Abstract
Abstract By reacting polyalkyl-piperidones-4 with the 0.5- to 1.1-molar amount of formaldehyde in the presence of an aliphatic monoalcohol at 50° to 180° C., polymers of a polymerization degree of from 2 to about 200 are obtained, which may be hydrogenated or partially hydrogenated. Especially in this form, they are suitable as light stabilizers for synthetic polymers and as intermediate products for the preparation of other stabilizers for plastic materials.
Inventors
- 👤 Hartmut Wiezer
- 👤 Helmut Korbanka
- 👤 Gerhard Pfahler
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 00:26
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/16; C08K5/34; C07; C07D; C07D211/00; C07D211/04; C07D211/68; C07D211/72; C07D211/74; C08G; C08G16/00; C08G16/02; C08G16/025; C08G16/0268; C08L; C08L101/00
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
149 words
A process for the preparation of polyalkyl-piperidine/formaldehyde polymers which comprises reacting a polyalkyl-piperidone-4 of the formula (I) ##STR6## in which R 1 is hydrogen, oxygen or C 1 -C 12 -alkyl, R 2 and R 3 are either identical and represent hydrogen or a C 1 -C 5 -alkyl group, R 4 being a methyl group in this case; or R 2 is hydrogen or C 1 -C 5 -alkyl, and R 3 and R 4 together with the carbon atoms linked to them form a C 5 or C 6 cycloalkyl group, or a group of the formula ##STR7## with the 0.5- to 1.1-fold molar amount of paraformaldehyde at a temperature of from 50° to 180° C. in the presence of an aliphatic C 1 -C 10 -monoalcohol and of an alkaline base, and subsequently optionally hydrogenating the product obtained either completely or partially according to known processes.
Claim 2
Dependent Claim
149 words
A process for the preparation of polyalkyl-piperidine/formaldehyde polymers which comprises reacting a polyalkyl-piperidone-4 of the formula (I) ##STR6## in which R 1 is hydrogen, oxygen or C 1 -C 12 -alkyl, R 2 and R 3 are either identical and represent hydrogen or a C 1 -C 5 -alkyl group, R 4 being a methyl group in this case; or R 2 is hydrogen or C 1 -C 5 -alkyl, and R 3 and R 4 together with the carbon atoms linked to them form a C 5 or C 6 cycloalkyl group, or a group of the formula ##STR7## with the 0.5- to 1.1-fold molar amount of paraformaldehyde at a temperature of from 50° to 180° C. in the presence of an aliphatic C 1 -C 10 -monoalcohol and of an alkaline base, and subsequently optionally hydrogenating the product obtained either completely or partially according to known processes.
Claim 3
Dependent Claim
26 words
Polyalkyl-piperidine/formaldehyde polymers of a polymerization degree of from 2 to about 200 and the hydrogenation or partial hydrogenation products thereof, obtained as claimed in claim 1.
Claim 4
Dependent Claim
46 words
A process for stabilizing synthetic polymers against the damaging influence of light, which comprises adding to the polymer from 0.01 to 5 parts by weight, relative to the polymer, of a polymer stabilizer as claimed in claim 2, optionally in addition to hitherto known stabilizing substances.
Claim 5
Dependent Claim
28 words
Synthetic polymers stabilized against UV decomposition, which contain from 0.01 to 5 parts by weight, relative to the polymer, of a polymer stabilizer as claimed in claim 2.
References Cited (Backward Citations)
US4139520A
Cited
US4154722A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-11-18 | 1984-05-19 | 1984-11-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-11-18 | 1988-05-19 | 1988-11-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-11-18 | 1992-05-19 | 1992-11-18 | $7700.00 | Window Closed / Lapsed |