Abstract

Abstract A process for making densified kaolin clay pellets of high bulk density, good handling and bulk flow properties, and low moisture content is disclosed. The process consists essentially of mixing substantially dry kaolin clay with water to bring the total moisture content of the finely divided kaolin clay to from about 17% to about 26% by weight based on the weight of said dry kaolin clay during mixing in a first pin mixer, followed by micropulverization, and subsequent pelletization by pin mixing. The pellets are dried to 1% or less moisture content by weight based on the weight of dry kaolin clay.

Inventors

  • 👤 Timothy G. Florea
  • 👤 Charles R. Price

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 21:06
CPC Classifications
B; B01; B01J; B01J2/00; B01J2/10; B28; B28C; B28C1/00; B28C1/003

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 178 words
A process for making densified kaolin clay pellets of high bulk density, good handling and bulk flow properties, and low moisture content by the steps comprising: (a) feeding substantially dry, finely divided kaolin clay to a first pin mixing means; (b) adding water in a fine spray to the kaolin clay to bring the total moisture content of the finely divided kaolin clay to about 17% to 26% by weight based on the weight of said dry kaolin clay, and working said moistened clay in said pin mixing means; (c) passing said kaolin clay from said first pin mixing means into a micropulverizing means; (d) micropulverizing said kaolin clay in said micropulverizing means; (e) passing said kaolin clay from said micropulverizing means into a second pin mixing means and forming pellets of said micropulverized kaolin clay; (f) passing said pelletized kaolin clay from said second pin mixing means into a rotary dryer means; and (g) drying said pellets to a moisture content of less than about 1% by weight based on the weight of said dry kaolin clay.
Claim 2
Dependent Claim 178 words
A process for making densified kaolin clay pellets of high bulk density, good handling and bulk flow properties, and low moisture content by the steps comprising: (a) feeding substantially dry, finely divided kaolin clay to a first pin mixing means; (b) adding water in a fine spray to the kaolin clay to bring the total moisture content of the finely divided kaolin clay to about 17% to 26% by weight based on the weight of said dry kaolin clay, and working said moistened clay in said pin mixing means; (c) passing said kaolin clay from said first pin mixing means into a micropulverizing means; (d) micropulverizing said kaolin clay in said micropulverizing means; (e) passing said kaolin clay from said micropulverizing means into a second pin mixing means and forming pellets of said micropulverized kaolin clay; (f) passing said pelletized kaolin clay from said second pin mixing means into a rotary dryer means; and (g) drying said pellets to a moisture content of less than about 1% by weight based on the weight of said dry kaolin clay.
Claim 3
Dependent Claim 46 words
A process according to claim 1 wherein sufficient water is added to said first pin mixing means to bring the total moisture content of the finely divided kaolin clay to from about 20% to 25% by weight based on the weight of said dry kaolin clay.
Claim 4
Dependent Claim 46 words
A process according to claim 1 wherein sufficient water is added to said first pin mixing means to bring the total moisture content of the finely divided kaolin clay to from about 22.5% to 25% by weight based on the weight of said dry kaolin clay.
Claim 5
Dependent Claim 42 words
A process according to claim 1 wherein sufficient water is added to said first pin mixing means to bring the total moisture content of the finely divided kaolin clay to 23% by weight based on the weight of said dry kaolin clay.
Claim 6
Dependent Claim 55 words
A process according to claim 1 wherein additional water is added to said second pin mixing means, said additional water not exceeding an amount sufficient to maintain the total moisture content of the kaolin clay in the range of about 17% to about 26% by weight based on the weight of said dry kaolin clay.
Claim 7
Dependent Claim 30 words
A process according to claim 1 wherein the total water employed in pelletization of the kaolin clay is added to the said kaolin clay in said first pin mixing means.
Claim 8
Dependent Claim 47 words
A process according to claim 1 wherein said pelletized kaolin clay from said second pin mixing means is passed to a third pin mixing means prior to introduction into the rotary dryer, said third pin mixing means serving to further pelletize and polish said kaolin clay pellets.

References Cited (Backward Citations)

US3406426A Cited
US3277218A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-06-25 1982-12-25 1983-06-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-06-25 1986-12-25 1987-06-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-06-25 1990-12-25 1991-06-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag