Cathode ray tube internal resistive coating and method of manufacture

Assignee: GTE Sylvania Inc
•
Filing: 1978-05-08
•
Granted: 1979-08-07
•
Expires: 1998-05-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An internal resistive coating for a cathode ray tube is derived from a suspension which includes electrically conductive particles, electrically insulative particles, silicate solids and a wetting agent of the anionic class. The internal resistive coating is made by mixing the insulative particles, a silicate solution and water, milling the mixture, adding electrically conductive particles to the mixture, milling the electrically conductive particles and mixture to provide a suspension, preparing a stock solution of wetting agent of the anionic class, and stirring the wetting agent stock solution into the suspension to provide a wall dispersed resistive coating suspension.

Inventors

  • 👤 Kenneth Speigel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 06:59
CPC Classifications
H; H01; H01J; H01J29/00; H01J29/86; H01J29/88; H01J2229/00; H01J2229/88; H01J2229/882

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 141 words
In a cathode ray tube having an envelope with an apertured mask assembly therein and interconnected funnel and neck portions wherein the funnel portion has an anode button sealed therein and the neck portion has a mount assembly with affixed snubbers sealed therein, an improved resistive coating disposed on the internal surface of said envelope and contacting said snubbers of said mount assembly, said resistive coating derived from a suspension consisting essentially of electrically conductive and insulative particles, silicate solids and an anionic wetting agent, sand conductive particles being in the range of about 10-45% by weight, said insulative particles in the range of about 30-60% of weight, said silicate solids in the range of about 20-45% by weight and said anionic wetting agent being an alkyl sulfonate in the range of about 0.0014 to 0.014% by weight of said coating.
Claim 2
Dependent Claim 141 words
In a cathode ray tube having an envelope with an apertured mask assembly therein and interconnected funnel and neck portions wherein the funnel portion has an anode button sealed therein and the neck portion has a mount assembly with affixed snubbers sealed therein, an improved resistive coating disposed on the internal surface of said envelope and contacting said snubbers of said mount assembly, said resistive coating derived from a suspension consisting essentially of electrically conductive and insulative particles, silicate solids and an anionic wetting agent, sand conductive particles being in the range of about 10-45% by weight, said insulative particles in the range of about 30-60% of weight, said silicate solids in the range of about 20-45% by weight and said anionic wetting agent being an alkyl sulfonate in the range of about 0.0014 to 0.014% by weight of said coating.
Claim 3
Dependent Claim 42 words
The improved resistive coating of claim 1 wherein said anionic wetting agent is in the form of an alkyl aryl sulfonate wetting agent represented by the formula: ##STR2## where M is selected from the group consisting essentially of sodium, potassium and lithium.
Claim 4
Dependent Claim 35 words
The improved resistive coating of claim 1 wherein said electrically insulative particles are selected from the group consisting essentially of Fe 2 O 3 , Fe 3 O 4 and Cr 2 O 3 .
Claim 5
Dependent Claim 92 words
The improved resistive coating of claim 1 wherein said electrically conductive particles are in the form of graphite in the range of about 10-45% by weight, said electrically insulative particles are in the form of Fe 2 O 3 in the range of about 30-60% by weight, said silicate solids are in the forms of sodium silicate in the range of about 20-45% by weight and said wetting agent is in the form of an alkyl aryl sulfonate in the range of about 0.0014 to 0.014% by weight of said resistive coating.
Claim 6
Dependent Claim 29 words
The improved resistive coating of claim 1 wherein said resistive coating extends from said snubbers to said anode button sealed in said funnel portion of said cathode ray tube.
Claim 7
Dependent Claim 23 words
The improved resistive coating of claim 1 wherein said resistive coating extends from said snubbers to said apertured mask assembly in said envelope.

References Cited (Backward Citations)

US3791546A Cited
US4041347A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-08-06 1983-02-05 1983-08-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-08-06 1987-02-05 1987-08-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-08-06 1991-02-05 1991-08-07 $7700.00 Window Closed / Lapsed