Abstract

Abstract A method for butt welding of austenitic stainless steel piping with forced cooling of the inside by the flow of a cooling medium comprises the steps of initially welding the pipe ends together by a root pass prior to the inflow of the cooling medium so as to prevent leakage of the medium to the outside, introducing an insert for constraining the flow of the cooling medium into the pipe, and welding the junction while forcing the medium to flow through the space between the insert and the surrounding wall of the pipe, the insert constructed so that it increases the flow velocity of the cooling medium to the maximum in the vicinity of the welded joint being formed.

Inventors

  • 👤 Isao Masaoka
  • 👤 Katsuyuki Imai

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 12:12
CPC Classifications
B; B23; B23K; B23K9/00; B23K9/02; B23K9/028; B23K9/0282; B23K37/00; B23K37/003

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 206 words
A method for butt welding austenitic stainless steel piping with forced cooling of the inside by the flow of a cooling liquid, which comprises the steps of initially welding the pipe ends of the austenitic stainless steel piping together by a root pass prior to the inflow of said cooling liquid so as to prevent leakage of said liquid to the outside, introducing an insert for forcibly changing the flow pattern of said cooling liquid into said piping, and welding the junction while forcing said liquid to flow through the space between said insert and the surrounding wall of said piping, wherein said insert is a column, cylinder, or cone having an outside diameter smaller than the inside diameter of said steel piping, and which forms a minimum constrained flow path between itself and the surrounding wall of said piping over a length of at least 25 mm from said welded joint being formed toward the outlet for said cooling liquid, said insert being constructed so that it increases the flow velocity of said cooling liquid to the maximum in the vicinity of the welded joint being formed, whereby the welded joint being formed is cooled to reduce chromium carbide precipitation and tensile residual stresses thereat.
Claim 2
Independent Claim 206 words
A method for butt welding austenitic stainless steel piping with forced cooling of the inside by the flow of a cooling liquid, which comprises the steps of initially welding the pipe ends of the austenitic stainless steel piping together by a root pass prior to the inflow of said cooling liquid so as to prevent leakage of said liquid to the outside, introducing an insert for forcibly changing the flow pattern of said cooling liquid into said piping, and welding the junction while forcing said liquid to flow through the space between said insert and the surrounding wall of said piping, wherein said insert is a column, cylinder, or cone having an outside diameter smaller than the inside diameter of said steel piping, and which forms a minimum constrained flow path between itself and the surrounding wall of said piping over a length of at least 25 mm from said welded joint being formed toward the outlet for said cooling liquid, said insert being constructed so that it increases the flow velocity of said cooling liquid to the maximum in the vicinity of the welded joint being formed, whereby the welded joint being formed is cooled to reduce chromium carbide precipitation and tensile residual stresses thereat.
Claim 3
Dependent Claim 42 words
A method according to claim 1, wherein the diameter of the insert increases from upstream of the junction to a point immediately under the junction, whereby the cooling liquid is diverted before the junction and impinges at an angle against the junction.
Claim 4
Independent Claim 186 words
A method for butt welding austenitic stainless steel piping with forced cooling of the inside by the flow of a cooling liquid, which comprises the steps of initially welding the pipe ends of the austenitic stainless steel piping together by a root pass prior to the inflow of said cooling liquid so as to prevent leakage of said liquid to the outside, introducing an insert for forcibly changing the flow pattern of said cooling liquid into said piping, and welding the junction while forcing said liquid to flow through the space between said insert and the surrounding wall of said piping, said insert being constructed so that it increases the flow velocity of said cooling liquid to the maximum in the vicinity of the welded joint being formed, whereby the welded joint being formed is cooled to reduce chromium carbide precipitation and tensile residual stresses thereat, wherein said insert is provided with a plurality of partitions on the outer surface, whereby said cooling liquid is flown substantially uniformly between said insert and said weld in the surrounding wall of said piping while welding is in progress.
Claim 5
Independent Claim 186 words
A method for butt welding austenitic stainless steel piping with forced cooling of the inside by the flow of a cooling liquid, which comprises the steps of initially welding the pipe ends of the austenitic stainless steel piping together by a root pass prior to the inflow of said cooling liquid so as to prevent leakage of said liquid to the outside, introducing an insert for forcibly changing the flow pattern of said cooling liquid into said piping, and welding the junction while forcing said liquid to flow through the space between said insert and the surrounding wall of said piping, said insert being constructed so that it increases the flow velocity of said cooling liquid to the maximum in the vicinity of the welded joint being formed, whereby the welded joint being formed is cooled to reduce chromium carbide precipitation and tensile residual stresses thereat, wherein said insert is provided with a plurality of partitions on the outer surface, whereby said cooling liquid is flown substantially uniformly between said insert and said weld in the surrounding wall of said piping while welding is in progress.
Claim 6
Dependent Claim 23 words
A method according to claim 3, wherein said partitions arranged axially of said insert protrude radially from said outer surface of said insert.
Claim 7
Dependent Claim 19 words
A method according to claim 3, wherein said partitions are spirally secured to said outer surface of said insert.
Claim 8
Independent Claim 172 words
A method for butt welding austenitic stainless steel piping with forced cooling of the inside by the flow of a cooling liquid, which comprises the steps of initially welding the pipe ends of the austenitic stainless steel piping together by a root pass prior to the inflow of said cooling liquid so as to prevent leakage of said liquid to the outside, introducing an insert for forcibly changing the flow pattern of said cooling liquid into said piping, and welding the junction while forcing said cooling liquid, by means of said insert, to impinge upon the welded joint being formed, at right angles thereto, and then flow through the constrained flow path formed between said insert and the surrounding wall of said piping over distances of at least 25 mm each upstream and downstream from said joint being formed, said constrained flow path being substantially parallel longitudinally to the surrounding wall of said piping, whereby the welded joint being formed is cooled to reduce chromium carbide precipitation and tensile residual stresses thereat.
Claim 9
Independent Claim 172 words
A method for butt welding austenitic stainless steel piping with forced cooling of the inside by the flow of a cooling liquid, which comprises the steps of initially welding the pipe ends of the austenitic stainless steel piping together by a root pass prior to the inflow of said cooling liquid so as to prevent leakage of said liquid to the outside, introducing an insert for forcibly changing the flow pattern of said cooling liquid into said piping, and welding the junction while forcing said cooling liquid, by means of said insert, to impinge upon the welded joint being formed, at right angles thereto, and then flow through the constrained flow path formed between said insert and the surrounding wall of said piping over distances of at least 25 mm each upstream and downstream from said joint being formed, said constrained flow path being substantially parallel longitudinally to the surrounding wall of said piping, whereby the welded joint being formed is cooled to reduce chromium carbide precipitation and tensile residual stresses thereat.
Claim 10
Dependent Claim 76 words
A method according to claim 6, wherein said insert has a length of at least 25 mm each upstream and downstream from the plane across the center of the annular weld and has an outside diameter smaller than the inside diameter of said piping, with a diametral cooling liquid passage formed midway to cause impingement of said liquid upon said weld, said insert including a cooling liquid inlet pipe extended therethrough in communication with said passage.
Claim 11
Dependent Claim 52 words
A method according to claim 7, wherein said cooling liquid passage formed diametrally in said insert to cause impingement of said liquid upon said weld is provided with a plurality of radially arranged partitions, whereby said cooling liquid is forced to impinge substantially uniformly upon said weld while welding is in progress.
Claim 12
Dependent Claim 18 words
A method according to claim 7, wherein said diametral cooling liquid passage is gradually narrowed toward its periphery.
Claim 13
Dependent Claim 35 words
A method according to claim 7, wherein the diametral cooling liquid passage is constructed such that it forces the cooling liquid to impinge substantially uniformly upon said weld over the entire circumference of the piping.

References Cited (Backward Citations)

US2259367A Cited
US2574003A Cited
US3802681A Cited
US4152568A Cited
JPS5222539A Cited
DE2758528A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-08-19 1984-02-18 1984-08-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-08-19 1988-02-18 1988-08-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-08-19 1992-02-18 1992-08-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag