Abstract
Abstract Casting side dam apparatus for use in a twin-belt continuous casting machine. The side dams each comprise a multiplicity of slotted dam blocks strung on a flexible metal band. The dam blocks are each formed of a beryllium-nickel-copper alloy and are resistant to intergranular cracking over a prolonged period of exposure to elevated temperatures ranging from about 300° F. to about 800° F.
Inventors
- 👤 Paul J. Kranz
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-09 05:24
CPC Classifications
B; B22; B22D; B22D11/00; B22D11/06; B22D11/0637; B22D11/0648; B22D11/066
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
203 words
Side dam apparatus adapted for use in a twin-belt continuous casting machine wherein two spaced-apart side dams each revolve in a loop and travel along a casting zone from its input end to its output end between a pair of revolving spaced-apart casting belts thereby defining a moving mold, the side dams returning from the output end to the input end of the casting zone along a return path located away from the casting zone, the side dams each comprising a multiplicity of dam blocks secured to a flexible continuous securing means, the dam blocks each being formed of a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, the blocks being resistant to intergranular cracking over a prolonged period of exposure to elevated temperatures up to about 800° F., said alloy comprising by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of nickel plus beryllium plus copper being 99.5% minimum.
Claim 2
Dependent Claim
203 words
Side dam apparatus adapted for use in a twin-belt continuous casting machine wherein two spaced-apart side dams each revolve in a loop and travel along a casting zone from its input end to its output end between a pair of revolving spaced-apart casting belts thereby defining a moving mold, the side dams returning from the output end to the input end of the casting zone along a return path located away from the casting zone, the side dams each comprising a multiplicity of dam blocks secured to a flexible continuous securing means, the dam blocks each being formed of a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, the blocks being resistant to intergranular cracking over a prolonged period of exposure to elevated temperatures up to about 800° F., said alloy comprising by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of nickel plus beryllium plus copper being 99.5% minimum.
Claim 3
Dependent Claim
36 words
The side dam apparatus of claim 1 wherein the alloy comprises, by weight, 0.2% to 0.6% beryllium,1.4% to 2.1% nickel, and 0 to 0.1% iron, the total of nickel plus beryllium plus copper being 99.5% minimum.
Claim 4
Dependent Claim
130 words
A dam block for use in a twin-belt continuous casting machine comprising a block of a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, the block being resistant to intergranular cracking over a prolonged period of exposure to elevated temperatures up to about 800° F., and means for securing the block to a flexible securing means, said alloy comprising, by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of beryllium plus nickel plus copper being 99.5% minimum.
Claim 5
Dependent Claim
130 words
A dam block for use in a twin-belt continuous casting machine comprising a block of a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, the block being resistant to intergranular cracking over a prolonged period of exposure to elevated temperatures up to about 800° F., and means for securing the block to a flexible securing means, said alloy comprising, by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of beryllium plus nickel plus copper being 99.5% minimum.
Claim 6
Dependent Claim
35 words
The dam block of claim 3 wherein the alloy comprises, by weight, 0.2% to 0.6% beryllium, 1.4% to 2.1% nickel, and 0 to 0.1% iron, the total beryllium plus nickel plus copper being 99.5% minimum.
Claim 7
Dependent Claim
208 words
Method for reducing the incidence of intergranular cracking of dam blocks subject to prolonged periods of exposure to temperatures up to about 800° F., said dam blocks adapted for use in a twin-belt continuous casting machine wherein two spaced-apart side dams each revolve in a loop and travel along a casting zone from its input end to its output end between a pair of revolving spaced-apart casting belts thereby defining a moving mold, the side dams returning from the output end to the input end of the casting zone along a return path located away from the casting zone, the side dams each comprising a multiplicity of said dam blocks secured to a flexible continuous securing means, said method including fabricating said dam blocks from a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, said alloy comprising by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of nickel plus berrylium plus coper being 99.5% minimum.
Claim 8
Dependent Claim
208 words
Method for reducing the incidence of intergranular cracking of dam blocks subject to prolonged periods of exposure to temperatures up to about 800° F., said dam blocks adapted for use in a twin-belt continuous casting machine wherein two spaced-apart side dams each revolve in a loop and travel along a casting zone from its input end to its output end between a pair of revolving spaced-apart casting belts thereby defining a moving mold, the side dams returning from the output end to the input end of the casting zone along a return path located away from the casting zone, the side dams each comprising a multiplicity of said dam blocks secured to a flexible continuous securing means, said method including fabricating said dam blocks from a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, said alloy comprising by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of nickel plus berrylium plus coper being 99.5% minimum.
Claim 9
Dependent Claim
35 words
The method of claim 5 wherein said alloy comprises, by weight, 0.2% to 0.6% beryllium, 1.4% to 2.1% nickel, and 0 to 0.1% iron, the total of nickel plus berrylium plus copper being 99.5% minimum.
Claim 10
Independent Claim
129 words
A method for reducing the incidence of intergranular cracking and chipping of a dam block for use in a twinbelt continuous casting machine subject to prolonged periods of exposure to temperatures up to about 800° F., said method including the employment of dam block fabricated from a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, said alloy comprising by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of nickel plus beryllium plus copper being 99.5% minimum.
Claim 11
Independent Claim
129 words
A method for reducing the incidence of intergranular cracking and chipping of a dam block for use in a twinbelt continuous casting machine subject to prolonged periods of exposure to temperatures up to about 800° F., said method including the employment of dam block fabricated from a copper base alloy comprising beryllium, nickel and copper, the alloy characterized by being a wrought alloy having a hardness in excess of 90 Rockwell B and a conductivity in excess of 35% IACS, said alloy comprising by weight, beryllium in amount in excess of a trace but not more than 0.6% of the alloy, and the nickel in amount greater than the beryllium but not more than 2.1% of the alloy, the total of nickel plus beryllium plus copper being 99.5% minimum.
Claim 12
Dependent Claim
35 words
The method of claim 7 wherein the alloy comprises, by weight, 0.2% to 0.6% beryllium, 1.4% to 2.1% nickel, and 0 to 0.1% iron, the total of beryllium plus nickel plus copper being 99.5% minimum.
References Cited (Backward Citations)
US2167684A
Cited
US2137281A
Cited
US2136212A
Cited
US2289593A
Cited
US2640235A
Cited
US2904860A
Cited
US2978761A
Cited
US3036348A
Cited
US3123874A
Cited
US3142873A
Cited
US3167830A
Cited
US3860057A
Cited
US3864973A
Cited
US3921697A
Cited
US3878883A
Cited
US3949805A
Cited
US3955615A
Cited
US3937270A
Cited
US4002197A
Cited
US3937274A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-12-16 | 1984-06-16 | 1984-12-16 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-12-16 | 1988-06-16 | 1988-12-16 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-12-16 | 1992-06-16 | 1992-12-16 | $7700.00 | Window Closed / Lapsed |