Patent US4264567A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4158643A Expired / Lapsed US ⏱️ 0.0 years remaining

Catalytic carbon for oxidation of carbon monoxide in the presence of sulfur dioxide

Assignee: Calgon Carbon Corp
•
Filing: 1977-09-09
•
Granted: 1979-06-19
•
Expires: 1997-09-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A carbon supported catalyst used for carbon monoxide oxidation is chemically modified by treating the activated carbon support with an oxidizing agent and/or a hydrophobic compound prior to impregnation with the catalyst mixture. The thus treated catalytic carbon is capable of oxidizing carbon monoxide in an air stream containing sulfur dioxide over an extended period of time.

Inventors

  • 👤 Rabindra K. Sinha

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 06:40
CPC Classifications
B; B01; B01D; B01D53/00; B01D53/34; B01D53/46; B01D53/62; B01J; B01J21/00; B01J21/18; B01J37/00; B01J37/12; Y; Y02; Y02A; Y02A50/00; Y02A50/20

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 248 words
In the method of preparing activated carbon supported catalysts for oxidation of carbon monoxide, comprising the step of impregnating an activated carbon support with a catalyst composition comprising one or more members selected from the group consisting of Cu, Cr, Ni, Fe, Mn, Au, Ag, Pt, Pd, Rh and oxides and chloride, hydroxide, carbonate and nitrate salts thereof, the improvement comprising the additional steps of, first, oxidatively modifying said activated carbon support by treating said carbon support with a fluid oxidizing agent prior to impregnating thereof with said catalyst, whereby oxygen is added to the surface of said activated carbon support in an amount of from about 1% to about 5% by weight of said activated carbon support and the reducing properties of said activated carbon support are substantially reduced, provided that, where the oxidizing agent is an oxyacid, that the acid is employed in a concentration of from 1 to 15 weight %, and in an amount, expressed as a weight ratio of acid to activated carbon, of from 1:1 to 5:1, whereby weight loss from the activated carbon as a result of acid treatment does not occur, and, second, impregnating said activated carbon support with an inert hydrophobic compound in an amount of from about 1% to about 20% by weight of said activated carbon, before the step of impregnating said activated carbon support with said catalyst composition, said improvement resulting in an activated carbon supported catalyst having improved efficiency in the presence of sulfur dioxide.
Claim 2
Dependent Claim 248 words
In the method of preparing activated carbon supported catalysts for oxidation of carbon monoxide, comprising the step of impregnating an activated carbon support with a catalyst composition comprising one or more members selected from the group consisting of Cu, Cr, Ni, Fe, Mn, Au, Ag, Pt, Pd, Rh and oxides and chloride, hydroxide, carbonate and nitrate salts thereof, the improvement comprising the additional steps of, first, oxidatively modifying said activated carbon support by treating said carbon support with a fluid oxidizing agent prior to impregnating thereof with said catalyst, whereby oxygen is added to the surface of said activated carbon support in an amount of from about 1% to about 5% by weight of said activated carbon support and the reducing properties of said activated carbon support are substantially reduced, provided that, where the oxidizing agent is an oxyacid, that the acid is employed in a concentration of from 1 to 15 weight %, and in an amount, expressed as a weight ratio of acid to activated carbon, of from 1:1 to 5:1, whereby weight loss from the activated carbon as a result of acid treatment does not occur, and, second, impregnating said activated carbon support with an inert hydrophobic compound in an amount of from about 1% to about 20% by weight of said activated carbon, before the step of impregnating said activated carbon support with said catalyst composition, said improvement resulting in an activated carbon supported catalyst having improved efficiency in the presence of sulfur dioxide.
Claim 3
Dependent Claim 37 words
The method of claim 1 wherein the hydrophobic compound is one or more members selected from the group consisting of aliphatic hydrocarbons of at least fourteen carbon atoms and aromatic hydrocarbons of at least ten carbon atoms.
Claim 4
Dependent Claim 12 words
An activated carbon supported catalyst produced by the method of claim 1.
Claim 5
Dependent Claim 40 words
The activated carbon supported catalyst of claim 3 wherein the hydrophobic compound is one or more members selected from the group consisting of aliphatic hydrocarbons of at least fourteen carbon atoms and aromatic hydrocarbons of at least ten carbon atoms.
Claim 6
Dependent Claim 248 words
In the method of preparing activated carbon supported catalysts for oxidation of carbon monoxide, comprising the step of impregnating an activated carbon support with a catalyst composition comprising one or more members selected from the group consisting of Cu, Cr, Ni, Fe, Mn, Au, Ag, Pt, Pd, Rh and oxides and chloride, hydroxide, carbonate and nitrate salts thereof, the improvement comprising the additional steps of, first, oxidatively modifying said activated carbon support by treating said carbon support with a fluid oxidizing agent prior to impregnating thereof with said catalyst, whereby oxygen is added to the surface of said activated carbon support in an amount of from about 1% to about 5% by weight of said activated carbon support and the reducing properties of said activated carbon support are substantially reduced, provided that, where the oxidizing agent is an oxyacid, that the acid is employed in a concentration of from 1 to 15 weight %, and in an amount, expressed as a weight ratio of acid to activated carbon, of from 1:1 to 5:1, whereby weight loss from the activated carbon as a result of acid treatment does not occur, and, second, impregnating said activated carbon support with an inert hydrophobic compound in an amount of from about 1% to about 20% by weight of said activated carbon, after the step of impregnating said activated carbon support with said catalyst composition, said improvement resulting in an activated carbon supported catalyst having improved efficiency in the presence of sulfur dioxide.
Claim 7
Dependent Claim 248 words
In the method of preparing activated carbon supported catalysts for oxidation of carbon monoxide, comprising the step of impregnating an activated carbon support with a catalyst composition comprising one or more members selected from the group consisting of Cu, Cr, Ni, Fe, Mn, Au, Ag, Pt, Pd, Rh and oxides and chloride, hydroxide, carbonate and nitrate salts thereof, the improvement comprising the additional steps of, first, oxidatively modifying said activated carbon support by treating said carbon support with a fluid oxidizing agent prior to impregnating thereof with said catalyst, whereby oxygen is added to the surface of said activated carbon support in an amount of from about 1% to about 5% by weight of said activated carbon support and the reducing properties of said activated carbon support are substantially reduced, provided that, where the oxidizing agent is an oxyacid, that the acid is employed in a concentration of from 1 to 15 weight %, and in an amount, expressed as a weight ratio of acid to activated carbon, of from 1:1 to 5:1, whereby weight loss from the activated carbon as a result of acid treatment does not occur, and, second, impregnating said activated carbon support with an inert hydrophobic compound in an amount of from about 1% to about 20% by weight of said activated carbon, after the step of impregnating said activated carbon support with said catalyst composition, said improvement resulting in an activated carbon supported catalyst having improved efficiency in the presence of sulfur dioxide.
Claim 8
Dependent Claim 37 words
The method of claim 5 wherein the hydrophobic compound is one or more members selected from the group consisting of aliphatic hydrocarbons of at least fourteen carbon atoms and aromatic hydrocarbons of at least ten carbon atoms.
Claim 9
Dependent Claim 12 words
An activated carbon supported catalyst produced by the method of claim 5.
Claim 10
Dependent Claim 40 words
The activated carbon supported catalyst of claim 7 wherein the hydrophobic compound is one or more members selected from the group consisting of aliphatic hydrocarbons of at least fourteen carbon atoms and aromatic hydrocarbons of at least ten carbon atoms.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-06-18 1982-12-18 1983-06-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-06-18 1986-12-18 1987-06-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-06-18 1990-12-18 1991-06-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag