US4170681A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of applying a varnish layer to a printed surface and product made thereby
Assignee: Lever Brothers Co
•
Filing: 1978-01-20
•
Granted: 1979-10-09
•
Expires: 1998-01-20
Abstract
Abstract A method of applying a protective varnish layer on a hydrophilic surface carrying at least one area of hydrophobic ink, and the resultant product. The method comprises: applying to at least the inked portions of the surface a layer of an aqueous dispersion containing 5% to about 60% by weight of a film forming polymer or copolymer and 0.5% to about 10% of an auxiliary film forming material capable of raising the critical surface tension of the hydrophobic inked area; and allowing the applied layer to dry.
Inventors
- 👤 John R. Edwards
- 👤 George K. Rennie
- 👤 David A. Rosser
- 👤 Colin Smart
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 03:13
CPC Classifications
B; B41; B41M; B41M7/00; B41M7/02; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24802; Y10T428/24851; Y10T428/24868; Y10T428/24884
Claims Analysis
Total Claims: 15
Claim 1
Independent Claim
116 words
A method of forming a varnish layer on a hydrophilic surface carrying at least one area of hydrophobic ink, comprising: applying to at least the inked portions of said surface a layer of an aqueous dispersion having a viscosity from about 25 to about 500 cps and containing from about 5% to about 60% by weight of a film forming copolymer or polymer, substantially insoluble in water at neutral pH, formed from a vinyl ester and/or acrylic ester, said dispersion further containing from about 0.5% to about 10% of an auxiliary film forming material capable of raising the critical surface tension of the hydrophobic ink area when coated thereon; and allowing said applied layer to dry.
Claim 2
Independent Claim
116 words
A method of forming a varnish layer on a hydrophilic surface carrying at least one area of hydrophobic ink, comprising: applying to at least the inked portions of said surface a layer of an aqueous dispersion having a viscosity from about 25 to about 500 cps and containing from about 5% to about 60% by weight of a film forming copolymer or polymer, substantially insoluble in water at neutral pH, formed from a vinyl ester and/or acrylic ester, said dispersion further containing from about 0.5% to about 10% of an auxiliary film forming material capable of raising the critical surface tension of the hydrophobic ink area when coated thereon; and allowing said applied layer to dry.
Claim 3
Dependent Claim
17 words
A method according to claim 1 wherein the viscosity is from about 50 to about 300 cps.
Claim 4
Dependent Claim
25 words
A method according to claim 1 wherein the critical surface tension of the hydrophobic ink area is less than about 30 dynes cm -1 .
Claim 5
Dependent Claim
25 words
A method according to claim 3 wherein the critical surface tension of the hydrophobic ink area is less than about 25 dynes cm -1 .
Claim 6
Dependent Claim
24 words
A method according to claim 1 wherein the auxiliary material raises the critical surface tension by at least about 5 dynes cm -1 .
Claim 7
Dependent Claim
22 words
A method according to claim 5 wherein the critical surface tension is raised by at least about 10 dynes cm -1 .
Claim 8
Dependent Claim
15 words
A method according to claim 1 wherein the monomer moiety contains a carboxylic acid group.
Claim 9
Dependent Claim
90 words
A method according to claim 1 wherein the film forming copolymer or polymer is selected from the group consisting of (i) polymers of vinyl esters, (ii) polymers of acrylic esters, (iii) copolymers of vinyl and acrylic esters, (iv) copolymers of vinyl and/or acrylic esters with a monomer moiety selected from the group consisting of styrene, crotonic acid, itaconic acid, acrylic acid, 2-ethyl hexyl acrylate, and alkenes with 2 to 12 carbon atoms, and (v) polymers of alkyl methacrylic esters, wherein the alkyl group contains from 1 to 12 carbon atoms.
Claim 10
Dependent Claim
88 words
A method according to claim 1 wherein the auxiliary material is selected from the group of film forming materials consisting of (i) casein, (ii) poly vinyl pyrollidone and copolymers thereof with vinyl acetate, and (iii) alkali soluble copolymers of maleic anhydride with a moiety selected from the group consisting of styrene, alkenes having from 2 to 16 carbon atoms, vinyl alkyl ethers having from 1 to 4 carbon atoms in the alkyl group, and rosin acids with subsequent reaction with polyhydric alcohols containing 2 to 6 carbon atoms.
Claim 11
Dependent Claim
14 words
A method according to claim 9 wherein the alkene is ethylene, propylene or 1-hexene.
Claim 12
Dependent Claim
13 words
A method according to claim 1 wherein the hydrophilic surface is of paper.
Claim 13
Dependent Claim
23 words
A method according to claim 1 wherein the varnish layer has a weight of from about 1 to about 25 g/m 2 .
Claim 14
Dependent Claim
33 words
A method according to claim 1 wherein said vinyl ester and/or acrylic ester is polymerized with a monomer moiety in the molar ratio of about 1:10 to about 10:1 to form said copolymer.
Claim 15
Dependent Claim
25 words
A hydrophilic surface carrying at least one area of hydrophobic ink and a varnish layer on the surface formed by the method of claim 1.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1982-10-08 | 1983-04-09 | 1983-10-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1986-10-08 | 1987-04-09 | 1987-10-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1990-10-08 | 1991-04-09 | 1991-10-09 | $7700.00 | Window Closed / Lapsed |