← Back to Patent Explorer
US4151315A Expired / Lapsed US ⏱️ 0.0 years remaining

Manufacture of coated split-resistant improvement webs from paper having unit weight 60 g/m2

Assignee: Casco AB
•
Filing: 1978-06-15
•
Granted: 1979-04-24
•
Expires: 1998-06-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for manufacturing split-resistant improvement webs from paper having a weight per unit area of ≦60 g/m 2 which has a hardened synthetic resin on the decorative side and which are used for gluing to the surface of wood-based panels wherein a solution or dispersion of a hardenable impregnating resin is first applied to the paper using a metered-roller application in an amount between about 8% based on the solids content of the resin (of the weight of the paper) but less than an amount such as to assure that the resin does not penetrate to the reverse side of the paper. The impregnated paper is then dried, decoratively printed, and then coated with a solution or dispersion of a hardenable resin followed by drying and hardening. Such webs are easily handled and can be rolled up and the method allows the use of conventional paper which does not have to be specially treated.

Inventors

  • 👤 Jurgen Fock
  • 👤 Helmut Buhler

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 12:36
CPC Classifications
B; B41; B41M; B41M3/00; B41M3/18; D; D21; D21H; D21H27/00; D21H27/18; D21H27/22; D21H27/26; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24802; Y10T428/24851; Y10T428/24868

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 122 words
In a method for the manufacture of split-resistant improvement webs wherein a thin paper having a weight per unit area of ≦60 g/m 2 is coated with a hardenable synthetic resin after decorative printing, dried, and hardened, the improvement which comprises, prior to decorative printing, applying a solution or dispersion of a hardenable impregnating resin to the side of the paper to be decorated using a metered roller application, the amount of said impregnating resin being between at least about 8% of the weight of the paper based on the solids content of the resin, and that amount of resin to assure that the resin does not penetrate through to the reverse side of the paper, and then drying the impregnated paper.
Claim 2
Dependent Claim 122 words
In a method for the manufacture of split-resistant improvement webs wherein a thin paper having a weight per unit area of ≦60 g/m 2 is coated with a hardenable synthetic resin after decorative printing, dried, and hardened, the improvement which comprises, prior to decorative printing, applying a solution or dispersion of a hardenable impregnating resin to the side of the paper to be decorated using a metered roller application, the amount of said impregnating resin being between at least about 8% of the weight of the paper based on the solids content of the resin, and that amount of resin to assure that the resin does not penetrate through to the reverse side of the paper, and then drying the impregnated paper.
Claim 3
Dependent Claim 26 words
The process of claim 1 wherein after the decorative printing and prior to coating with the hardenable resin, an intermediate layer is applied to the paper.
Claim 4
Dependent Claim 21 words
The process of claim 1 wherein the impregnating resin is applied by means of the printing mechanism of a printing machine.
Claim 5
Dependent Claim 26 words
The process of claim 3 wherein the impregnating process and the subsequent decorative print process are carried out in the printing machine in one operating step.
Claim 6
Dependent Claim 19 words
The process of claim 1 wherein an aqueous solution of an aminoplast resin is used as an impregnating resin.

References Cited (Backward Citations)

US1634830A Cited
US2380047A Cited
US2668124A Cited
GB850948A Cited
US3654044A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-04-23 1982-10-23 1983-04-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-04-23 1986-10-23 1987-04-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-04-23 1990-10-23 1991-04-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags