Process for automatically vertically butt welding steel sheet material for containers
Assignee: Voestalpine AG
•
Filing: 1977-12-20
•
Granted: 1979-11-20
•
Expires: 1997-12-20
Abstract
Abstract Chemically resistant steels for containers are butt welded by using an automatic welding process. The electrode is oscillated over the whole width of the seam and is kept to a maximum thickness of 1 mm.
Inventors
- 👤 Erich Kasper
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 11:18
CPC Classifications
B; B23; B23K; B23K33/00; B23K33/004; B23K35/00; B23K35/22; B23K35/24; B23K35/30; B23K35/3053; B23K35/308; B23K35/3086; B23K9/00; B23K9/02; B23K9/0209; B23K9/23
Claims Analysis
Total Claims: 15
Claim 1
Independent Claim
178 words
An automatic process for butt welding a vertical seam along a vertical butt joint between sheets of rust-proof and chemically resistant steels containing more than 2 percent by weight Ni, in which method the feed motion of a welding wire toward the weld seam, an oscillating movement of the welding wire transverse to the weld seam and the movement of the welding wire along the weld seam are automatically controlled and in which method the edges of the sheets are bevelled on one side only so as to form an open side of the butt joint, said method comprising performing the welding operation along the open side of the butt joint by providing an electrode having a maximum wire thickness of 1 mm, by oscillating the electrode over the whole width of the weld seam with a frequency of 70 to 140 double strokes per minute, by moving the electrode downwardly along the vertical weld seam and by keeping the welding area under a reactive gas atmosphere which contains carbon dioxide, oxygen and a major proportion of argon.
Claim 2
Dependent Claim
178 words
An automatic process for butt welding a vertical seam along a vertical butt joint between sheets of rust-proof and chemically resistant steels containing more than 2 percent by weight Ni, in which method the feed motion of a welding wire toward the weld seam, an oscillating movement of the welding wire transverse to the weld seam and the movement of the welding wire along the weld seam are automatically controlled and in which method the edges of the sheets are bevelled on one side only so as to form an open side of the butt joint, said method comprising performing the welding operation along the open side of the butt joint by providing an electrode having a maximum wire thickness of 1 mm, by oscillating the electrode over the whole width of the weld seam with a frequency of 70 to 140 double strokes per minute, by moving the electrode downwardly along the vertical weld seam and by keeping the welding area under a reactive gas atmosphere which contains carbon dioxide, oxygen and a major proportion of argon.
Claim 3
Dependent Claim
16 words
A process as in claim 1 wherein the electrode has a wire thickness of 0.8 mm.
Claim 4
Dependent Claim
20 words
A process as in claim 1 wherein the electrode oscillates at a frequency of 90 to 120 double-strokes per minute.
Claim 5
Dependent Claim
22 words
A process as in claim 1 wherein the composition of the electrode is stainless steel containing niobium for increasing the corrosion resistance.
Claim 6
Dependent Claim
51 words
A process as in claim 1 wherein a gap is maintained between the edges of the sheets which are to be welded and wherein, after the open side of the butt joint has been welded, a counter-weld is applied in an analogous manner along the other side of the butt joint.
Claim 7
Dependent Claim
27 words
A process as in claim 5 wherein, prior to applying said counter-weld, the side of the butt joint to be counter-welded is subjected to a grinding operation.
Claim 8
Dependent Claim
23 words
A process as in claim 6 wherein the grinding operation forms a groove in the sheets which is filled subsequently by the counter-weld.
Claim 9
Dependent Claim
33 words
A process as in claim 1 wherein the weld seam is effected by welding a plurality of layers in sequence, each subsequent layer being welded in the same manner as the previous layer.
Claim 10
Dependent Claim
21 words
A process as in claim 6 wherein one layer is ground to a concave contour before the next layer is applied.
Claim 11
Dependent Claim
29 words
A process as in claim 1 wherein the sheets have a thickness up to about 4 mm and wherein the weld seam is formed by welding a single layer.
Claim 12
Dependent Claim
34 words
A process as in claim 1 wherein the sheets have a thickness in the range about 4 mm to 7 mm and wherein the weld seam is formed by welding two layers in sequence.
Claim 13
Dependent Claim
32 words
A process as in claim 1 wherein the sheets have a thickness greater than about 7 mm and wherein the weld seam is formed by welding at least three layers in sequence.
Claim 14
Dependent Claim
32 words
A process as in claim 1 wherein the gas atmosphere is a gas mixture containing 84 percent by volume argon, 13 percent by volume carbon dioxide and 3 percent by volume oxygen.
Claim 15
Dependent Claim
45 words
A process as in claim 1 wherein the composition of the electrode is 18-20 percent by weight Cr, 9.5-12 percent by weight Ni, up to 2.5 percent by weight Mo, about 0.05 percent by weight C and traces of Nb, remainder Fe and usual impurities.
References Cited (Backward Citations)
US1812123A
Cited
US2258913A
Cited
US3139506A
Cited
US3328556A
Cited
US3597583A
Cited
US3825712A
Cited
US3845271A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1982-11-19 | 1983-05-21 | 1983-11-20 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1986-11-19 | 1987-05-21 | 1987-11-20 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1990-11-19 | 1991-05-21 | 1991-11-20 | $7700.00 | Window Closed / Lapsed |