Abstract

Abstract A rotary rock drill bit comprising a plurality of cutting elements or cutters mounted in the crown of the drill bit. Each cutting element comprises a thin planar layer of polycrystalline diamond bonded in the crown of the bit at a rake angle of between -10° and -25°. In another embodiment each cutting element comprises an elongated pin mounted at one end in the drill crown and thin layer of polycrystalline diamond bonded to the free end of the pin so as to be disposed at a rake angle of between -10° and -25°.

Inventors

  • 👤 Phillip E. Bonnice

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 18:22
CPC Classifications
B; B22; B22F; B22F7/00; B22F7/06; B22F7/062; B22F7/064; B23; B23P; B23P15/00; B23P15/28; E; E21; E21B; E21B10/00; E21B10/46; E21B10/48; E21B10/56; E21B10/567

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 92 words
A method for making a diamond compact drill bit comprising the steps: (a) mounting a plurality of cutting elements, each comprised of a diamond compact, in a mold; (b) filling a drill crown portion of the mold surrounding said elements with a metal powder; (c) inserting a drill shaft into said mold; (d) filling said portion of said mold surrounding said elements with a molten solder having a flow point of less than 700° C.; (e) allowing said solder to solidify; and (f) removing the drill bit so formed from the mold.
Claim 2
Independent Claim 92 words
A method for making a diamond compact drill bit comprising the steps: (a) mounting a plurality of cutting elements, each comprised of a diamond compact, in a mold; (b) filling a drill crown portion of the mold surrounding said elements with a metal powder; (c) inserting a drill shaft into said mold; (d) filling said portion of said mold surrounding said elements with a molten solder having a flow point of less than 700° C.; (e) allowing said solder to solidify; and (f) removing the drill bit so formed from the mold.
Claim 3
Dependent Claim 34 words
The method of claim 1 wherein said elements are located in said mold so as to dispose said elements at a rake angle between about -10° and -25° in the crown of the bit.
Claim 4
Dependent Claim 12 words
The method of claim 1 wherein said solder is a silver solder.
Claim 5
Dependent Claim 22 words
The method of claim 3 wherein said solder consists of about, by weight, 45% Ag, 15% Cu, 16% Zn, and 24% Cd.
Claim 6
Independent Claim 136 words
A method of making a diamond compact drill bit comprising the steps of: (a) mounting a plurality of diamond compact cutting elements in a mold; (b) filling a drill crown portion of the mold surrounding said elements with a matrix metal powder; (c) inserting a drill shaft into said mold; (d) positioning low temperature alloy material around the drill body at the top of the mold, said alloy having a flow point below the thermal degradation point of said diamond compacts; (e) heating the mold and its contents to a temperature below the thermal degradation point of said diamond compacts to cause said alloy material to melt and flow into the mold cavity; (f) cooling the mold and its contents to solidify the molten alloy; and (g) removing the drill bit so formed from the mold.
Claim 7
Independent Claim 136 words
A method of making a diamond compact drill bit comprising the steps of: (a) mounting a plurality of diamond compact cutting elements in a mold; (b) filling a drill crown portion of the mold surrounding said elements with a matrix metal powder; (c) inserting a drill shaft into said mold; (d) positioning low temperature alloy material around the drill body at the top of the mold, said alloy having a flow point below the thermal degradation point of said diamond compacts; (e) heating the mold and its contents to a temperature below the thermal degradation point of said diamond compacts to cause said alloy material to melt and flow into the mold cavity; (f) cooling the mold and its contents to solidify the molten alloy; and (g) removing the drill bit so formed from the mold.
Claim 8
Dependent Claim 20 words
The method of claim 5 wherein said low temperature alloy has a flow point of less than about 700° C.

References Cited (Backward Citations)

US3175427A Cited
US3407445A Cited
US3726351A Cited
US4006788A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-02-04 1983-08-06 1984-02-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-02-04 1987-08-06 1988-02-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-02-04 1991-08-06 1992-02-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag