Abstract

Abstract A method for preventing the deposition of sulfide and/or sulfate scale during the production of a hot two-phase geothermal fluid which contains hydrogen sulfide, barium heavy and/or transition metals, and at least a critical minimum amount of calcium in solution. Gaseous oxygen is injected into the geothermal fluid at a critical rate to selectively oxidize the hydrogen sulfide to intermediate sulfide oxidation products, such as thiosulfates. Thereafter the geothermal fluid is separated into gaseous and liquid phases. Where iron is present in the geothermal fluid, the degree of turbulence induced during the oxidation step is selectively controlled in order to prevent the deposition of iron pyrites.

Inventors

  • 👤 John W. Jost

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 09:46
CPC Classifications
C; C02; C02F; C02F1/00; C02F1/72

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 170 words
A method for preventing scale deposition from a hydrogen sulfide-containing, two-phase geothermal fluid, comprising: (a) flowing from a subterranean formation through a well to the earth surface a hot two-phase geothermal fluid comprised of (1) a hydrogen sulfide-containing vapor phase and (2) a liquid phase contaning dissolved hydrogen sulfide, dissolved barium and dissolved heavy and/or transition metals; (b) injecting into the geothermal fluid which also contains at least about 10 moles of dissolved calcium per mole of hydrogen sulfide a gas comprised of oxygen at a rate sufficient to provide therein an oxygen to hydrogen sulfide molar ratio between about 0.75 and about 1.75, and mixing said gas with said geothermal fluid so as to selectively oxidize said hydrogen sulfide to sulfur and/or water soluble sulfide oxidation products wherein the sulfur has a valence less than plus six; and (c) thereafter separating said two-phase geothermal fluid into (1) a gaseous phase comprised of steam and noncondensible gases and (2) a hot brine containing said sulfur and/or water-soluble sulfide oxidation products.
Claim 2
Independent Claim 170 words
A method for preventing scale deposition from a hydrogen sulfide-containing, two-phase geothermal fluid, comprising: (a) flowing from a subterranean formation through a well to the earth surface a hot two-phase geothermal fluid comprised of (1) a hydrogen sulfide-containing vapor phase and (2) a liquid phase contaning dissolved hydrogen sulfide, dissolved barium and dissolved heavy and/or transition metals; (b) injecting into the geothermal fluid which also contains at least about 10 moles of dissolved calcium per mole of hydrogen sulfide a gas comprised of oxygen at a rate sufficient to provide therein an oxygen to hydrogen sulfide molar ratio between about 0.75 and about 1.75, and mixing said gas with said geothermal fluid so as to selectively oxidize said hydrogen sulfide to sulfur and/or water soluble sulfide oxidation products wherein the sulfur has a valence less than plus six; and (c) thereafter separating said two-phase geothermal fluid into (1) a gaseous phase comprised of steam and noncondensible gases and (2) a hot brine containing said sulfur and/or water-soluble sulfide oxidation products.
Claim 3
Dependent Claim 35 words
The method defined in claim 1 wherein said gas is injected at a rate selected to provide an oxygen to hydrogen sulfide molar ratio between about 1.0 and about 1.5 in said two-phase geothermal fluid.
Claim 4
Dependent Claim 30 words
The method defined in claim 1 wherein said hydrogen sulfide is oxidized in step (b) to water-soluble sulfide oxidation products consisting essentially of thiosulfate anions, bisulfite anions and polythionate anions.
Claim 5
Dependent Claim 11 words
The method defined in claim 1 wherein said gas is air.
Claim 6
Dependent Claim 29 words
The method defined in claim 1 wherein said liquid phase contains at least about 50 moles of dissolved calcium per mole of hydrogen sulfide in said two-phase geothermal fluid.
Claim 7
Dependent Claim 19 words
The method defined in claim 1 wherein said liquid phase contains at least about 1000 ppm of dissolved calcium.
Claim 8
Dependent Claim 54 words
The method defined in claim 1 wherein said liquid phase contains at least about 1 ppm of dissolved iron, and wherein said method further comprises the step of selectively controlling the degree of turbulence during the mixing of said gas and said two-phase geothermal fluid so as to avoid the formation of iron pyrites.
Claim 9
Dependent Claim 72 words
The method defined in claim 7 wherein said gas is injected into a conduit conducting said two-phase geothermal fluid from the well to a wellhead separator and wherein the mixing of said gas and said geothermal fluid is controlled by passing the combined fluids through a plurality of restriction orifices mounted in said conduit each of which orifices induces a pressure drop of about 5 p.s.i. on the combined fluid flowing therethrough.
Claim 10
Dependent Claim 81 words
The method defined in claim 1 wherein the geothermal fluid produced from said subterranean formation contains less than about 10 moles of dissolved calcium per mole of hydrogen sulfide, and wherein said method further comprises the step of adding a source of calcium ions to said geothermal fluid prior to step (b) to thereby increase the calcium ion concentration of said liquid phase to at least about 10 moles of dissolved calcium per mole of hydrogen sulfide in said geothermal fluid.
Claim 11
Independent Claim 184 words
A method for preventing scale deposition from a hydrogen sulfide-containing, two-phase geothermal fluid, comprising: (a) flowing through a conduit and into a gas/liquid separator a hot two-phase geothermal fluid comprised of (1) a hydrogen sulfide-containing vapor phase and (2) a liquid phase containing dissolved hydrogen sulfide, dissolved barium, dissolved heavy and/or transition metals and at least about 1,000 ppm of dissolved calcium, said calcium comprising at least about 10 moles of dissolved calcium per mole of hydrogen sulfide in said geothermal fluid; (b) injecting into said geothermal fluid flowing through said conduit a gas comprised of oxygen at a rate selected to provide therein an oxygen to hydrogen sulfide molar ratio between about 0.75 and about 1.75; (c) mixing said gas with said geothermal fluid in said conduit so as to selectively oxidize said hydrogen sulfide to water-soluble intermediate sulfide oxidation products consisting essentially of thiosulfate anions, bisulfite anions and polythionate anions; and (d) thereafter separating said two-phase geothermal fluid in said gas/liquid separator into (1) a gaseous phase comprised of steam and noncondensible gases and (2) a hot brine containing said oxidation products.
Claim 12
Independent Claim 184 words
A method for preventing scale deposition from a hydrogen sulfide-containing, two-phase geothermal fluid, comprising: (a) flowing through a conduit and into a gas/liquid separator a hot two-phase geothermal fluid comprised of (1) a hydrogen sulfide-containing vapor phase and (2) a liquid phase containing dissolved hydrogen sulfide, dissolved barium, dissolved heavy and/or transition metals and at least about 1,000 ppm of dissolved calcium, said calcium comprising at least about 10 moles of dissolved calcium per mole of hydrogen sulfide in said geothermal fluid; (b) injecting into said geothermal fluid flowing through said conduit a gas comprised of oxygen at a rate selected to provide therein an oxygen to hydrogen sulfide molar ratio between about 0.75 and about 1.75; (c) mixing said gas with said geothermal fluid in said conduit so as to selectively oxidize said hydrogen sulfide to water-soluble intermediate sulfide oxidation products consisting essentially of thiosulfate anions, bisulfite anions and polythionate anions; and (d) thereafter separating said two-phase geothermal fluid in said gas/liquid separator into (1) a gaseous phase comprised of steam and noncondensible gases and (2) a hot brine containing said oxidation products.
Claim 13
Dependent Claim 25 words
The method defined in claim 10 wherein said gas is air, and said heavy and/or transition metals are manganese, iron, copper, silver, lead and/or zinc.
Claim 14
Dependent Claim 42 words
The method defined in claim 10 wherein said liquid phase contains at least about 1 ppm of dissolved iron and wherein, during step (c), the degree of turbulence caused by said mixing is selectively controlled to avoid the formation of iron pyrites.
Claim 15
Dependent Claim 29 words
The method defined in claim 12 wherein said mixing is provided by flowing said gas and said geothermal fluid through a plurality of restriction orifices mounted in said conduit.
Claim 16
Independent Claim 263 words
A method for preventing scale deposition from a hydrogen sulfide-containing, two-phase geothermal fluid, comprising: (a) flowing from a subterranean geothermal reservoir through a well to the earth surface a hot two-phase geothermal fluid comprised of (1) a hydrogen sulfide-containing vapor phase and (2) a liquid phase containing dissolved hydrogen sulfide, dissolved barium, dissolved iron, dissolved heavy and/or transition metals and at least about 5,000 ppm of dissolved calcium, said calcium comprising at least about 50 moles of dissolved calcium per mole of hydrogen sulfide in said geothermal fluid; (b) flowing said geothermal fluid through a conduit containing between about 2 and about 5 restriction orifices and into a gas/liquid separator, each of said orifices being sized to induce about a 5 p.s.i. drop in the pressure of the fluid flowing therethrough; (c) injecting air into said geothermal fluid through at least one injection nozzle mounted in said conduit so as to discharge said air into said geothermal fluid at a point upstream of said restriction orifices, said air being injected at a rate selected to provide therein an oxygen to hydrogen sulfide molar ratio between about 1.0 and about 1.5, whereby in flowing through the restriction orifices in said conduit said air is mixed with said geothermal fluid so as to selectively oxidize said hydrogen sulfide to water-soluble sulfide oxidation products consisting essentially of thiosulfate anions, bisulfite anions and polythionate anions; and (d) thereafter separating said two-phase geothermal fluid in said gas/liquid separator into (1) a gaseous phase comprised of steam and noncondensible gases and (2) a hot brine containing said oxidation products.
Claim 17
Independent Claim 263 words
A method for preventing scale deposition from a hydrogen sulfide-containing, two-phase geothermal fluid, comprising: (a) flowing from a subterranean geothermal reservoir through a well to the earth surface a hot two-phase geothermal fluid comprised of (1) a hydrogen sulfide-containing vapor phase and (2) a liquid phase containing dissolved hydrogen sulfide, dissolved barium, dissolved iron, dissolved heavy and/or transition metals and at least about 5,000 ppm of dissolved calcium, said calcium comprising at least about 50 moles of dissolved calcium per mole of hydrogen sulfide in said geothermal fluid; (b) flowing said geothermal fluid through a conduit containing between about 2 and about 5 restriction orifices and into a gas/liquid separator, each of said orifices being sized to induce about a 5 p.s.i. drop in the pressure of the fluid flowing therethrough; (c) injecting air into said geothermal fluid through at least one injection nozzle mounted in said conduit so as to discharge said air into said geothermal fluid at a point upstream of said restriction orifices, said air being injected at a rate selected to provide therein an oxygen to hydrogen sulfide molar ratio between about 1.0 and about 1.5, whereby in flowing through the restriction orifices in said conduit said air is mixed with said geothermal fluid so as to selectively oxidize said hydrogen sulfide to water-soluble sulfide oxidation products consisting essentially of thiosulfate anions, bisulfite anions and polythionate anions; and (d) thereafter separating said two-phase geothermal fluid in said gas/liquid separator into (1) a gaseous phase comprised of steam and noncondensible gases and (2) a hot brine containing said oxidation products.

References Cited (Backward Citations)

US4044830A Cited
US3963611A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-09-23 1984-03-24 1984-09-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-09-23 1988-03-24 1988-09-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-09-23 1992-03-24 1992-09-23 $7700.00 Window Closed / Lapsed