← Back to Patent Explorer
US4178186A Expired / Lapsed US ⏱️ 0.0 years remaining

Resin for coatings

Assignee: Sumitomo Chemical Co Ltd
•
Filing: 1976-02-05
•
Granted: 1979-12-11
•
Expires: 1996-02-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A resin for coatings, particularly useful as a medium for printing inks and paints, comprising a modified polymer produced by adding at least one alpha , beta -unsaturated dicarboxylic acid or anhydride thereof to at least one liquid conjugated diolefinic polymer having a number average molecular weight of 150 to 3,000, a viscosity of 2 to 5,000 cps at 30 DEG C. and at least 50% of cis-1,4 structure and subjecting the resulting adduct to imidation or diamidation with at least one amine having 1 to 27 carbon atoms and whereby the total amine value of the resulting modified polymer being made not more than 3.

Inventors

  • 👤 Seimei Yasui
  • 👤 Minoru Hino

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 07:47
CPC Classifications
C; C08; C08C; C08C19/00; C08C19/30; C08C19/34; C08C19/36; C08C19/28

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 99 words
A resin for coatings comprising a modified polymer consisting of an adduct of at least one liquid conjugated diolefinic polymer having a number average molecular weight of 150 to 3,000, a viscosity of 2 to 5,000 cps at 30° C., and at least 50% of cis-1,4 structure with at least one α,β-unsaturated dicarboxylic acid or anhydride thereof, wherein the carboxyl group or the carboxylic anhydride group is imidated by reacting with at least one primary amine having 1 to 27 carbon atoms and thereby the total amine value of the resulting modified polymer is made not more than 3.
Claim 2
Dependent Claim 99 words
A resin for coatings comprising a modified polymer consisting of an adduct of at least one liquid conjugated diolefinic polymer having a number average molecular weight of 150 to 3,000, a viscosity of 2 to 5,000 cps at 30° C., and at least 50% of cis-1,4 structure with at least one α,β-unsaturated dicarboxylic acid or anhydride thereof, wherein the carboxyl group or the carboxylic anhydride group is imidated by reacting with at least one primary amine having 1 to 27 carbon atoms and thereby the total amine value of the resulting modified polymer is made not more than 3.
Claim 3
Dependent Claim 34 words
The resin according to claim 1, wherein the α,β-unsaturated dicarboxylic acid or anhydride thereof is a member selected from the group consisting of maleic acid, maleic anhydride, fumaric acid, itaconic acid and citraconic acid.
Claim 4
Dependent Claim 28 words
The resin according to claim 1, wherein the α,β-unsaturated dicarboxylic acid or anhydride thereof is a member selected from the group consisting of maleic acid and maleic anhydride.
Claim 5
Dependent Claim 23 words
The resin according to claim 1, wherein the adduct contains 3 to 50% by weight of the α,β-unsaturated dicarboxylic acid or anhydride thereof.
Claim 6
Dependent Claim 40 words
The resin according to claim 1, wherein the liquid conjugated diolefinic polymer is a member selected from the group consisting of a liquid polybutadiene, a liquid polyisoprene, a liquid butadiene-isoprene copolymer, a liquid butadiene-styrene copolymer and a liquid isoprene-styrene copolymer.
Claim 7
Dependent Claim 88 words
A process for producing a resin for coatings, which comprises adding at least one α,β-unsaturated dicarboxylic acid or anhydride thereof to at least one liquid conjugated diolefinic polymer having a number average molecular weight of 150 to 3,000, a viscosity of 2 to 5,000 cps at 30° C. and at least 50% of cis-1,4 structure, and reacting the resulting adduct with at least one primary amine having 1 to 27 carbon atoms, whereby the total amine value of the resulting modified polymer being made not more than 3.
Claim 8
Dependent Claim 88 words
A process for producing a resin for coatings, which comprises adding at least one α,β-unsaturated dicarboxylic acid or anhydride thereof to at least one liquid conjugated diolefinic polymer having a number average molecular weight of 150 to 3,000, a viscosity of 2 to 5,000 cps at 30° C. and at least 50% of cis-1,4 structure, and reacting the resulting adduct with at least one primary amine having 1 to 27 carbon atoms, whereby the total amine value of the resulting modified polymer being made not more than 3.
Claim 9
Dependent Claim 40 words
The process according to claim 6, wherein the liquid conjugated diolefinic polymer is a member selected from the group consisting of a liquid polybutadiene, a liquid polyisoprene, a liquid butadiene-isoprene copolymer, a liquid butadiene-styrene copolymer and a liquid isoprene-styrene copolymer.
Claim 10
Dependent Claim 34 words
The process according to claim 6, wherein the α,β-unsaturated dicarboxylic acid or anhydride thereof is a member selected from the group consisting of maleic acid, maleic anhydride, fumaric acid, itaconic acid and citraconic acid.
Claim 11
Dependent Claim 28 words
The process according to claim 6, wherein the α,β-unsaturated dicarboxylic acid or anhydride thereof is a member selected from the group consisting of maleic acid and maleic anhydride.
Claim 12
Dependent Claim 66 words
The process according to claim 6, wherein the primary amine having 1 to 27 carbon atoms is a member selected from the group consisting of methylamine, ethylamine, propylamine, butylamine, amylamine, hexylamine, oxtylamine, nonylamine, decylamine, undecylamine, dodecylamine, tridecylamine, tetradecylamine, pentadecylamine, hexadecylamine, heptadecylamine, octadecylamine, docosylamine, isopropylamine, isobutylamine, sec-butylamine, tert-butylamine, 2-aminopentane, 3-aminopentane, 1-amino-2-methylbutane, 2-amino-2-methylbutane, 3-amino-2-methylbutane, 4-amino-2-methylbutane, 1-amino-2,2-dimethylpropane, 5-amino-2-methylpentane and aniline, and a mixture of two or more kinds thereof.
Claim 13
Dependent Claim 45 words
A printing ink comprising 3 to 50% by weight of the resin set forth in claim 1, and the remaining amount being a conventional printing ink component selected from at least one member of the group consisting of pigments, solvents, resins, driers, and ultraviolet absorbents.
Claim 14
Dependent Claim 43 words
A paint composition comprising 5 to 80% by weight of the resin set forth in claim 1, and the remaining amount being a conventional paint component selected from at least one member of the group consisting of pigments, solvents, resins, and metallic driers.

References Cited (Backward Citations)

US3429952A Cited
US3654203A Cited
US3778418A Cited
US3804788A Cited
US3856759A Cited
US3884712A Cited
US3971746A Cited
US3983062A Cited
US4051198A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-12-10 1983-06-11 1983-12-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-12-10 1987-06-11 1987-12-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-12-10 1991-06-11 1991-12-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag