← Back to Patent Explorer
US4176720A Expired / Lapsed US ⏱️ 0.0 years remaining

Well cementing in permafrost

Assignee: Atlantic Richfield Co
•
Filing: 1978-07-27
•
Granted: 1979-12-04
•
Expires: 1998-07-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for cementing a string of pipe in the permafrost region of a borehole of a well wherein aqueous drilling fluid actually used in drilling the wellbore in the permafrost region of a wellbore is employed. The drilling fluid contains or is adjusted to contain from about 2 to about 16 volume percent solids. Mixing with the drilling fluid (1) an additive selected from the group consisting of lignosulfonate, lignite, tannin, and mixtures thereof, (2) sufficient base to raise the pH of the drilling fluid into the range of from about 9 to about 12, and (3) cementitious material which will harden in from about 30 to about 40 hours at 40° F. The resulting mixture is pumped into the permafrost region of a wellbore to be cemented and allowed to harden in the wellbore. There is also provided a process for treating an aqueous drilling fluid after it has been used in drilling the wellbore in permafrost, and a cementitious composition for cementing in a permafrost region of a wellbore.

Inventors

  • 👤 William N. Wilson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 12:25
CPC Classifications
C; C04; C04B; C04B28/00; C04B28/02; C04B28/06; C09; C09K; C09K8/00; C09K8/42; C09K8/46; C04B2111/00; C04B2111/76; Y; Y10; Y10S; Y10S166/00; Y10S166/901

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 183 words
A process for cementing in the permafrost region of a wellbore comprising recovering at least part of the aqueous drilling fluid used in drilling a wellbore in the permafrost region, said drilling fluid containing from about 2 to about 16 volume percent solids, mixing with said drilling fluid an additive selected from the group consisting of lignosulfonate, lignite, tannin, and mixtures thereof in an amount of from about 0.05 to about 0.4 pounds per barrel per equivalent pounds per barrel of bentonite as determined by the methylene blue test, essentially contemporaneous with and/or subsequent to the addition of said additive, mixing with said drilling fluid sufficient of at least one base to raise the pH of the mixture into the range of from about 9 to about 12 and from about 50 to about 250 pounds per barrel of at least one cementitious material which will harden in from about 30 to about 40 hours at about 40° F., pumping the resulting final mixture into the permafrost region of the wellbore to be cemented, and allowing said mixture to harden in said wellbore.
Claim 2
Dependent Claim 183 words
A process for cementing in the permafrost region of a wellbore comprising recovering at least part of the aqueous drilling fluid used in drilling a wellbore in the permafrost region, said drilling fluid containing from about 2 to about 16 volume percent solids, mixing with said drilling fluid an additive selected from the group consisting of lignosulfonate, lignite, tannin, and mixtures thereof in an amount of from about 0.05 to about 0.4 pounds per barrel per equivalent pounds per barrel of bentonite as determined by the methylene blue test, essentially contemporaneous with and/or subsequent to the addition of said additive, mixing with said drilling fluid sufficient of at least one base to raise the pH of the mixture into the range of from about 9 to about 12 and from about 50 to about 250 pounds per barrel of at least one cementitious material which will harden in from about 30 to about 40 hours at about 40° F., pumping the resulting final mixture into the permafrost region of the wellbore to be cemented, and allowing said mixture to harden in said wellbore.
Claim 3
Dependent Claim 18 words
A process according to claim 1 wherein said additive is chrome lignosulfonate and said base is sodium hydroxide.
Claim 4
Dependent Claim 16 words
A process according to claim 2 wherein said cementitious material is high in alumina calcium aluminate.
Claim 5
Dependent Claim 17 words
A process according to claim 2 wherein said cementitious material contains a substantial amount of fondu cement.
Claim 6
Dependent Claim 14 words
A process according to claim 1 wherein said cementitious material is high in alumina.
Claim 7
Dependent Claim 17 words
A process according to claim 1 wherein said cementitious material contains a substantial amount of fondu cement.
Claim 8
Dependent Claim 149 words
A process for treating an aqueous drilling fluid after it has been used in drilling a wellbore in permafrost, said drilling fluid containing from about 2 to about 16 volume percent solids, comprising mixing with said drilling fluid an additive selected from the group consisting of lignosulfonate, lignite, tannin, and mixtures thereof in an amount of from about 0.05 to about 0.4 pounds per barrel per equivalent pounds per barrel of bentonite as determined by the methylene blue test, essentially contemporaneous with and/or subsequent to the addition of said additive, mixing with said drilling fluid sufficient of at least one base to raise the pH of the mixture into the range of from about 9 to about 12 and from about 50 to about 250 pounds per barrel of at least one cementitious material which will harden in from about 30 to about 40 hours at about 40° F.
Claim 9
Dependent Claim 149 words
A process for treating an aqueous drilling fluid after it has been used in drilling a wellbore in permafrost, said drilling fluid containing from about 2 to about 16 volume percent solids, comprising mixing with said drilling fluid an additive selected from the group consisting of lignosulfonate, lignite, tannin, and mixtures thereof in an amount of from about 0.05 to about 0.4 pounds per barrel per equivalent pounds per barrel of bentonite as determined by the methylene blue test, essentially contemporaneous with and/or subsequent to the addition of said additive, mixing with said drilling fluid sufficient of at least one base to raise the pH of the mixture into the range of from about 9 to about 12 and from about 50 to about 250 pounds per barrel of at least one cementitious material which will harden in from about 30 to about 40 hours at about 40° F.
Claim 10
Dependent Claim 18 words
A process according to claim 7 wherein said additive is chrome lignosulfonate and said base is sodium hydroxide.
Claim 11
Dependent Claim 16 words
A process according to claim 8 wherein said cementitious material is high in alumina calcium aluminate.
Claim 12
Dependent Claim 17 words
A process according to claim 8 wherein said cementitious material contains a substantial amount of fondu cement.
Claim 13
Dependent Claim 14 words
A process according to claim 7 wherein said cementitious material is high in alumina.
Claim 14
Dependent Claim 17 words
A process according to claim 7 wherein said cementitious material contains a substantial amount of fondu cement.

References Cited (Backward Citations)

US2582459A Cited
US2609882A Cited
US3581825A Cited
US3937282A Cited
US4065318A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-12-03 1983-06-04 1983-12-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-12-03 1987-06-04 1987-12-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-12-03 1991-06-04 1991-12-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag