US4199490A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Block copolymer latex composition
Assignee: Asahi Kasei Corp
•
Filing: 1977-02-16
•
Granted: 1980-04-22
•
Expires: 1997-02-16
Abstract
Abstract A block copolymer latex composition comprising (A) an aqueous latex containing at least one of block copolymers consisting of conjugated diolefin blocks and monovinyl-substituted aromatic compound blocks prepared by solution-polymerization, and having a molecular weight of 5,000 to 500,000 and a content of monovinyl-substituted aromatic compound of 10 to 70% by weight, and (B) a latex of rubber system, latex of synthetic resin system or a mixture thereof, the composition containing 5 to 87% by weight of (A) and 95 to 13% by weight of (B) in terms of solid matters, has very superior film-forming properties and provides films having improved strength.
Inventors
- 👤 Shunji Kamiya
- 👤 Kunio Satake
- 👤 Tomiho Sone
- 👤 Tsutomu Teraoka
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 17:08
CPC Classifications
C; C08; C08L; C08L53/00; C08L53/02; C08L101/00
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
88 words
A latex composition comprising 63-83% by weight (per solid matter) of (A) an aqueous latex of at least one block copolymer consisting of conjugated diolefin blocks and 10-70% by weight of monovinyl-substituted aromatic compound blocks and having a molecular weight of 5,000-500,000 prepared by solution polymerization, and 37-17% by weight (per solid matter) of (B) a rubber latex, a synthetic resin latex, a mixture of these latices or a latex in which the constitutional elements of the rubber or synthetic resin are modified with carboxyl or hydroxyl groups.
Claim 2
Dependent Claim
88 words
A latex composition comprising 63-83% by weight (per solid matter) of (A) an aqueous latex of at least one block copolymer consisting of conjugated diolefin blocks and 10-70% by weight of monovinyl-substituted aromatic compound blocks and having a molecular weight of 5,000-500,000 prepared by solution polymerization, and 37-17% by weight (per solid matter) of (B) a rubber latex, a synthetic resin latex, a mixture of these latices or a latex in which the constitutional elements of the rubber or synthetic resin are modified with carboxyl or hydroxyl groups.
Claim 3
Dependent Claim
39 words
A latex composition of block copolymer according to claim 1 wherein said monovinyl-substituted aromatic compound is at least one member selected from the group consisting of styrene, o- or p- vinyltoluene, vinylxylene, ethylstyrene, isopropylstyrene, ethylvinyltoluene, tertiary-butylstyrene, diethylstyrene and vinylnaphthalene.
Claim 4
Dependent Claim
30 words
A latex composition of block copolymer according to claim 1 wherein said conjugated diolefin is at least one member selected from the group consisting of 1,3-butadiene, 1,3-pentadiene, isoprene and 2,3-dimethylbutadiene.
Claim 5
Dependent Claim
21 words
A latex composition of block copolymer according to claim 1 wherein said block copolymer consists of 1,3-butadiene blocks and styrene blocks.
Claim 6
Dependent Claim
21 words
A latex composition of block copolymer according to claim 1 wherein said block copolymer consists of isoprene blocks and styrene blocks.
Claim 7
Dependent Claim
60 words
A latex composition of block copolymer according to claim 1 wherein said rubber latex is at least one member selected from the group consisting of natural rubber latex, styrene-butadiene copolymer latex, methyl methacrylate-butadiene copolymer latex, acrylonitrile-butadiene copolymer latex, isoprene-isobutylene copolymer latex, styrene-butadiene-vinylpyridine copolymer latex, ethylene-propylene copolymer latex, ethylene-propylene-diene copolymer latex, chloroprene polymer latex, butadiene polymer latex and isoprene polymer latex.
Claim 8
Dependent Claim
135 words
A latex composition of block copolymer according to claim 1 wherein said synthetic resin type latex is at least one member selected from the group consisting of methyl acrylate polymer latex, ethyl acrylate polymer latex, butyl acrylate polymer latex, 2-ethylhexyl acrylate polymer latex, ethyl acrylate-butyl acrylate copolymer latex, butyl acrylate-2-ethylhexyl acrylate copolymer latex, acrylic acid ester-vinyl acetate copolymer latex, acrylic acid ester-styrene copolymer latex, acrylic acid ester-methyl methacrylate copolymer latex, vinyl acetate polymer latex, vinyl acetate-ethylene copolymer latex, vinyl acetate-ethylene-acrylic acid copolymer latex, vinyl acetate-acrylic acid copolymer latex, vinyl acetate-maleic anhydride copolymer latex, vinyl acetate-maleic acid ester copolymer latex, vinyl acetate-veova copolymer latex, vinyl acetate-vinyl chloride copolymer latex, vinyl acetate-vinyl chloride-acrylic acid copolymer latex, vinyl chloride polymer latex, vinylidene chloride polymer latex, vinyl chloride-vinylidene chloride copolymer latex, urethane polymer latex, polyamide latex and polyester latex.
References Cited (Backward Citations)
GB644022A
Cited
US3265765A
Cited
US3304281A
Cited
US3458602A
Cited
US3293197A
Cited
US3539475A
Cited
US3700757A
Cited
US3878153A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1983-04-22 | 1983-10-22 | 1984-04-22 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1987-04-22 | 1987-10-22 | 1988-04-22 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1991-04-22 | 1991-10-22 | 1992-04-22 | $7700.00 | Window Closed / Lapsed |