← Back to Patent Explorer
US4163032A Expired / Lapsed US ⏱️ 0.0 years remaining

Thermoplastic molding compositions

Assignee: Bayer AG
•
Filing: 1978-10-20
•
Granted: 1979-07-31
•
Expires: 1998-10-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A thermoplastic molding composition having improved flow, toughness. and heat distortion comprising a polymer mixture of (A) 25 to 95% by weight of a graft polymer of 70 to 30% by weight of a mixture of styrene (95 to 50% by weight) and acrylonitrile (5 to 50% by weight) on 30 to 70% by weight of an EPDM-rubber, and (B) 50 to 75% by weight of a terpolymer of acrylonitrile, maleic acid anhydride and styrene, the terpolymer containing 10 to 30 parts by weight of acrylonitrile, 7.5 to 15 parts by weight of maleic acid anhydride, and 82.5 to 55 parts by weight of styrene in copolymerised form.

Inventors

  • 👤 Lothar Liebig
  • 👤 Frank Wingler
  • 👤 Karl-Heinz Ott
  • 👤 Gert Humme
  • 👤 Alfred Pischtschan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 16:50
CPC Classifications
C; C08; C08L; C08L25/00; C08L25/02; C08L25/04; C08L25/08; C08L25/12; C08L51/00; C08L51/04; C08L51/06

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 105 words
A thermoplastic molding composition comprising a polymer mixture of (A) 25 to 95% by weight of a graft polymer of 70 to 30% by weight of a mixture of 95 to 50% by weight of styrene and of 5 to 50% by weight of and acrylonitrile on 30 to 70% by weight of an EPDM-rubber, and (B) 5 to 75% by weight of a terpolymer of acrylonitrile, maleic acid anhydride and styrene, the terpolymer containing 10 to 30 parts by weight of acrylonitrile, 7.5 to 15 parts by weight of maleic acid anhydride, and 82.5 to 55 parts by weight of styrene in copolymerised form.
Claim 2
Dependent Claim 105 words
A thermoplastic molding composition comprising a polymer mixture of (A) 25 to 95% by weight of a graft polymer of 70 to 30% by weight of a mixture of 95 to 50% by weight of styrene and of 5 to 50% by weight of and acrylonitrile on 30 to 70% by weight of an EPDM-rubber, and (B) 5 to 75% by weight of a terpolymer of acrylonitrile, maleic acid anhydride and styrene, the terpolymer containing 10 to 30 parts by weight of acrylonitrile, 7.5 to 15 parts by weight of maleic acid anhydride, and 82.5 to 55 parts by weight of styrene in copolymerised form.
Claim 3
Dependent Claim 21 words
A thermoplastic molding composition, as claimed in claim 1, wherein the terpolymer has a heterogeneity index U of 0.5 to 1.5.
Claim 4
Dependent Claim 24 words
A thermoplastic molding composition, as claimed in claim 1, wherein the terpolymer has been obtained by continuous mixed polymerisation under steady state concentration conditions.
Claim 5
Dependent Claim 26 words
A thermoplastic molding composition, as claimed in claim 1, wherein the acrylonitrile content of the terpolymer is substantially the same as that of the graft polymer.

References Cited (Backward Citations)

US3267178A Cited
US3278642A Cited
DE1245131B Cited
DE1949487U Cited
GB1315219A Cited
US4104328A Cited
US4107234A Cited
US4113798A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-07-30 1983-01-29 1983-07-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-07-30 1987-01-29 1987-07-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-07-30 1991-01-29 1991-07-31 $7700.00 Window Closed / Lapsed