Abstract
Abstract Aqueous coating compositions comprising latices containing a copolymer of vinyl acetate in the range of about 95-99.9% by weight and maleic anhydride in the range of about 0.1-5% by weight have been found to have improved starch binder compatibility. Vinyl acetate and maleic anhydride are polymerized in an aqueous medium in the presence of a free radical initiator and a surfactant which prevents the vinyl acetate-maleic anhydride copolymer from dissolving in the aqueous medium. The resulting latex coating compositions have a high solids content (greater than about 50% by weight) and a copolymer particle size of under 0.5 microns in addition to the excellent starch compatibility.
Inventors
- 👤 Wallace H. Pippin
- 👤 Wiley E. Daniels
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 03:39
CPC Classifications
C; C09; C09D; C09D131/00; C09D131/02; C09D131/04; C09D103/00; C09D103/02
Claims Analysis
Total Claims: 20
Claim 1
Independent Claim
93 words
A coating composition comprising a latex which contains a copolymer of vinyl acetate in the range of about 95 to 99.9% by weight and maleic anhydride in the range of about 5.0 to 0.1% by weight polymerized in an aqueous medium in the presence of a surfactant which prevents the resulting vinyl acetate-maleic anhydride copolymer from becoming solubilized in said aqueous medium and a free radical initiator, said latex being characterized by having a solids content of at least 50% by weight and a copolymer particle size of not more than 0.5 micron.
Claim 2
Dependent Claim
93 words
A coating composition comprising a latex which contains a copolymer of vinyl acetate in the range of about 95 to 99.9% by weight and maleic anhydride in the range of about 5.0 to 0.1% by weight polymerized in an aqueous medium in the presence of a surfactant which prevents the resulting vinyl acetate-maleic anhydride copolymer from becoming solubilized in said aqueous medium and a free radical initiator, said latex being characterized by having a solids content of at least 50% by weight and a copolymer particle size of not more than 0.5 micron.
Claim 3
Dependent Claim
13 words
The coating composition of claim 1 wherein said surfactant is an anionic surfactant.
Claim 4
Dependent Claim
17 words
The coating composition of claim 1 wherein said surfactant is a combination of anionic and nonionic surfactants.
Claim 5
Dependent Claim
24 words
The coating composition of claim 1 wherein said surfactant is a water soluble surfactant containing 10 to 22 carbon atoms in its hydrophobic moiety.
Claim 6
Dependent Claim
20 words
The coating composition of claim 4 wherein said surfactant contains at least four ethylene oxide units in its hydrophilic moiety.
Claim 7
Dependent Claim
13 words
The coating composition of claim 4 wherein said surfactant is an anionic surfactant.
Claim 8
Dependent Claim
13 words
The coating composition of claim 5 wherein said surfactant is an anionic surfactant.
Claim 9
Dependent Claim
69 words
The coating composition of claim 1 wherein said surfactant is a water soluble anionic surfactant having the general formula: R(OCH.sub.2 CH.sub.2).sub.n XM wherein R is an alkyl, alkaryl or cyclic alkyl radical having 10 to 22 carbon atoms, X is a sulfate, sulfonate, sulfosuccinate or phosphate radical, M is an alkali metal, an alkaline earth metal or an ammonium radical, and n is an interger of 4 to 30.
Claim 10
Dependent Claim
14 words
The coating composition of claim 8 wherein said surfactant also contains a non-ionic surfactant.
Claim 11
Dependent Claim
32 words
The coating composition of claim 1 wherein mineral pigments are contained therein so that the weight ratio of the mineral pigments to said latex is in the range of 3.33:1 to 50:1.
Claim 12
Dependent Claim
98 words
A coating composition comprising a latex which contains a copolymer of vinyl acetate in the range of about 98 to 99.6% by weight and maleic anhydride in the range of about 2 to 0.4% by weight polymerized in an aqueous medium in the presence of a water soluble anionic surfactant which prevents the resulting vinyl acetate-maleic anhydride copolymer from becoming solubilized in said aqueous medium and a free radical initiator, said coating composition being characterized by having a solids content of at least 55% by weight and a particle size in the range of 0.05 to 0.3 micron.
Claim 13
Dependent Claim
98 words
A coating composition comprising a latex which contains a copolymer of vinyl acetate in the range of about 98 to 99.6% by weight and maleic anhydride in the range of about 2 to 0.4% by weight polymerized in an aqueous medium in the presence of a water soluble anionic surfactant which prevents the resulting vinyl acetate-maleic anhydride copolymer from becoming solubilized in said aqueous medium and a free radical initiator, said coating composition being characterized by having a solids content of at least 55% by weight and a particle size in the range of 0.05 to 0.3 micron.
Claim 14
Dependent Claim
41 words
The coating composition of claim 11 wherein a portion of the latex is replaced by starch so that the final composition contains up to 9 parts by weight starch to 1 part by weight latex without substantial loss of binding strength.
Claim 15
Dependent Claim
41 words
The coating composition of claim 11 wherein a portion of the latex is replaced by starch so that the final composition contains up to 3 parts by weight starch to 1 part by weight latex without substantial loss of binding strength.
Claim 16
Dependent Claim
32 words
The coating composition of claim 11 wherein mineral pigments are contained therein so that the weight ratio of the mineral pigments to said latex is in the range of 3.33:1 to 50:1.
Claim 17
Dependent Claim
109 words
A coating composition comprising 3.33 to 50 parts by weight of mineral pigments and one part by weight latex which contains a copolymer prepared by copolymerizing vinyl acetate in the range of about 95 to 99.9 parts by weight and maleic anhydride in the range of about 5.0 to 0.1 parts by weight in an aqueous medium in the presence of a surfactant which prevents the resulting vinyl acetate-maleic anhydride copolymer from becoming solubilized in said aqueous medium and a free radical initiator, said coating composition being characterized by having a solids content of at least 50% by weight and a particle size of not more than 0.5 micron.
Claim 18
Dependent Claim
109 words
A coating composition comprising 3.33 to 50 parts by weight of mineral pigments and one part by weight latex which contains a copolymer prepared by copolymerizing vinyl acetate in the range of about 95 to 99.9 parts by weight and maleic anhydride in the range of about 5.0 to 0.1 parts by weight in an aqueous medium in the presence of a surfactant which prevents the resulting vinyl acetate-maleic anhydride copolymer from becoming solubilized in said aqueous medium and a free radical initiator, said coating composition being characterized by having a solids content of at least 50% by weight and a particle size of not more than 0.5 micron.
Claim 19
Dependent Claim
38 words
The coating composition of claim 15 wherein said vinyl acetate is in the range of about 98 to 99.6 parts by weight and said maleic anhydride is in the range of about 2.0 to 0.4 parts by weight.
Claim 20
Dependent Claim
21 words
The coating composition of claim 15 wherein at least a part of said maleic anhydride has become converted to maleic acid.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-10-14 | 1984-04-14 | 1984-10-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-10-14 | 1988-04-14 | 1988-10-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-10-14 | 1992-04-14 | 1992-10-14 | $7700.00 | Window Closed / Lapsed |