Direct casting method for producing low-stress glass/plastic composite lenses

Assignee: Corning Glass Works
•
Filing: 1979-04-05
•
Granted: 1980-10-14
•
Expires: 1999-04-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A glass-plastic composite lens combining a glass element with a high-shrinkage thermosetting plastic is provided in accordance with a direct casting process comprising a consolidation heating step, subsequent to plastic curing and shrinkage, during which a thermoplastic coating between the glass element and the cured plastic bonds the assembly into a unitary low-stress composite.

Inventors

  • 👤 Anton A. Spycher

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 05:16
CPC Classifications
G; G02; G02C; G02C7/00; G02C7/02; B; B29; B29D; B29D11/00; B29D11/0073; Y; Y10; Y10S; Y10S359/00; Y10S359/90

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 205 words
A direct casting method for producing an optically clear, optical-distortion-free composite lens comprising a glass element bonded to a high-shrinkage thermosetting plastic element, with low residual stress between the glass and plastic elements, which comprises the steps of: (a) providing selected surface portions of the glass element with a solid coating of a thermoplastic adhesive having a heat sealing temperature above the minimum curing temperature of the thermosetting plastic, said coating being solid, of uniform thickness, and essentially non-adhesive with respect to said thermosetting plastic at a curing temperature for said thermosetting plastic; (b) casting the thermosetting plastic in liquid form against the surface portions of the glass element which have been provided with the coating of thermoplastic adhesive while maintaning the uniform thickness and solid character of said coating of thermoplastic adhesive; (c) curing the thermosetting plastic by heating the plastic, the glass element and the coating of thermoplastic adhesive to a temperature below the heat sealing temperature of the thermoplastic adhesive but above the minimum curing temperature of the thermosetting plastic; and (d) consolidating the cured thermosetting plastic, thermoplastic adhesive, and glass element to a unitary glass-plastic composite by heating them to a temperature above the heat sealing temperature of the thermoplastic adhesive.
Claim 2
Dependent Claim 205 words
A direct casting method for producing an optically clear, optical-distortion-free composite lens comprising a glass element bonded to a high-shrinkage thermosetting plastic element, with low residual stress between the glass and plastic elements, which comprises the steps of: (a) providing selected surface portions of the glass element with a solid coating of a thermoplastic adhesive having a heat sealing temperature above the minimum curing temperature of the thermosetting plastic, said coating being solid, of uniform thickness, and essentially non-adhesive with respect to said thermosetting plastic at a curing temperature for said thermosetting plastic; (b) casting the thermosetting plastic in liquid form against the surface portions of the glass element which have been provided with the coating of thermoplastic adhesive while maintaning the uniform thickness and solid character of said coating of thermoplastic adhesive; (c) curing the thermosetting plastic by heating the plastic, the glass element and the coating of thermoplastic adhesive to a temperature below the heat sealing temperature of the thermoplastic adhesive but above the minimum curing temperature of the thermosetting plastic; and (d) consolidating the cured thermosetting plastic, thermoplastic adhesive, and glass element to a unitary glass-plastic composite by heating them to a temperature above the heat sealing temperature of the thermoplastic adhesive.
Claim 3
Dependent Claim 19 words
A method in accordance with claim 1 wherein the glass element has a thickness not exceeding about 0.020 inches.
Claim 4
Dependent Claim 15 words
A method in accordance with claim 1 wherein the thermoplastic adhesive consists of polyvinyl butyral.
Claim 5
Dependent Claim 18 words
A method in accordance with claim 1 wherein the high-shrinkage thermosetting plastic is an allyl diglycol carbonate plastic.

References Cited (Backward Citations)

US2047253A Cited
US2976197A Cited
US3135645A Cited
US3987449A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-10-14 1984-04-14 1984-10-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-10-14 1988-04-14 1988-10-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-10-14 1992-04-14 1992-10-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag