Claims Analysis
Total Claims: 37
Claim 1
Independent Claim
62 words
A treated aggregate composition comprising an aggregate of stone and finely divided particles; water in an amount of at least 1000 gallons per 100 tons of aggregate and a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid in an amount such that the pH of the composition is less than 3.5.
Claim 2
Dependent Claim
62 words
A treated aggregate composition comprising an aggregate of stone and finely divided particles; water in an amount of at least 1000 gallons per 100 tons of aggregate and a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid in an amount such that the pH of the composition is less than 3.5.
Claim 3
Dependent Claim
27 words
A composition as defined by claim 1 wherein the amount of the sulfonic acid source is in the range of 0.5-8 gallons per 100 tons of aggregate.
Claim 4
Dependent Claim
22 words
A composition as defined by claim 1 wherein the amount of water is less than 3,000 gallons per 100 tons of aggregate.
Claim 5
Dependent Claim
19 words
An aggregate composition as defined by claim 1 wherein the aggregate comprises 40-60% stone, and 40-60% finely divided particles.
Claim 6
Dependent Claim
19 words
An aggregate composition as defined by claim 1 wherein the sulfonic acid source contains at least 60% sulfuric acid.
Claim 7
Independent Claim
70 words
A method of treating aggregate comprising contacting said aggregate with water in an amount of at least 1,000 gallons of water per 100 tons of aggregate, combining a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid with said water to form a mixture of aggregate, water, and sulfonic acid source, said mixture having a pH of less than 3.5.
Claim 8
Independent Claim
70 words
A method of treating aggregate comprising contacting said aggregate with water in an amount of at least 1,000 gallons of water per 100 tons of aggregate, combining a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid with said water to form a mixture of aggregate, water, and sulfonic acid source, said mixture having a pH of less than 3.5.
Claim 9
Dependent Claim
27 words
A method as defined in claim 6 wherein said sulfonic acid source is combined in an amount of at least 0.5 gallon per 100 tons of aggregate.
Claim 10
Dependent Claim
26 words
A method as defined in claim 7 wherein said sulfonic acid source is combined in an amount less than 8 gallons per 100 tons of aggregate.
Claim 11
Dependent Claim
27 words
A method as defined in claim 6 wherein said sulfonic acid source is combined in an amount of at least 1 gallon per 100 tons of aggregate.
Claim 12
Dependent Claim
26 words
A method as defined in claim 9 wherein said sulfonic acid source is combined in an amount less than 8 gallons per 100 tons of aggregate.
Claim 13
Independent Claim
98 words
A method of coating aggregate with asphalt to form an asphaltic concrete composition comprising contacting an aggregate of stone and finely divided particles with water in an amount of at least 1,000 gallons of water per 100 tons of aggregate, combining a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid with said water to form a mixture of aggregate in an acid-water solution, said mixture having a pH less than 3.5, and combining asphalt with said aggregate in an amount sufficient to substantially completely coat said aggregate.
Claim 14
Independent Claim
98 words
A method of coating aggregate with asphalt to form an asphaltic concrete composition comprising contacting an aggregate of stone and finely divided particles with water in an amount of at least 1,000 gallons of water per 100 tons of aggregate, combining a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid with said water to form a mixture of aggregate in an acid-water solution, said mixture having a pH less than 3.5, and combining asphalt with said aggregate in an amount sufficient to substantially completely coat said aggregate.
Claim 15
Dependent Claim
22 words
A method as defined in claim 11 further including removing a majority of said acid-water solution before combining asphalt with said aggregate.
Claim 16
Dependent Claim
24 words
A method as defined in claim 12 wherein at least 95% of said acid-water solution is removed prior to contacting said aggregate with asphalt.
Claim 17
Dependent Claim
21 words
A method as defined in claim 13 wherein said aggregate is substantially completely dried prior to contacting said aggregate with asphalt.
Claim 18
Independent Claim
65 words
A method of preparing an asphaltic composition comprising admixing a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid, aggregate, and water in an amount of at least 1,000 gallons of water per 100 tons of aggregate, heating the composition to at least 210° F., coating the composition with hot asphalt, and compacting said composition.
Claim 19
Independent Claim
65 words
A method of preparing an asphaltic composition comprising admixing a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid, aggregate, and water in an amount of at least 1,000 gallons of water per 100 tons of aggregate, heating the composition to at least 210° F., coating the composition with hot asphalt, and compacting said composition.
Claim 20
Dependent Claim
21 words
A method as defined by claim 15 including adding said sulfonic acid source to said aggregate and thereafter adding the asphalt.
Claim 21
Dependent Claim
21 words
A method as defined by claim 16 wherein the sulfonic acid source is added after heating the aggregate to 150°-350° F.
Claim 22
Dependent Claim
27 words
A method as defined by claim 15 wherein the sulfonic acid source is added in an amount of at least 0.5 gallon per 100 tons of aggregate.
Claim 23
Dependent Claim
27 words
A method as defined by claim 15 wherein the sulfonic acid source is added in an amount of at least 1.0 gallon per 100 tons of aggregate.
Claim 24
Dependent Claim
30 words
A method as defined by claim 15 wherein the sulfonic acid source is added in an amount sufficient to adjust the pH of the asphaltic composition to less than 3.5.
Claim 25
Dependent Claim
30 words
A method as defined by claim 15 wherein the sulfonic acid source is added in an amount sufficient to adjust the pH of the asphaltic composition to less than 2.
Claim 26
Dependent Claim
31 words
A method as defined by claim 15 wherein the sulfonic acid source is added in an amount sufficient to adjust the pH of the asphaltic composition to between 1 and 2.
Claim 27
Independent Claim
96 words
A method of making a hot asphaltic composition comprising admixing a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid, an aggregate of stone and finely divided material, and water in an amount of at least 1,000 gallons per ton of aggregate to form a treated aggregate having a pH of less then 3.5, heating the aggregate to 150°-350° F., adding asphalt to the aggregate in an amount of about 0.5-6% based on the combined weight of aggregate and asphalt to form a hot asphalt composition.
Claim 28
Independent Claim
96 words
A method of making a hot asphaltic composition comprising admixing a sulfonic acid source selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid, an aggregate of stone and finely divided material, and water in an amount of at least 1,000 gallons per ton of aggregate to form a treated aggregate having a pH of less then 3.5, heating the aggregate to 150°-350° F., adding asphalt to the aggregate in an amount of about 0.5-6% based on the combined weight of aggregate and asphalt to form a hot asphalt composition.
Claim 29
Dependent Claim
29 words
A method as defined by claim 23 wherein the sulfonic acid source is added in an amount such that the pH of the asphaltic composition is less than 2.
Claim 30
Dependent Claim
30 words
A method as defined by claim 23 wherein the sulfonic acid source is added in an amount such that the pH of the asphaltic composition is between 1 and 2.
Claim 31
Dependent Claim
25 words
A method as defined by claim 23 wherein the water is added in an amount of 1,000 to 3,000 gallons per 100 tons of aggregate.
Claim 32
Dependent Claim
70 words
Method of rejuvenating worn asphaltic paving which comprises preheating said paving to a temperature from about 300° F. to about 500° F., rolling said preheated paving with a wheeled roller while applying concurrently an aqueous sulfonic acid solution selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid in an amount such that the pH of the paving surface composition is 3.5 or less.
Claim 33
Dependent Claim
70 words
Method of rejuvenating worn asphaltic paving which comprises preheating said paving to a temperature from about 300° F. to about 500° F., rolling said preheated paving with a wheeled roller while applying concurrently an aqueous sulfonic acid solution selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid in an amount such that the pH of the paving surface composition is 3.5 or less.
Claim 34
Dependent Claim
20 words
Method of claim 27 wherein the surface of the paving is maintained at a pH of from 1 to 2.
Claim 35
Dependent Claim
91 words
Method of recycling existing asphaltic paving in situ which comprises breaking the paving into pieces of a size suitable for spreading and leveling with a grader blade, admixing said pieces with an aqueous sulfonic acid solution, said sulfonic acid selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid at a temperature of at least 140° F. to achieve a composition having a pH of 3.5 or less, and spreading and rolling said composition of a temperature of 200°-250° F. to form an asphaltic paving.
Claim 36
Dependent Claim
91 words
Method of recycling existing asphaltic paving in situ which comprises breaking the paving into pieces of a size suitable for spreading and leveling with a grader blade, admixing said pieces with an aqueous sulfonic acid solution, said sulfonic acid selected from the group consisting of sulfuric acid sludge, spent sulfuric sludge, and spent sulfuric acid at a temperature of at least 140° F. to achieve a composition having a pH of 3.5 or less, and spreading and rolling said composition of a temperature of 200°-250° F. to form an asphaltic paving.
Claim 37
Dependent Claim
18 words
Method of claim 29 wherein the sulfonic acid solution is at a temperature of at least 200° F.