← Back to Patent Explorer
US4148946A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for maintaining a non-oxidizing atmosphere at positive pressure within the metallic strip preparation furnace of a metallic coating line during line stops

Assignee: Armco Inc
•
Filing: 1977-02-14
•
Granted: 1979-04-10
•
Expires: 1997-02-14
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a line for coating a ferrous base metal strip with a molten coating metal, the line being of the type having a preparation furnace for the strip comprising a direct fired furnace, a controlled atmosphere heating furnace, one or more cooling chambers and a snout leading beneath the surface of the molten coating metal bath, all in sealed relationship to each other, the improvement comprising a method and means for maintaining a non-oxidizing atmosphere at positive pressure within the entire preparation furnace during line stop. To this end, a retractable, refractory lined door means is provided in the conduit between the direct fired furnace and its exhaust fan to seal off the direct fired furnace from its exhaust fan and an air dilution opening in that conduit. Additionally, means are provided to add excess nitrogen flow to the preparation furnace to maintain a positive pressure therein. Thus, during a line stop, the refractory lined door will be shifted from its normal retracted position to its position sealing off the direct fired furnace and the means for adding excess nitrogen will be actuated to maintain a positive pressure within the entire strip preparation furnace of the metallic coating line.

Inventors

  • 👤 Fred Byrd
  • 👤 James A. Fisher

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 20:25
CPC Classifications
C; C23; C23C; C23C2/00; C23C2/003; C23C2/0035; C23C2/0038; C23C2/004; C23C2/02; C23C2/022; C23C2/0224

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 252 words
In a process of coating a ferrous base metal strip with a molten coating metal, in a coating line of the type having a strip preparation furnace comprising a direct fired furnace with an exhaust system for products of combustion comprising a duct leading from said direct fired furnace to an exhaust fan, a controlled atmosphere heating furnace, at least one cooling chamber and a snout extending beneath the surface of a bath of said molten coating metal, all connected serially in sealed relationship, the steps of providing an air dilution opening in said duct in the form of a gap in said duct to cool and dilute said products of combustion ahead of said fan, providing a slab-like refractory lined door shiftable between an open position out of said gap and a closed position within said gap to seal said direct fired furnace from said exhaust fan and said air dilution opening, shifting said door means from said open position to said closed position at the time of a line stop and at the same time introducing into said strip preparation furnace a non-oxidizing atmosphere at a positive pressure so as to purge said strip preparation furnace and to prevent oxygen from the ambient atmosphere from entering said strip preparation furnace, said door means being thinner than said gap, and using said exhaust fan to draw ambient air through the upper portion of said gap and over said door when said door is in said closed position to cool said door.
Claim 2
Dependent Claim 252 words
In a process of coating a ferrous base metal strip with a molten coating metal, in a coating line of the type having a strip preparation furnace comprising a direct fired furnace with an exhaust system for products of combustion comprising a duct leading from said direct fired furnace to an exhaust fan, a controlled atmosphere heating furnace, at least one cooling chamber and a snout extending beneath the surface of a bath of said molten coating metal, all connected serially in sealed relationship, the steps of providing an air dilution opening in said duct in the form of a gap in said duct to cool and dilute said products of combustion ahead of said fan, providing a slab-like refractory lined door shiftable between an open position out of said gap and a closed position within said gap to seal said direct fired furnace from said exhaust fan and said air dilution opening, shifting said door means from said open position to said closed position at the time of a line stop and at the same time introducing into said strip preparation furnace a non-oxidizing atmosphere at a positive pressure so as to purge said strip preparation furnace and to prevent oxygen from the ambient atmosphere from entering said strip preparation furnace, said door means being thinner than said gap, and using said exhaust fan to draw ambient air through the upper portion of said gap and over said door when said door is in said closed position to cool said door.
Claim 3
Dependent Claim 12 words
The process claimed in claim 1 wherein said non-oxidizing atmosphere is nitrogen.
Claim 4
Dependent Claim 35 words
The process claimed in claim 1 including the step of providing a purge valve in said strip preparation furnace for said non-oxidizing atmosphere and opening said purge valve at the time of a line stop.
Claim 5
Dependent Claim 12 words
The process claimed in claim 3, wherein said non-oxidizing atmosphere is nitrogen.
Claim 6
Dependent Claim 35 words
The process claimed in claim 1 including the step of providing a purge valve in said strip preparation furnace for said non-oxidizing atmosphere and opening said purge valve at the time of a line stop.
Claim 7
Dependent Claim 218 words
In a process of coating a ferrous base metal strip with a molten coating metal, in a coating line of the type having a strip preparation furnace comprising a direct fired furnace with an exhaust system for products of combustion comprising a duct leading from said direct fired furnace to an exhaust fan, a controlled atmosphere heating furnace, at least one cooling chamber and a snout extending beneath the surface of a bath of said molten coating metal, all connected serially in sealed relationship, the steps of providing an air dilution opening in said duct in the form of a gap in said duct to cool and dilute said products of combustion ahead of said fan, providing a door shiftable between an open position out of said gap and a closed position within said gap to seal said direct fired furnace from said exhaust fan and said air dilution opening, shifting said door means from said open position to said closed position at the time of a line stop and at the same time introducing into said strip preparation furnace a non-oxidizing atmosphere at a positive pressure so as to purge said strip preparation furnace and to prevent oxygen from the ambient atmosphere from entering said strip preparation furnace, and cooling said door when in said closed position.
Claim 8
Dependent Claim 218 words
In a process of coating a ferrous base metal strip with a molten coating metal, in a coating line of the type having a strip preparation furnace comprising a direct fired furnace with an exhaust system for products of combustion comprising a duct leading from said direct fired furnace to an exhaust fan, a controlled atmosphere heating furnace, at least one cooling chamber and a snout extending beneath the surface of a bath of said molten coating metal, all connected serially in sealed relationship, the steps of providing an air dilution opening in said duct in the form of a gap in said duct to cool and dilute said products of combustion ahead of said fan, providing a door shiftable between an open position out of said gap and a closed position within said gap to seal said direct fired furnace from said exhaust fan and said air dilution opening, shifting said door means from said open position to said closed position at the time of a line stop and at the same time introducing into said strip preparation furnace a non-oxidizing atmosphere at a positive pressure so as to purge said strip preparation furnace and to prevent oxygen from the ambient atmosphere from entering said strip preparation furnace, and cooling said door when in said closed position.

References Cited (Backward Citations)

US1890065A Cited
US2711683A Cited
US3222042A Cited
US3396951A Cited
US3551185A Cited
US3827854A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-04-09 1982-10-09 1983-04-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-04-09 1986-10-09 1987-04-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-04-09 1990-10-09 1991-04-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag