Thermoplastic molding composition comprising styrene-maleimide and polycarbonate

Assignee: Atlantic Richfield Co
•
Filing: 1978-10-10
•
Granted: 1979-07-10
•
Expires: 1998-10-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Thermoplastic molding compositions consist of: (a) 10-90% by weight copolymer of maleimide and styrene containing about 5-35% maleimide and 60-95% styrene; and (b) 10-90% by weight of a polycarbonate of a dihydric phenol and a derivative of carbonic acid.

Inventors

  • 👤 Ronald A. Fava

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 17:26
CPC Classifications
C; C08; C08L; C08L51/00; C08L51/04; C08L69/00

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 50 words
A thermoplastic molding composition which comprises: A. from about 10% to about 90% by weight of a polycarbonate; B. from about 10% to about 90% by weight of a copolymer of maleimide and styrene containing from about 5% to about 35% maleimide and from about 65% to about 95% styrene.
Claim 2
Dependent Claim 50 words
A thermoplastic molding composition which comprises: A. from about 10% to about 90% by weight of a polycarbonate; B. from about 10% to about 90% by weight of a copolymer of maleimide and styrene containing from about 5% to about 35% maleimide and from about 65% to about 95% styrene.
Claim 3
Dependent Claim 20 words
The composition of claim 1 in which the concentration range of each component is from about 25% to about 75%.
Claim 4
Dependent Claim 15 words
The composition of claim 2 in which the concentration of each component is about 50%.
Claim 5
Dependent Claim 13 words
The composition of claim 1 in which the polycarbonate is a polyphenylene carbonate.
Claim 6
Dependent Claim 57 words
The composition of claim 1 in which the copolymer of maleimide and styrene is prepared by subjecting a copolymer of maleic anhydride and styrene to a basic aqueous nitrogenous system at a temperature of from about 125° to about 200° C. at an autogenous pressure for 0.5 to 48 hours and thereafter depressurizing and devolatilizing the product.

References Cited (Backward Citations)

US3652715A Cited
US3770697A Cited
US3998907A Cited
US3862998A Cited
US3966842A Cited
US4122130A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-07-09 1983-01-08 1983-07-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-07-09 1987-01-08 1987-07-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-07-09 1991-01-08 1991-07-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag