Method for preventing the degradation of a hydrophilic colloid solution for silver halide photographic light-sensitive material
Assignee: Fujifilm Holdings Corp
•
Filing: 1978-08-03
•
Granted: 1980-09-23
•
Expires: 1998-08-03
Abstract
Abstract A method for preventing the degradation of a hydrophilic colloid solution for a silver halide photographic light-sensitive material of which the viscosity has been or is to be increased using an anionic polymer containing an acid group, which comprises incorporating into the hydrophilic colloid solution at least one compound represented by the formula (I): ##STR1## wherein R.sub. represents a hydrogen atom or an alkyl group; and R 2 , R 3 and R 4 , which may be the same or different, each represents a hydrogen atom, a halogen atom, an alkyl group or an alkoxy group.
Inventors
- 👤 Yuzo Toda
- 👤 Keiichi Adachi
- 👤 Shoji Ishiguro
- 👤 Yasuhiro Nakayama
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 16:10
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/005; G03C1/06; G03C1/04; G03C1/37; Y; Y10; Y10S; Y10S430/00; Y10S430/136; Y10S430/14
Claims Analysis
Total Claims: 15
Claim 1
Independent Claim
175 words
A method for preventing the degradation of a hydrophilic colloid solution by the action of bacteria, mold or yeast for a silver halide photographic light-sensitive material, in which the viscosity of the solution thereof has been or is to be increased using an anionic polymer containing an acid group, whereafter said hydrophilic colloid solution is used in a multi-coating process at a speed of about 20 m/min or more, which comprises incorporating into said hydrophilic colloid solution at least one compound represented by the formula (I): ##STR6## wherein R 1 represents a hydrogen atom or an alkyl group; and R 2 , R 3 and R 4 , which may be the same or different, each represents a hydrogen atom, a halogen atom, an alkyl group or an alkoxy group and, increasing said viscosity if said viscosity has not already been increased by the addition of said anionic polymer by adding said anionic polymer containing an acid group to said hydrophilic colloid soluton, whereby said degradation is prevented without any adverse effect on viscosity increase.
Claim 2
Independent Claim
175 words
A method for preventing the degradation of a hydrophilic colloid solution by the action of bacteria, mold or yeast for a silver halide photographic light-sensitive material, in which the viscosity of the solution thereof has been or is to be increased using an anionic polymer containing an acid group, whereafter said hydrophilic colloid solution is used in a multi-coating process at a speed of about 20 m/min or more, which comprises incorporating into said hydrophilic colloid solution at least one compound represented by the formula (I): ##STR6## wherein R 1 represents a hydrogen atom or an alkyl group; and R 2 , R 3 and R 4 , which may be the same or different, each represents a hydrogen atom, a halogen atom, an alkyl group or an alkoxy group and, increasing said viscosity if said viscosity has not already been increased by the addition of said anionic polymer by adding said anionic polymer containing an acid group to said hydrophilic colloid soluton, whereby said degradation is prevented without any adverse effect on viscosity increase.
Claim 3
Dependent Claim
15 words
The method of claim 1, wherein said hydrophilic colloid is gelatin or a gelatin derivative.
Claim 4
Dependent Claim
15 words
The method of claim 1, wherein R 1 through R 4 are all hydrogen atoms.
Claim 5
Dependent Claim
23 words
The method of claim 1, wherein said anionic polymer is a polymer having a sulfonyl group, a carboxyl group or a sulfato group.
Claim 6
Dependent Claim
31 words
The method of claim 1, wherein said compound is incorporated in an amount of about 1×10 -2 to about 2.5×10 -1 wt% based on the dry weight of the hydrophilic colloid.
Claim 7
Dependent Claim
27 words
The method of claim 4, wherein said anionic polymer is at least one polymer selected from a polystyrene sulfonic acid salt and a cellulose sulfuric acid salt.
Claim 8
Dependent Claim
12 words
The method of claim 1, wherein the viscosity has already been increased.
Claim 9
Dependent Claim
20 words
The method of claim 1, wherein the viscosity has not been increased and is increased by adding said anionic polymer.
Claim 10
Dependent Claim
37 words
The method of claim 1, wherein the acid group is at least one sulfonic acid group, carboxylic acid group or sulfonic acid group, and the acid group is present in a side chain of the anionic polymer.
Claim 11
Dependent Claim
56 words
The method of claim 9, wherein the anionic polymer containing an acid group is selected from polymers or copolymers of monomers from the class consisting of styrene sulfonic acid, 2-acrylamido-2-methylpropane sulfonic acid, acrylic acid, methacrylic acid, maleic acid, half esters of maleic acid, phosphoric acid mono esters of hydroxyethyl acrylate and a cellulose sulfuric acid salt.
Claim 12
Dependent Claim
29 words
The method of claim 9, wherein the anionic polymer containing an acid group is selected from the class consisting of polystyrene sodium sulfonate, sodium polyacrylate and sodium cellulose sulfate.
Claim 13
Dependent Claim
33 words
The method of claim 10, wherein the anionic polymer having an acid group is present in an amount of 1 to 100 wt % based on the dry weight of the hydrophilic colloid.
Claim 14
Dependent Claim
33 words
The method of claim 11, wherein the anionic polymer having an acid group is present in an amount of 1 to 100 wt % based on the dry weight of the hydrophilic colloid.
Claim 15
Dependent Claim
29 words
The method of claim 1, wherein the compound of general formula (I) and the anionic polymer having an acid group are present in a non-light sensitive hydrophilic colloid solution.
References Cited (Backward Citations)
US2870015A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-09-23 | 1984-03-24 | 1984-09-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-09-23 | 1988-03-24 | 1988-09-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-09-23 | 1992-03-24 | 1992-09-23 | $7700.00 | Window Closed / Lapsed |