Abstract
Abstract Electrochemical storage cell of the alkali metal and chalcogen type with an anode and a cathode chamber separated by a solid electrolyte wall and confined by a metal wall. A first current collector has an outer sub-part which extends outside the reactant chamber enclosed by the solid electrolyte, and an inner sub-part which extends into the interior of this reactant chamber. The outer sub-part and the inner sub-part are connected to an electrically conducting contact element which melts at a predetermined temperature exceeding the operating temperature of the cell. A second current collector is formed by part of the metal wall which confines the other reactant chamber.
Inventors
- 👤 Henner Meinhold
- 👤 Wilhelm Haar
- 👤 Wilfried Fischer
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 18:11
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/36; H01M10/39; H01M10/3909; H01M50/00; H01M50/50; H01M50/572; H01M50/574; H01M50/581; H01H; H01H37/00; H01H37/74; H01H37/76; H01H37/761; Y; Y02; Y02E; Y02E60/00; Y02E60/10
Claims Analysis
Total Claims: 22
Claim 1
Independent Claim
168 words
Electrochemical storage cell having an anode chamber for an alkali metal anolyte as a reactant and a cathode chamber for a chalcogen catholyte as a second reactant, which chambers are separated from each other by an alkali ion-conducting solid electrolyte wall, with one reactant chamber defined by the solid electrolyte wall and the other reactant chamber confined, at least in part by a metal wall, an electrode as a first current collector extending from outside the reactant chamber defined by the solid-electrolyte wall to the interior of said reactant chamber, and a second current collector formed by part of said metal wall which confines the chamber containing the other reactant, the improvement comprising said first current collector having an outer sub-part which extends outside the reactant chamber and an inner sub-part which extends into the interior of said reactant chamber, and the outer sub-part and the inner sub-part connected to an electrically conducting contact element which melts at a predetermined temperature exceeding the operating temperature of the cell.
Claim 2
Dependent Claim
168 words
Electrochemical storage cell having an anode chamber for an alkali metal anolyte as a reactant and a cathode chamber for a chalcogen catholyte as a second reactant, which chambers are separated from each other by an alkali ion-conducting solid electrolyte wall, with one reactant chamber defined by the solid electrolyte wall and the other reactant chamber confined, at least in part by a metal wall, an electrode as a first current collector extending from outside the reactant chamber defined by the solid-electrolyte wall to the interior of said reactant chamber, and a second current collector formed by part of said metal wall which confines the chamber containing the other reactant, the improvement comprising said first current collector having an outer sub-part which extends outside the reactant chamber and an inner sub-part which extends into the interior of said reactant chamber, and the outer sub-part and the inner sub-part connected to an electrically conducting contact element which melts at a predetermined temperature exceeding the operating temperature of the cell.
Claim 3
Dependent Claim
50 words
Electrochemical storage cell according to claim 1, wherein the cell has a metal lid and the inner sub-part is directly connected to the inside of the metal lid of the cell and the outer sub-part is connected to the outside of the metal lid via the electrically conducting contact element.
Claim 4
Dependent Claim
27 words
Electrochemical storage cell according to claim 1, wherein the melting point of the contact element is 20° to 100° K. above the operating temperature of the cell.
Claim 5
Dependent Claim
34 words
Electrochemical storage cell according to claim 2, wherein the outer sub-part of the current collector is in electrically conducting contact with the metal lid of the cell via the contact element and a spring.
Claim 6
Dependent Claim
20 words
Electrochemical storage cell according to claim 4, wherein the outer sub-part is held at the metal lid by a bracket.
Claim 7
Dependent Claim
18 words
Electrochemical storage cell according to claim 5, wherein the outer sub-part is in the shape of a plunger.
Claim 8
Dependent Claim
31 words
Electrochemical storage cell according to claim 6, wherein the plunger-shaped lower surface of the outer sub-part, the contact element and the spring are arranged between the bracket and the metal lid.
Claim 9
Dependent Claim
25 words
Electrochemical storage cell according to claim 7, wherein the spring is bent in the shape of a frame in which the contact element is set.
Claim 10
Dependent Claim
30 words
Electrochemical storage cell according to claim 8, wherein the metal lid, the spring, the contact element and the outer sub-part are connected to each other in an electrically conducting manner.
Claim 11
Dependent Claim
18 words
Electrochemical storage cell according to claim 9, wherein the inner sub-part is directly connected to the metal lid.
Claim 12
Dependent Claim
33 words
Electrochemical storage cell according to claim 1, wherein the outer sub-part is disposed on the outside of the metal lid and is directly connected to the metal lid in an electrically conducting manner.
Claim 13
Dependent Claim
27 words
Electrochemical storage cell according to claim 11, wherein the melting point of the contact element is 20° to 100° K. above the operating temperature of the cell.
Claim 14
Dependent Claim
39 words
Electrochemical storage cell according to claim 1, wherein the inner sub-part is connected to the metal lid in a conducting manner via the contact element and extends into the interior of said reactant chamber defined by the solid electrolyte.
Claim 15
Dependent Claim
27 words
Electrochemical storage cell according to claim 13, wherein the melting point of the contact element is 20° to 100° K. above the operating temperature of the cell.
Claim 16
Dependent Claim
45 words
Electrochemical storage cell according to claim 1, or claim 11, or claim 13, wherein the inner sub-part, at its end which connects to the contact element, has an inward-pointing recess with a capacity which is slightly larger than the volume of the melted contact element.
Claim 17
Dependent Claim
60 words
Electrochemical storage cell according to claim 1, or claim 11, or claim 13, wherein the inner sub-part, at its end which connects to the contact element, has an inward-pointing recess with a capacity which is slightly larger than the volume of the melted contact element, and wherein the inner sub-part is fastened to the metal lid by a nonconducting sleeve.
Claim 18
Dependent Claim
74 words
Electrochemical storage cell according to claim 1, or claim 11, or claim 13, wherein the inner sub-part, at its end which connects to the contact element, has an inward-pointing recess with a capacity which is slightly larger than the volume of the melted contact element, and wherein the inner sub-part is fastened to the metal lid by a nonconducting sleeve with the sleeve surrounding the contact element and the end of the inner sub-part.
Claim 19
Dependent Claim
142 words
Electrochemical storage cell of the alkali metal and chalcogen type, with an anode chamber for anolyte as a reactant and a cathode chamber for catholyte as a reactant, which reactant chambers are separated from each other by an alkali ion-conducting solid electrolyte wall and are confined by a metal wall housing, wherein a first current collector is an electrode which conductively extends from outside to the metal wall into the reactant chamber bounded by the solid-electrolyte wall and the metal wall housing, and a second current collector extending into the interior of reactant chamber defined by the solid electrolyte wall, the improvement comprising disposing an electrical conducting contact element in electrical conducting contact with the metal housing which forms in part the first current collector, said electrically conducting contact element melting at a predetermined temperature exceeding the operating temperature of the cell.
Claim 20
Dependent Claim
142 words
Electrochemical storage cell of the alkali metal and chalcogen type, with an anode chamber for anolyte as a reactant and a cathode chamber for catholyte as a reactant, which reactant chambers are separated from each other by an alkali ion-conducting solid electrolyte wall and are confined by a metal wall housing, wherein a first current collector is an electrode which conductively extends from outside to the metal wall into the reactant chamber bounded by the solid-electrolyte wall and the metal wall housing, and a second current collector extending into the interior of reactant chamber defined by the solid electrolyte wall, the improvement comprising disposing an electrical conducting contact element in electrical conducting contact with the metal housing which forms in part the first current collector, said electrically conducting contact element melting at a predetermined temperature exceeding the operating temperature of the cell.
Claim 21
Dependent Claim
47 words
Electrochemical storage cell according to claim 18, wherein the first current collector is formed by the metal housing and a pipe clamp and between them a ring of nonconducting material on the outside of the metal housing and a ring-shaped contact element connected to the metal housing.
Claim 22
Dependent Claim
39 words
Electrochemical storage cell according to claim 18, or claim 19, wherein the ring-shaped contact element is made of metal or an alloy, with a melting point which is 20° to 100° K. above the operating temperature of the cell.
References Cited (Backward Citations)
US3758337A
Cited
US4011366A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-06-10 | 1983-12-10 | 1984-06-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-06-10 | 1987-12-10 | 1988-06-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-06-10 | 1991-12-10 | 1992-06-10 | $7700.00 | Window Closed / Lapsed |