Abstract
Abstract A high impact sight glass assembly and production method are described, in which the glass lens is fused into an enamel coated metal ring such that the glass lens is fused to the enamel coating and the entire glass area is under compression. The glass lens is placed in the bore of a flange, and the lens and flange ring are heated, whereby the lens flows to conform to the bore of the flange and is fused to the enamel coating.
Inventors
- 👤 Roland R. Van der Beck
- 👤 James W. Chapman
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 12:17
CPC Classifications
G; G02; G02B; G02B7/00; G02B7/007; C; C03; C03C; C03C27/00; C03C27/04; C03C27/042
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
54 words
A sight glass assembly comprising a lens of soda-lime plate glass mounted in and compressed by an enamelled steel, Inconel or Incolloy metal ring having a wall thickness at least equal to 0.3 times the diameter of said lens, said metal ring having an enamel coating, and said lens being fused to said coating.
Claim 2
Dependent Claim
54 words
A sight glass assembly comprising a lens of soda-lime plate glass mounted in and compressed by an enamelled steel, Inconel or Incolloy metal ring having a wall thickness at least equal to 0.3 times the diameter of said lens, said metal ring having an enamel coating, and said lens being fused to said coating.
Claim 3
Independent Claim
120 words
A method of making a sight glass assembly comprising: (a) placing a non-adhesive substrate setter within a bore of a steel, Inconel or Incolloy metal ring having a wall thickness at least equal to 0.3 times the inside diameter of the ring and having an enamel coating (b) placing a soda-lime plate glass lens in the bore of said enameled ring; (c) heating the substrate, the metal ring and the glass lens so arranged to the flowpoint temperature of said lens so that said ring expands and said lens conforms to the bore of said ring and is fused to said enamel coating; (d) and cooling said ring and said lens to compress said glass lens within said enameled ring.
Claim 4
Independent Claim
120 words
A method of making a sight glass assembly comprising: (a) placing a non-adhesive substrate setter within a bore of a steel, Inconel or Incolloy metal ring having a wall thickness at least equal to 0.3 times the inside diameter of the ring and having an enamel coating (b) placing a soda-lime plate glass lens in the bore of said enameled ring; (c) heating the substrate, the metal ring and the glass lens so arranged to the flowpoint temperature of said lens so that said ring expands and said lens conforms to the bore of said ring and is fused to said enamel coating; (d) and cooling said ring and said lens to compress said glass lens within said enameled ring.
Claim 5
Dependent Claim
19 words
Method of claim 2 wherein the glass lens initially is longer in diameter than the bore of the ring.
Claim 6
Dependent Claim
13 words
Method of claim 2 wherein the heating temperature employed is approximately 1600° F.
Claim 7
Dependent Claim
15 words
Method of claim 2 wherein the enameled metal ring is placed on a non-adhesive substrate.
References Cited (Backward Citations)
US1695830A
Cited
US2946156A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1982-07-30 | 1983-01-29 | 1983-07-31 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1986-07-30 | 1987-01-29 | 1987-07-31 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1990-07-30 | 1991-01-29 | 1991-07-31 | $7700.00 | Window Closed / Lapsed |