Abstract
Abstract The invention provides an improved wireline that comprises one or more insulated conductors contained within a smooth walled metal sheath; which improved wireline is satisfactory to perform all of the normal wireline operations in an earth borehole and particularly in very deep boreholes; and in which the sheath material of the wireline is a metal having a high yield strength to weight ratio, and the sheath is swaged into intimate contact with the inner insulated conductor or conductors, such that the weight of the inner conductor or conductors and insulation is effectively supported by the sheath.
Inventors
- 👤 William D. Smith
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-01 12:30
CPC Classifications
E; E21; E21B; E21B17/00; E21B17/003; E21B17/20; G; G02; G02B; G02B6/00; G02B6/44; G02B6/4479; G02B6/4486; G02B6/4488; H; H01; H01B; H01B13/00; H01B13/0006; H01B7/00; H01B7/16; H01B7/17; H01B7/18; H01B7/20; H01B7/207; Y; Y10; Y10S; Y10S359/00; Y10S359/90; Y10T; Y10T29/00; Y10T29/49; Y10T29/49826; Y10T29/49908; Y10T29/49925; Y10T29/49927; Y10T29/49929
Claims Analysis
Total Claims: 24
Claim 1
Independent Claim
181 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material the tensile strength of which can be raised by cold working and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting said predetermined number of insulated conductors within said tubing, said conductors being of a length substantially the same as that of the tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; said tubing after swaging having a tensile strength above that of mild steel.
Claim 2
Independent Claim
181 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material the tensile strength of which can be raised by cold working and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting said predetermined number of insulated conductors within said tubing, said conductors being of a length substantially the same as that of the tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; said tubing after swaging having a tensile strength above that of mild steel.
Claim 3
Dependent Claim
23 words
The method of claim 1 wherein said tubing after swaging has a yield strength to weight ratio of at least fifteen to one.
Claim 4
Dependent Claim
13 words
The method of claim 1 wherein said tubing is made of stainless steel.
Claim 5
Independent Claim
171 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material the tensile strength of which can be raised by cold working and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting while making said tubing said predetermined number of insulated conductors within said tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; said tubing after swaging having a tensile strength above that of mild steel.
Claim 6
Independent Claim
171 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material the tensile strength of which can be raised by cold working and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting while making said tubing said predetermined number of insulated conductors within said tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; said tubing after swaging having a tensile strength above that of mild steel.
Claim 7
Dependent Claim
42 words
The method of claim 4 wherein said tubing is made from a strip of material that is formed into generally tubular shape as said conductors are inserted, then closed to tubular shape and the seam welded, all prior to the swaging step.
Claim 8
Dependent Claim
23 words
The method of claim 5 wherein said tubing after swaging has a yield strength to weight ratio of at least fifteen to one.
Claim 9
Dependent Claim
13 words
The method of claim 5 wherein said strip of material is stainless steel.
Claim 10
Dependent Claim
20 words
The method of claim 5 wherein said tubing is drawn after welding the seam and prior to the swaging step.
Claim 11
Dependent Claim
23 words
The method of claim 8 wherein said tubing after swaging has a yield strength to weight ratio of at least fifteen to one.
Claim 12
Dependent Claim
13 words
The method of claim 8 wherein said strip of material is stainless steel.
Claim 13
Independent Claim
191 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material having a high strength to weight ratio after swaging and heat treating and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting said predetermined number of insulated conductors within said tubing, said conductors being of a length substantially the same as that of the tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; d. heat treating the swaged tubing; said tubing, after swaging and heat treating having a tensile strength above that of mild steel.
Claim 14
Independent Claim
191 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material having a high strength to weight ratio after swaging and heat treating and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting said predetermined number of insulated conductors within said tubing, said conductors being of a length substantially the same as that of the tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; d. heat treating the swaged tubing; said tubing, after swaging and heat treating having a tensile strength above that of mild steel.
Claim 15
Dependent Claim
26 words
The method of claim 11 wherein said tubing after swaging and heat treating has a yield strength to weight ratio of at least fifteen to one.
Claim 16
Dependent Claim
13 words
The method of claim 11 wherein said tubing is made of carbon steel.
Claim 17
Independent Claim
181 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material having a high strength to weight ratio after swaging and heat treating and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting while making said tubing, said predetermined number of insulated conductors within said tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; d. heat treating the swaged tubing, said tubing, after swaging and heat treating having a tensile strength above that of mild steel.
Claim 18
Independent Claim
181 words
The method of making a wireline suitable for use with wireline apparatus for use in earth boreholes and wherein a wireline is utilized to suspend a downhole tool in a borehole from aboveground cable drum and winch means and to transmit electrical signals between said tool and aboveground equipment, said method comprising the steps of: a. making a continuous piece of smooth walled metal tubing of a material having a high strength to weight ratio after swaging and heat treating and having an inside diameter such that a predetermined number of insulated conductors can be inserted into said tubing; b. inserting while making said tubing, said predetermined number of insulated conductors within said tubing; c. swaging by means of hammering action said tubing into intimate contact with said insulated conductor or conductors, such that it or they are supported by said tubing and consequently can be of length greater than could be supported by said conductor or conductors alone; d. heat treating the swaged tubing, said tubing, after swaging and heat treating having a tensile strength above that of mild steel.
Claim 19
Dependent Claim
42 words
The method of claim 14 wherein said tubing is made from a strip of material that is formed into generally tubular shape as said conductors are inserted, then closed to tubular shape and the seam welded, all prior to the swaging step.
Claim 20
Dependent Claim
26 words
The method of claim 15 wherein said tubing after swaging and heat treating has a yield strength to weight ratio of at least fifteen to one.
Claim 21
Dependent Claim
13 words
The method of claim 16 wherein said strip of material is carbon steel.
Claim 22
Dependent Claim
20 words
The method of claim 15 wherein said tubing is drawn after welding the seam and prior to the swaging step.
Claim 23
Dependent Claim
26 words
The method of claim 18 wherein said tubing after swaging and heat treating has a yield strength to weight ratio of at least fifteen to one.
Claim 24
Dependent Claim
13 words
The method of claim 19 wherein said strip of material is carbon steel.
References Cited (Backward Citations)
US1227346A
Cited
US1794902A
Cited
US2644353A
Cited
US2606849A
Cited
US2975087A
Cited
US2998472A
Cited
US3430330A
Cited
US3583060A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-07-29 | 1984-01-28 | 1984-07-29 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-07-29 | 1988-01-28 | 1988-07-29 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-07-29 | 1992-01-28 | 1992-07-29 | $7700.00 | Window Closed / Lapsed |