the direction of web movement and being peripherally grooved in the direction of bar rotation, for rotating contact with said web on said second side, forming a liquid pool of said second coating solution upstream of said moving web and between said rotating bar and a portion of said web supported by said pressurized gas, and rotating said peripherally grooved rotatable bar at a peripheral speed in excess of the velocity of web movement in the same direction as the travelling direction of said web, to pick up a sufficient amount of said coating liquid to cause said second coating solution to flow onto said second side of said travelling web, over the grooved periphery of said rotating bar to insure evenness and the absence of longitudinal streaks of said second coating on said second side of said travelling web.
Claim 3
Dependent Claim 19 words
The process of claim 1, wherein said first coating solution and said second coating solution have a different composition.
Claim 4
Dependent Claim 19 words
The process of claim 1, wherein said first coating solution and said second coating solution have the same composition.
Claim 5
Dependent Claim 24 words
The process of claim 1, wherein the coating of said first coating solution is by extrusion coating, curtain coating, bead coating, or fountain coating.
Claim 6
Dependent Claim 19 words
The process of claim 1, wherein said second coating solution has a viscosity of about 100 cp or less.

References Cited (Backward Citations)

US3496005A Cited
US3533833A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-12-23 1984-06-23 1984-12-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-12-23 1988-06-23 1988-12-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-12-23 1992-06-23 1992-12-23 $7700.00 Window Closed / Lapsed