← Back to Patent Explorer
US4207140A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of producing groundwood pulp

Assignee: Mo och Domsjo AB
•
Filing: 1978-10-25
•
Granted: 1980-06-10
•
Expires: 1998-10-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process is provided for preparing groundwood pulp from debarked pulpwood logs, which comprises grinding the logs under a superatmospheric pressure of a gas selected from the group consisting of steam, air, and steam and air, while continuously supplying thereto water comprising spent bleaching liquor at a temperature of at least 70 DEG C. and forming a pulp suspension in the resulting aqueous liquor; centrifugally separating steam from the pulp suspension and using the separated hot steam to heat spent bleaching liquor supplied for the grinding; thickening the pulp suspension to a concentration within the range from about 5 to about 40% and supplying water separated therefrom to the grinding; diluting the pulp suspension to a concentration within the range from about 0.5 to about 4.0%; screening the pulp suspension; thickening the pulp suspension to a concentration within the range from about 10 to about 50% and supplying water separated therefrom to the screening; adding bleaching chemicals to the pulp and bleaching the pulp; diluting the bleached pulp with spent bleaching liquor to a concentration within the range from about 1 to about 6%; thickening the bleached pulp suspension to a concentration within the range from about 10 to about 50%; and separating, heating and recycling to the grinding spent bleaching liquor containing residual bleaching chemicals.

Inventors

  • 👤 Jonas A. I. Lindahl

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 05:11
CPC Classifications
D; D21; D21C; D21C9/00; D21C9/10; D21C9/1026; D21B; D21B1/00; D21B1/04; D21B1/12; D21B1/14; D21B1/16

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 232 words
A process for preparing groundwood pulp of improved quality and with reduced energy requirements, which comprises: (1) grinding debarked pulpwood logs under a superatmospheric pressure of a gas selected from the group consisting of steam, air and steam and air while continuously supplying thereto water and spent bleaching liquor at a temperature of at least 70° C. and forming a pulp suspension in the resulting aqueous liquor; (2) centrifugally separating steam from the pulp suspension and using the separated hot steam to heat the spent bleaching liquor supplied to the grinding; (3) thickening the pulp suspension to a pulp concentration within the range from about 5 to about 40% and supplying water separated therefrom to the grinding; (4) diluting the pulp suspension to a pulp concentration within the range from about 0.5 to about 4.0%; (5) screening the pulp suspension; (6) thickening the pulp suspension to a pulp concentration within the range from about 10 to about 50% and supplying water separated therefrom to the screening; (7) adding bleaching chemicals thereto and bleaching the pulp; (8) diluting the bleached pulp with spent bleaching liquor to a pulp concentration within the range from about 1 to about 6%; (9) thickening the bleached pulp suspension to a pulp concentration within the range from about 10 to about 50%; and (10) separating, heating and recycling to the grinder spent bleaching liquor containing residual bleaching chemicals.
Claim 2
Dependent Claim 232 words
A process for preparing groundwood pulp of improved quality and with reduced energy requirements, which comprises: (1) grinding debarked pulpwood logs under a superatmospheric pressure of a gas selected from the group consisting of steam, air and steam and air while continuously supplying thereto water and spent bleaching liquor at a temperature of at least 70° C. and forming a pulp suspension in the resulting aqueous liquor; (2) centrifugally separating steam from the pulp suspension and using the separated hot steam to heat the spent bleaching liquor supplied to the grinding; (3) thickening the pulp suspension to a pulp concentration within the range from about 5 to about 40% and supplying water separated therefrom to the grinding; (4) diluting the pulp suspension to a pulp concentration within the range from about 0.5 to about 4.0%; (5) screening the pulp suspension; (6) thickening the pulp suspension to a pulp concentration within the range from about 10 to about 50% and supplying water separated therefrom to the screening; (7) adding bleaching chemicals thereto and bleaching the pulp; (8) diluting the bleached pulp with spent bleaching liquor to a pulp concentration within the range from about 1 to about 6%; (9) thickening the bleached pulp suspension to a pulp concentration within the range from about 10 to about 50%; and (10) separating, heating and recycling to the grinder spent bleaching liquor containing residual bleaching chemicals.
Claim 3
Dependent Claim 45 words
A process according to claim 1 in which only water and spent bleaching liquor from the process are supplied to the grinding, and only hot steam or water from the process are applied to heat the spent bleaching liquor and water supplied to the grinding.
Claim 4
Dependent Claim 31 words
A process according to claim 1 which comprises separately storing the heated spent bleaching liquor and the process water from the first thickening step before mixing and supplying to the grinding.
Claim 5
Dependent Claim 26 words
A process according to claim 1 in which the heated spent bleaching liquor supplied to the grinding is supplied with stabilizers for the bleaching chemicals present.
Claim 6
Dependent Claim 26 words
A process according to claim 1 in which the heated spent bleaching liquor supplied to the grinding is supplied with complexing agents to chelate heavy metals.
Claim 7
Dependent Claim 23 words
A process according to claim 1 in which the heated spent bleaching liquor supplied to the grinding is supplied with fresh bleaching chemicals.
Claim 8
Dependent Claim 42 words
A process according to claim 1 which comprises adjusting the proportion of preheated spent bleaching liquor and process water from the first thickening step within the range from about 1:30 to about 5:1 according to the process heat balance and grinding conditions.
Claim 9
Dependent Claim 23 words
A process according to claim 1 which comprises after grinding separating large wood particles and then separating the steam therefrom in a hydrocyclone.
Claim 10
Dependent Claim 24 words
A process according to claim 1 which comprises separating steam from the grinder and heating therewith the debarked pulpwood logs fed to the grinder.
Claim 11
Dependent Claim 35 words
A process according to claim 1 in which a portion of the process water tapped from the thickening step (3) is carried to a heat exchanger, and from there brought to the screening stage (5).
Claim 12
Dependent Claim 29 words
A process according to claim 1 which comprises filtering the water from the thickening step (3) to separate fibers and other suspended impurities before carrying it to the grinding.
Claim 13
Dependent Claim 33 words
A process according to claim 1 in which the bleaching of the groundwood pulp uses a bleaching agent selected from the group consisting of chlorinating bleaching agents, peroxide bleaching chemicals and sodium dithionite.
Claim 14
Dependent Claim 49 words
A process according to claim 1 in which the bleaching is carried out in a bleaching tower, and the pulp suspension is thickened immediately after mixing with the bleaching chemicals and before introduction into the tower, and the excess bleaching liquor recycled to the bleaching chemicals addition step (7).
Claim 15
Dependent Claim 79 words
A process according to claim 1 in which during the grinding step, the superatmospheric pressure is maintained within the range from about 0.2 to about 10 kp/cm 2 above atmospheric pressure, the temperature of the water or aqueous solution supplied to the grinding is maintained within the range from about 85° to about 100° C., and the pressure of the logs against the grindstone surface is maintained within the range from about 4 to about 40 kp/cm 2 .
Claim 16
Dependent Claim 29 words
A process according to claim 1 in which the groundwood pulp obtained is mixed with chemical pulp, in a proportion within the range from about 1:9 to about 9:1.
Claim 17
Dependent Claim 20 words
A process according to claim 15 in which the groundwood chemical pulp mixture is used for the manufacture of paper.

References Cited (Backward Citations)

GB1266898A Cited
US3808090A Cited
US4029543A Cited
US4082233A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-06-10 1983-12-10 1984-06-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-06-10 1987-12-10 1988-06-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-06-10 1991-12-10 1992-06-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag