Abstract

Abstract A resin composition comprising a modified polypropylene obtained by reacting a polypropylene with a liquid rubber and maleic anhydride in a solvent in the presence of a radical generator, another polyolefin and, if desired, an inorganic and/or an organic filler. The resin composition has excellent coating, adhesion and plating properties.

Inventors

  • 👤 Kikuo Nagatoshi
  • 👤 Toshimichi Ito
  • 👤 Akio Inayoshi
  • 👤 Atsunobu Sakoda
  • 👤 Noriki Fujimoto
  • 👤 Hidehiko Kaji
  • 👤 Hirozo Sugahana

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 22:05
CPC Classifications
C; C08; C08F; C08F291/00; C08F291/02; C08F255/00; C08F255/02; C08K; C08K5/00; C08K5/04; C08K5/09; C08K5/14; C08L; C08L23/00; C08L23/02; C08L23/10; C08L23/12; C08L23/26; C08L2312/00; C08L2555/00; C08L2555/40; C08L51/00; C08L51/06; C08L9/00

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 33 words
Polyolefin resin composition comprising a polyolefin resin and a modified polypropylene obtained by reacting a polypropylene with a liquid rubber and maleic anhydride in a solvent in the presence of a radical generator.
Claim 2
Dependent Claim 33 words
Polyolefin resin composition comprising a polyolefin resin and a modified polypropylene obtained by reacting a polypropylene with a liquid rubber and maleic anhydride in a solvent in the presence of a radical generator.
Claim 3
Dependent Claim 39 words
Polyolefin resin composition according to claim 1, wherein the amount of polyolefin resin is from about 10 to about 90 percent by weight and the amount of modified polypropylene is from about 90 to about 10 percent by weight.
Claim 4
Dependent Claim 74 words
Polyolefin resin composition according to claim 1, wherein the modified polypropylene is a modified polypropylene produced by reacting 100 parts by weight of a polypropylene with from 1 to 20 parts by weight of a liquid rubber and from 5 to 50 parts by weight of maleic anhydride in from 500 to 1,000 parts by weight of a solvent in the presence of from 0.5 to 10 parts by weight of a radical generator.
Claim 5
Dependent Claim 24 words
Polyolefin resin composition according to claim 1, wherein the modified polypropylene has a maleic anhydride content of from 1 to 10 percent by weight.
Claim 6
Dependent Claim 15 words
Polyolefin resin composition according to claim 1, wherein the polyolefin resin is polyethylene or polypropylene.
Claim 7
Dependent Claim 22 words
Polyolefin resin composition according to claim 1, wherein the liquid rubber has a number average molecular weight of from 500 to 10,000.
Claim 8
Dependent Claim 44 words
Polyolefin resin composition which comprises a polyolefin resin, a modified polypropylene obtained by reacting a polypropylene with a liquid rubber and maleic anhydride in a solvent in the presence of a radical generator and at least one of an inorganic filler and organic filler.
Claim 9
Dependent Claim 44 words
Polyolefin resin composition which comprises a polyolefin resin, a modified polypropylene obtained by reacting a polypropylene with a liquid rubber and maleic anhydride in a solvent in the presence of a radical generator and at least one of an inorganic filler and organic filler.
Claim 10
Dependent Claim 29 words
Polyolefin resin composition according to claim 7, wherein the amount of inorganic filler is from 20 to 60 percent by weight based upon the total weight of the composition.
Claim 11
Dependent Claim 28 words
Polyolefin resin composition according to claim 7, wherein the amount of organic filler from 1 to 50 percent by weight based upon the total weight of the composition.
Claim 12
Dependent Claim 22 words
Polyolefin resin composition according to claim 7, wherein the liquid rubber has a number average molecular weight of from 500 to 10,000.

References Cited (Backward Citations)

US3131990A Cited
US4000111A Cited
US3862266A Cited
US3856889A Cited
US3998909A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-12-31 1983-07-02 1984-01-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-12-31 1987-07-02 1988-01-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-12-31 1991-07-02 1992-01-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag